Process for the production of stable dispersions, the dispersions so
produced, and the use thereof in the manufacture of polyurethanes
    2.
    发明授权
    Process for the production of stable dispersions, the dispersions so produced, and the use thereof in the manufacture of polyurethanes 失效
    用于生产稳定分散体的方法,如此制备的分散体及其在制备聚氨酯中的用途

    公开(公告)号:US4855352A

    公开(公告)日:1989-08-08

    申请号:US225403

    申请日:1988-07-28

    摘要: Stable finely-divided dispersions of polyureas and/or polyhydrazodicarbonamides in a hydroxyl-group-containing material are made by reacting (i) an isocyanate with (ii) a compound selected from polyamines, hydrazines, hydrazides and mixtures thereof in the presence of (iii) a hydroxyl compound selected from polyethers, polyesters, polyester amides, polycarbonates and mixtures thereof and (iv) a catalyst. The catalyst is a compound which catalyzes the reaction of isocyanate groups with hydroxyl groups. The catalyst is used in a quantity of at least 50 parts per million parts of (i), (ii) and (iii). These dispersions are particularly useful in the production of polyurethanes.

    摘要翻译: 通过使(i)异氰酸酯与(ii)选自多胺,肼,酰肼及其混合物的化合物在(iii)的存在下,使(ⅰ)异氰酸酯与(ⅱ)化合物反应,制备聚脲和/或聚肼基二酰胺在含羟基的材料中的稳定的微细分散体。 )选自聚醚,聚酯,聚酯酰胺,聚碳酸酯及其混合物的羟基化合物和(iv)催化剂。 催化剂是催化异氰酸酯基与羟基反应的化合物。 催化剂的用量至少为(i),(ii)和(iii)每百万份的50份。 这些分散体在聚氨酯的生产中特别有用。

    Stable dispersions and the manufacture thereof
    3.
    发明授权
    Stable dispersions and the manufacture thereof 失效
    稳定的分散体及其制造

    公开(公告)号:US4847320A

    公开(公告)日:1989-07-11

    申请号:US225691

    申请日:1988-07-28

    摘要: The present invention relates to a process for the production of stable dispersions of polyureas and/or polyhydrazodicarbonamides in a hydroxyl-group-containing material by reacting an organic di- or polyisocyanate with a composition selected from the group consisting of polyamines containing primary and/or secondary amine groups, hydrazines, hydrazides, and mixtures thereof, in said hydroxyl-group containing material, in the presence of a dispersion stabilizing compound.

    摘要翻译: 本发明涉及通过使有机二异氰酸酯或多异氰酸酯与选自以下的组合物反应制备聚脲和/或聚二酰二酰胺在含羟基材料中的稳定分散体的方法,所述组合物选自含有主要和/或 仲胺基,肼,酰肼及其混合物,在所述含羟基的物质中,在分散体稳定化合物的存在下。

    Polyols derived from 4,4,4-trichloro-1,2-epoxybutane and/or
epihalohydrin for use in the production of heat sealable foams
    5.
    发明授权
    Polyols derived from 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin for use in the production of heat sealable foams 失效
    衍生自4,4,4-三氯-1,2-环氧丁烷和/或表卤代醇的多元醇用于生产可热封泡沫

    公开(公告)号:US4282332A

    公开(公告)日:1981-08-04

    申请号:US146983

    申请日:1980-05-05

    摘要: The instant invention is directed to a polyol having a molecular weight of 2,000 to 8,000 which is especially suited for use in the production of heat sealable foams, comprising the adduct obtained by sequentially reacting:(a) a polyhydroxyl initiator, with a functionality of 2 to 5 and a weight average molecular weight as determined by gel permeation chromatography of from 62 to 200; with(b) 10 to 90%, by weight, based on the total oxide present in (b)+(c)+(d), a first alkylene oxide; and subsequently reacting the product with(c) 10 to 80%, by weight, based on the total oxide present in (b)+(c)+(d), 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin; and subsequently reacting the product with(d) 10 to 60%, by weight, based on the total oxide present in (b)+(c)+(d), a second alkylene oxide.

    摘要翻译: 本发明涉及分子量为2,000至8,000的多元醇,其特别适用于生产可热封泡沫体,该多元醇包括通过使(a)多羟基引发剂的官能度为2 至5,通过凝胶渗透色谱法测定的重均分子量为62至200; 与(b)+(c)+(d)中存在的总氧化物相比,(b)10〜90重量%的第一烯化氧; (c)+(d),4,4,4-三氯-1,2-环氧丁烷和(b)+(c)+(d))中存在的总氧化物和(c)10至80重量% /或表卤代醇; 然后使产物与(b)+(c)+(d)中存在的总氧化物的重量比为10至60重量%的第二烯化氧反应。

    Process for heat sealing polyurethane foam
    6.
    发明授权
    Process for heat sealing polyurethane foam 失效
    聚氨酯泡沫热封工艺

    公开(公告)号:US4302272A

    公开(公告)日:1981-11-24

    申请号:US112046

    申请日:1980-01-14

    摘要: The instant invention is directed to a process for heat sealing flexible polyurethane foam, comprising:A. reacting and foaming a polyurethane foam produced by the steps comprising reacting:(I) an organic polyisocyanate;(II) a polyol having a molecular weight of 2,000 to 8,000 comprising the adduct obtained by sequentially reacting:(a) a polyhydroxyl initiator, with a functionality of 2 to 5 and a weight average molecular weight as determined by gel permeation chromatography of from 62 to 200; with(b) 10 to 90%, most preferably 10 to 50%, by weight, based on the total oxide present in (b)+(c)+(d), a first alkylene oxide; and subsequently reacting the product with(c) 10 to 80%, preferably 20 to 50% by weight, based on the total oxide present in (b)+(c)+(d), 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin; and subsequently reacting the product with(d) 10 to 60%, most preferably 10 to 40%, by weight, based on the total oxide present in (b)+(c)+(d), a second alkylene oxide.(III) foaming agent; and optionally(IV) catalyst;B. heating a portion of the surface of said flexible polyurethane foam of (A) above its melting or fusion point; andC. cooling said flexible polyurethane foam below its melting or fusion point.

