摘要:
The present invention relates to a process for the production of polyarylene ether block copolymers comprising, in a first stage, the reaction of at least one aromatic dihydroxy compound comprising 4,4′-dihydroxybiphenyl in a molar excess and of at least one aromatic dihalogen compound, to form a polybiphenyl sulfone polymer, and then, in a second stage, the reaction of the polybiphenyl sulfone polymer with at least one aromatic dihydroxy compound and of at least one aromatic dihalogen compound.The invention further relates to the resultant polyarylene sulfone block copolymers and to the use of the polyarylene sulfone block copolymers for the production of moldings, fibers, films, or foams.
摘要:
The present invention relates to a process for the production of polyarylene ether block copolymers comprising, in a first stage, the reaction of at least one aromatic dihydroxy compound comprising 4,4′-dihydroxybiphenyl in a molar excess and of at least one aromatic dihalogen compound, to form a polybiphenyl sulfone polymer, and then, in a second stage, the reaction of the polybiphenyl sulfone polymer with at least one aromatic dihydroxy compound and of at least one aromatic dihalogen compound.The invention further relates to the resultant polyarylene sulfone block copolymers and to the use of the polyarylene sulfone block copolymers for the production of moldings, fibers, films, or foams.
摘要:
The present invention relates to compositions comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, and (C) at least one anhydride of a polybasic carboxylic acid with a number-average molar mass of at most 600 g/mol. The present invention moreover relates to the use of the abovementioned anhydrides of polybasic carboxylic acids in compositions comprising at least one polyarylene ether and at least one polyarylene sulfide.
摘要:
The present invention relates to thermoplastic molding materials comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, (C) optionally at least one functionalized polyarylene ether comprising carboxyl groups, (D) at least one fibrous or particulate filler and (E) optionally further additives and/or processing assistants, the ratio of the apparent viscosity of the component (A) to that of the component (B), determined at 350° C. and a shear rate of 1150 s−1, being from 2.5 to 3.7.
摘要:
The present invention relates to thermoplastic molding compositions composed of the following components: (A) at least one polyarylene ether (A1) having an average of at most 0.1 phenolic end groups per polymer chain, and at least one polyarylene ether (A2) having an average of at least 1.5 phenolic end groups per polymer chain, (B) at least one fibrous or particulate filler, and (C) optionally further additives and/or processing aids. The present invention further relates to a process for producing the thermoplastic molding compositions of the invention, the use of these for producing moldings, fibers, foams, or films, and to the resultant moldings, fibers, foams, and films.
摘要:
The present invention relates to thermoplastic molding compositions comprising the following components: (A) at least one polyarylene ether (A1) having an average of at most 0.1 phenolic end group per polymer chain and at least one polyarylene ether (A2) having an average of at least 1.5 phenolic end groups per polymer chain, (B) at least one polyarylene sulfide, (C) at least one functionalized polyarylene ether comprising carboxy groups, (D) at least one fibrous or particulate filler, and (E) optionally further additives and/or processing aids. The present invention further relates to a process for producing the thermoplastic molding compositions of the invention, to the use of these for producing moldings, fibers, foams, or films, and to the resultant moldings, fibers, foams, and films.
摘要:
The present invention relates to a process for the production of low-halogen-content polybiphenyl sulfone polymers, to the resultant polybiphenyl sulfone polymers, to polybiphenyl sulfone polymers having less than 400 ppm content of polymer-bonded halogen, to thermoplastic molding compositions comprising these polybiphenyl sulfone polymers, and to their use for the production of moldings, of fibers, of films, of membranes, or of foams.
摘要:
The present invention relates to a process for preparing a block copolymer comprising poly-arylene ether and polyalkylene oxide blocks, comprising the reaction of an HO-terminated poly-arylene ether with a monomeric alkylene oxide.The present invention also relates to a block copolymer obtainable from this process.The invention additionally relates to a triblock polymer with polyalkylene oxide-polyaryl ether-polyalkylene oxide blocks.
摘要:
The present invention relates to the use of a molding composition for producing a feed container consisting essentially of a copolymer composed of (A) from 5 to 60% by weight of units of the formula (I) (B) from 40 to 95% by weight of units of the formula (II) where the total of the proportions by weight is 100% by weight, based on the copolymer, and where the demolding force of the molding composition is from 1800 to 2800 N.
摘要:
A thermoplastic molding composition, comprising: A) from 40 to 97.9% by weight of at least one polyether sulfone, B) from 2 to 59.9% by weight of at least one polysulfone, C) from 0.1 to 2% by weight of stearic acid, and also, if appropriate, further additives and auxiliaries, has improved flowability, surface quality, and notched impact resistance, and can be used for the construction of headlamps.