摘要:
A vinylidene chloride copolymer film having excellent bubble stability in an inflation-stretching process and excellent cold resistance is prepared by inflation-stretching a tubular amorphous substance obtained by melt-extruding and quenching a composition comprising vinylidene chloride copolymer, a miscible type elastomer (A component) and a particle dispersion type elastomer (B component) in a range surrounded by the lines (a), (b), (c) and (d) ##EQU1## WHEREIN A WEIGHT PERCENT OF THE B component to total elastomers is plotted on X axis (abscissa) and a weight percent of total content of the A component and the B component to total components is plotted on Y axis (ordinate).
摘要:
Food packaging-use formed articles including at least one layer of a 3 to 90 microns thickness which comprises a composition consisting of polyvinyl alcohol resin having a degree of saponification of 60 to 95 mole % (A) and a compound elected from a group of alkylene glycol polymer, etc. falling within the range of from 3 weight parts of (B) to 100 weight parts of (A) to the saturated solubility of (B) in (A) and having a carbon dioxide/oxygen solubility ratio (SCO.sub.2 /SO.sub.2) of 30 or higher.Furthermore, a resin composition consisting of the aforementioned (A), (B) and a saponified ethylene/vinylacetate copolymer resin (C) wherein the blending ratio of (B) is within the range of from 3 weight parts of (B) to 100 weight parts of (A) to the saturated solubility of (B) in (A), and the blending ratio of (C) being 20 to 50 weight parts of (C) to 100 weight parts of an aggregate of (A) and (C), and food packaging-use melt extruded articles containing at least one layer comprising the aforementioned composition.
摘要:
Food packaging-use formed articles including at least one layer of a 3 to 90 microns thickness which comprises a composition consisting of (A) polyvinyl alcohol resin having a degree of saponification of 60 to 95 mole % (A) and (B) a hydroxy containing compound falling within the range of from 3 weight parts of (B) to 100 weight parts of (A) to the saturated solubility of (B) in (A) and having a carbon dioxide/oxygen solubility ratio (SCO.sub.2 /SO.sub.2) of 30 or higher.
摘要:
Disclosed herein is a smokable food-packaging film comprising at least one layer of a mixture of 45 to 85 wt % polyamide, 10 to 45 wt % copolymer of olefin and vinyl alcohol, and 5 to 30 wt % polyolefin, in which the mixture falls in the pantagonal range defined in FIG. 1 by linear lines connecting the points A, B, C, D and E, respectively, said layer having the properties of a permability to 50% concentration of methanol of not less than 200 g/m.sup.2.day.atm at a temperature of 60.degree. C. and a relative humidity of 0% and an oxygen gas-permeability of not more than 50 cc/m.sup.2.day.atm at a temperature of 30.degree. C. and a relative humidity of 60% and a water vapor-transmission rate of not more than 70 g/m.sup.2.day at a temperature of 40.degree. C. and a relative humidity of 90%.
摘要翻译:本文公开了一种可吸收的食品包装膜,其包含至少一层45至85重量%的聚酰胺,10至45重量%的烯烃和乙烯醇的共聚物和5至30重量%的聚烯烃的混合物,其中混合物下降 在图3中限定的三角形范围内。 1,分别连接点A,B,C,D和E的线性线,所述层在60℃的温度下具有不低于200g / m 2·天的浓度的50%浓度的甲醇的性质 相对湿度为0%,氧气渗透率为50cc / m 2·天以上的温度为30℃,相对湿度为60%,水蒸气透过率 在40℃的温度和90%的相对湿度下不大于70g / m 2。
摘要:
Disclosed herein is a smokable food-packaging film comprising:at least one layer of a mixture of 50 to 80 wt % polyamide having a melting point of 120.degree. to 210.degree. C. and a recrystallization temperature of not lower than 50.degree. C. and 20 to 50 wt % .alpha.-olefin - vinyl alcohol copolymer, said film having properties of an initial stress of not higher than 0.6 Kg/mm.sup.2 at a 25% elongation, a transmission to 50% concentration of methanol of not less than 200 g/m.sup.2.day.atm at a temperature of 60.degree. C. and a relative humidity of 0%, and an oxygen gas-transmission of not more than 50 cc/m.sup.2.day.atm at a temperature of 30.degree. C. and a relative humidity of 60%, and the thickness of said film being 20 to 60 .mu.m.
摘要:
A laminated film containing at least two layers of which one layer is a gas-barriering layer comprising a copolymer of vinylidene chloride with a reduced viscosity of 0.030 to 0.050 and the other layer is a strengthening layer arranged to be adjacent to the gas-barriering layer, comprising a copolymer of vinylidene chloride with a reduced viscosity of 0.050 to 0.075.