    摘要翻译: 本发明涉及一种用于热封柔性聚氨酯泡沫的方法,其包括:A.使由以下步骤制备的聚氨酯泡沫反应并发泡,所述步骤包括:(I)有机多异氰酸酯; (II)分子量为2,000至8,000的多元醇,其包含通过顺序地使以下反应获得的加合物:(a)通过凝胶渗透色谱法测定的官能度为2-5的多羟基引发剂和通过62测定的重均分子量 至200; 与(b)+(c)+(d)中存在的总氧化物相比,(b)10至90%,最优选10至50重量%的第一烯化氧; (c)+(d)中存在的总氧化物,4,4,4-三氯-1(ⅰ)和(c)+(d))中的总氧化物,随后使产物与(c)10至80重量%,优选20至50重量% ,2-环氧丁烷和/或表卤代醇; 然后使产物与(b)+(c)+(d)中存在的总氧化物,第二烯化氧反应,与(d)10至60重量%,最优选10至40重量%反应。 (三)发泡剂; 和任选的(Ⅳ)催化剂; B.将(A)的所述软质聚氨酯泡沫的表面的一部分加热到其熔点或熔点以上; 和C.将所述软质聚氨酯泡沫体冷却到低于其熔点或熔点。

    Aliphatic rim elastomers
    7.
    发明授权
    Aliphatic rim elastomers 失效
    脂肪族边缘弹性体

    公开(公告)号:US5502147A

    公开(公告)日:1996-03-26

    申请号:US171282

    申请日:1993-12-21

    摘要: The present invention is directed to polyurethane moldings produced via the RIM process. These polyurethane moldings have excellent reactivity, demold properties (at a 30 s demold), and good elongation and tear strength, and comprise the reaction product of an aliphatic polyisocyanate having a viscosity of less than about 20,000 mPa.multidot.s at 25.degree. C. and a NCO functionality of 2.3 to 4.0 with an isocyanatereactive component comprising b1) a relatively high molecular weight organic compound containing at least one of the groups selected from the group consisting of hydroxy groups and amine groups; and b2) a low molecular weight chain extender selected from the group consisting of diols, triols, primary amines, secondary amines, aminoalcohols, and mixtures thereof; in the presence of a catalyst. The OH:NH ratio of the chain extender is from 1:1 to 25:1.

    摘要翻译: 本发明涉及通过RIM工艺生产的聚氨酯模制品。 这些聚氨酯模制品具有优异的反应性,脱模性(30秒脱模)和良好的伸长率和撕裂强度,并且包括在25℃下具有小于约20,000mPax的粘度的脂族多异氰酸酯与NCO的反应产物 具有异氰酸酯反应性组分的2.3至4.0的官能度包含:b1)含有至少一种选自羟基和胺基的基团的相对高分子量的有机化合物; 和b2)选自二醇,三醇,伯胺,仲胺,氨基醇及其混合物的低分子量增链剂; 在催化剂存在下。 扩链剂的OH:NH比为1:1至25:1。

    Polyols derived from 4,4,4-trichloro-1,2-epoxybutane and/or
epihalohydrin for use in the production of heat sealable foams
    9.
    发明授权
    Polyols derived from 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin for use in the production of heat sealable foams 失效
    衍生自4,4,4-三氯-1,2-环氧丁烷和/或表卤代醇的多元醇用于生产可热封泡沫

    公开(公告)号:US4234745A

    公开(公告)日:1980-11-18

    申请号:US8147

    申请日:1979-01-31

    摘要: The instant invention is directed to a polyol having a molecular weight of 2,000 to 8,000 which is especially suited for use in the production of heat sealable foams, comprising the adduct obtained by sequentially reacting:(a) a polyhydroxyl initiator, with a functionality of 2 to 5 and a weight average molecular weight as determined by gel permeation chromatography of from 62 to 200; with(b) 10 to 90%, by weight, based on the total oxide present in (b)+(c)+(d), a first alkylene oxide; and subsequently reacting the product with(c) 10 to 80%, by weight, based on the total oxide present in (b)+(c)+(d), 4,4,4-trichloro-1,2-epoxybutane and/or epihalohydrin; and subsequently reacting the product with(d) 10 to 60%, by weight, based on the total oxide present in (b)+(c)+(d), a second alkylene oxide.

    摘要翻译: 本发明涉及分子量为2,000至8,000的多元醇,其特别适用于生产可热封泡沫体,该多元醇包括通过使(a)多羟基引发剂的官能度为2 至5,通过凝胶渗透色谱法测定的重均分子量为62至200; 与(b)+(c)+(d)中存在的总氧化物相比,(b)10〜90重量%的第一烯化氧; (c)+(d),4,4,4-三氯-1,2-环氧丁烷和(b)+(c)+(d))中存在的总氧化物和(c)10至80重量% /或表卤代醇; 然后使产物与(b)+(c)+(d)中存在的总氧化物的重量比为10至60重量%的第二烯化氧反应。