摘要:
The present disclosure is directed to polymeric compositions and methods for making the same. The polymeric composition includes a clarified polypropylene and a plurality of ethylene and alpha-olefin copolymers. The polymeric composition has low haze and exhibits increased impact strength when compared to clarified polypropylene.
摘要:
A lubricant composition comprises a base oil and a viscosity modifier including an ethylene/α-olefin interpolymer. The ethylene/α-olefin interpolymer is a block copolymer having at least a hard block and at least a soft block. The soft block comprises a higher amount of comonomers than the hard block. The block copolymer has a number of unique characteristics disclosed here. Such block copolymers offer the possibility of improved low temperature performance and flexibility in formulating motor oil, gear lubricants and greases, etc.
摘要:
A blend of polycarbonate and a homogeneously branched, linear ethylene polymer, which blend has a desirable balance of impact resistance and toughness properties.
摘要:
A method of improving the oxidative thermal stability of ethylene polymers is disclosed. The method comprises removing residual unreacted monomer(s), solvent and thermally unstable species from the molten polymer. The resulting polymer is characterized by having an oxidative exotherm of not more than about 50 percent of the original polymer, as measured by differential scanning calorimetry.
摘要:
Substantially linear ethylene polymers, e.g., polyethylenes prepared by constrained geometry catalysis (substantially linear ethylene), which are grafted with one or more unsaturated organic compounds containing both ethylenic unsaturation and a carbonyl group, e.g., maleic anhydride, exhibit desirable adhesive properties. These graft-modified substantially linear ethylene polymers also impart desirable compatibility and impact properties to various thermoplastic polymer blends.
摘要:
The foaming window for making a foam useful in the manufacture of artificial leather is expanded through the use of a foamable composition comprising (A) a propylene-α-olefin copolymer, (B) a molecular melt (MM) comprising 4,4′-oxydibenzenesulfonylazide (DPO-BSA) and an antioxidant, and (C) a blowing agent. The foaming window can be expanded such that foaming can occur at 220° C. for 20 to 200 or more seconds.
摘要:
The invention is related to an ethylene/α-olefin interpolymer having at least a hard segment and at least a soft segment. The soft segment contains a higher amount of comonomers than the hard segment. The hard segment has low crystallinity. The copolymer has a number of unique characteristics disclosed herein.ethylene/α-olefin interpolymers containing low crystallinity hard blocks
摘要:
A thermoplastic vulcanizate composition comprising from 5 wt % to 95 wt %, based on the total weight of the thermoplastic vulcanizate composition, of a first component comprising a first propylene-based polymer selected from the group consisting of (i) propylene/α-olefin copolymers comprising from 1 to 20 wt % α-olefin and characterized by a g′ ratio of less than 1, measured at interpolymer number average molecular weight (Mn), an MFR (2.16 kg @ 230° C.) greater than or equal to 0.01, a density greater than or equal to 0.850 g/cc, and a molecular weight distribution, Mw/Mn, less than or equal to 3.5, and (ii) combinations thereof; and from 5 wt % to 95 wt %, based on the total weight of the thermoplastic vulcanizate composition, of a second component selected from the group consisting of curable or vulcanizable rubbers, having a density from 0.85 to 0.88 g/cc, I2 from 0.001 to 5 g/10 min, and a Mooney viscosity from 5 to 400, and combinations thereof; wherein at least one of the rubbers is vulcanizable; wherein the thermoplastic vulcanizate composition has a tensile strength at break of greater than or equal to 8 MPa and tear strength at 23° C. of at least 190 lb-f/in. is provided. Methods of making the composition and articles made from the composition are also provided.
摘要:
A composition of matter particularly well suited for use as a peelable seal layer is described. The composition comprises from about 50 to about 85 percent by weight of a first polymer and from 15 to 50 percent of a second polymer. The first polymer is a propylene based polymer characterized by having a melting point of at least 125° C. together with a Comonomer Composition Distribution Breadth (“CCDB”) less than 2. The second polymer is characterized by having an interfacial adhesion with the first polymer of less than 1 lb/inch.