摘要:
The present invention relates to thermoplastic molding compositions comprising the following components: (A1) at least one polyarylene ether having an average of at most 0.5 phenolic end groups per polymer chain, (A2) optionally at least one polyarylene ether having an average of at least 1.5 phenolic end groups per polymer chain, (B) at least one polyarylene sulfide, (C) at least one hyperbranched polymer selected from hyperbranched polycarbonates and hyperbranched polyesters, (D) optionally at least one functionalized polyarylene ether comprising carboxy groups, (E) optionally at least one fibrous or particulate filler, and (F) optionally further additives and/or processing aids. The present invention further relates to a process for producing the thermoplastic molding compositions of the invention, to the use of these for producing moldings, fibers, foams, or films, and to the resultant moldings, fibers, foams, and films.
摘要:
The present invention relates to thermoplastic molding materials comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, (C) optionally at least one functionalized polyarylene ether comprising carboxyl groups, (D) at least one fibrous or particulate filler and (E) optionally further additives and/or processing assistants, the ratio of the apparent viscosity of the component (A) to that of the component (B), determined at 350° C. and a shear rate of 1150 s−1, being from 2.5 to 3.7.
摘要:
The present invention relates to thermoplastic molding materials comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, (C) at least one functionalized polyarylene ether comprising carboxyl groups having a viscosity number according to DIN EN ISO 1628-1 of 45 to 65 ml/g measured in 1% strength by weight solution in N-methyl-2-pyrrolidone at 25° C., (D) at least one fibrous or particulate filler and (E) optionally further additives and/or processing assistants. In addition, the present invention relates to a process for the preparation of the thermoplastic molding materials according to the invention, the use thereof for the production of shaped articles and the use of functionalized polyarylene ethers comprising carboxyl groups having a viscosity number according to DIN EN ISO 1628-1 of 45 to 65 ml/g measured in 1% strength by weight solution in N-methyl-2-pyrrolidone at 25° C. for increasing the elongation at break and for improving the impact strength.
摘要翻译:本发明涉及包含以下组分的热塑性模塑材料:(A)至少一种聚亚芳基醚,(B)至少一种聚芳硫醚,(C)至少一种官能化聚亚芳基醚,其含有根据DIN 在25℃下,在N-甲基-2-吡咯烷酮中的1重量%的重量溶液中测量的EN ISO 1628-1为45至65ml / g,(D)至少一种纤维或颗粒填料和(E)任选进一步 添加剂和/或加工助剂。 此外,本发明涉及一种制备本发明的热塑性成型材料的方法,其用于生产成型制品的用途,以及使用包含羧基的官能化聚亚芳基醚,其粘度值根据DIN EN 在25℃下在1-甲基-2-吡咯烷酮中的1重量%溶液中测量的ISO 1628-1为45至65ml / g,用于增加断裂伸长率和改善冲击强度。
摘要:
The present invention relates to thermoplastic molding materials comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, (C) optionally at least one functionalized polyarylene ether comprising carboxyl groups, (D) at least one fibrous or particulate filler and (E) optionally further additives and/or processing assistants, the ratio of the apparent viscosity of the component (A) to that of the component (B), determined at 350° C. and a shear rate of 1150 s−1, being from 2.5 to 3.7.
摘要:
The present invention relates to thermoplastic molding compositions comprising the following components: (A) at least one polyarylene ether (A1) having an average of at most 0.1 phenolic end group per polymer chain and at least one polyarylene ether (A2) having an average of at least 1.5 phenolic end groups per polymer chain, (B) at least one polyarylene sulfide, (C) at least one functionalized polyarylene ether comprising carboxy groups, (D) at least one fibrous or particulate filler, and (E) optionally further additives and/or processing aids. The present invention further relates to a process for producing the thermoplastic molding compositions of the invention, to the use of these for producing moldings, fibers, foams, or films, and to the resultant moldings, fibers, foams, and films.
摘要:
The present invention relates to compositions comprising the following components: (A) at least one polyarylene ether, (B) at least one polyarylene sulfide, and (C) at least one anhydride of a polybasic carboxylic acid with a number-average molar mass of at most 600 g/mol. The present invention moreover relates to the use of the abovementioned anhydrides of polybasic carboxylic acids in compositions comprising at least one polyarylene ether and at least one polyarylene sulfide.
摘要:
The present invention relates to thermoplastic molding compositions and moldings with improved wear resistance comprising at least one thermoplastic matrix M, at least one carbon reinforcing fiber F, at least one carbon component K; at least one silicate component S, where the at least one silicate component S comprises particles which have, in any particle dimension, a length/thickness ratio greater than or equal to 3, and at least one titanium dioxide T.
摘要:
The present invention relates to thermoplastic molding compositions and moldings with improved wear resistance comprising at least one thermoplastic matrix M, at least one carbon reinforcing fiber F, at least one carbon component K; at least one silicate component S, where the at least one silicate component S comprises particles which have, in any particle dimension, a length/thickness ratio greater than or equal to 3, and at least one titanium dioxide T.
摘要:
A thermoplastic molding composition, comprising: A) from 40 to 97.9% by weight of at least one polyether sulfone, B) from 2 to 59.9% by weight of at least one polysulfone, C) from 0.1 to 2% by weight of stearic acid, and also, if appropriate, further additives and auxiliaries, has improved flowability, surface quality, and notched impact resistance, and can be used for the construction of headlamps.
摘要:
A thermoplastic molding composition, comprising: A) from 40 to 97.9% by weight of at least one polyether sulfone, B) from 2 to 59.9% by weight of at least one polysulfone, C) from 0.1 to 2% by weight of stearic acid, and also, if appropriate, further additives and auxiliaries, has improved flowability, surface quality, and notched impact resistance, and can be used for the construction of headlamps.