Multilayer foil
    4.
    发明申请
    Multilayer foil 审中-公开
    多层箔

    公开(公告)号:US20070166560A1

    公开(公告)日:2007-07-19

    申请号:US10589264

    申请日:2005-06-09

    IPC分类号: B32B27/34

    摘要: An adhesion promoter which comprises from 2 to 100% by weight of a copolymer which contains the following monomer units: a) from 70 to 99.9% by weight of monomer units which derive from vinyl compounds selected from acrylic acid derivatives, methacrylic acid derivatives, and vinylaromatics, and also b) from 0.1 to 30% by weight of monomer units which contain a functional group selected from a carboxylic anhydride group, an epoxy group, and an oxazoline group, is used for production of a bond between I. a layer composed of a polyamide molding compound, and II. a part composed of an ABS molding composition.

    摘要翻译: 一种粘合促进剂,其包含2至100重量%的共聚物,其含有以下单体单元:a)70至99.9重量%的衍生自选自丙烯酸衍生物,甲基丙烯酸衍生物和乙烯基化合物的乙烯基化合物的单体单元 乙烯基芳族化合物,以及b)0.1〜30重量%的含有选自羧酸酐基团,环氧基和恶唑啉基团的官能团的单体单元用于生成I. 的聚酰胺模塑料,II。 由ABS成型组合物构成的部分。

    Process for producing moldings with an increase in the melt stiffness
    5.
    发明申请
    Process for producing moldings with an increase in the melt stiffness 有权
    具有增加熔体刚度的生产模制品的方法

    公开(公告)号:US20060183869A1

    公开(公告)日:2006-08-17

    申请号:US11354114

    申请日:2006-02-15

    IPC分类号: C08C19/24

    摘要: A process for producing moldings with condensing-up of a polyamide molding composition whose polyamide component contains, as a result of the method of preparation, at least 5 ppm of phosphorus in the form of an acidic compound by means of a compound having at least two carbonate units, wherein a) from 0.001 to 10% by weight, based on the polyamide, of a salt of a weak acid is added to the polyamide molding composition prior to compounding or during compounding, b) a mixture of the finished composition and the compound having at least two carbonate units is prepared, c) the mixture is, if appropriate, stored and/or transported and d) the mixture is subsequently processed to produce the molding, with the condensing-up occurring only in this step, effects a significant increase in the melt stiffness combined with moderate processing presssures, which considerably simplifies, in particular, the production of hollow bodies and hollow profiles having large diameters.

    摘要翻译: 一种聚酰胺成型组合物的制造用模制品的制造方法,其聚酰胺成分作为制备方法的结果,含有至少5ppm的酸性化合物形式的磷,该化合物具有至少两个 碳酸酯单元,其中a)基于聚酰胺的0.001至10重量%的弱酸盐在配混之前或在配混期间加入到聚酰胺模塑组合物中,b)成品组合物和 制备具有至少两个碳酸酯单元的化合物,c)如果合适的话,该混合物被储存和/或运输,以及d)随后将该混合物加工以产生模制物,其中仅在该步骤中发生冷凝, 结合中等加工压力的熔体刚度的显着增加,这特别地简化了具有大直径的中空体和中空型材的生产。

    Process for producing moldings with an increase in the melt stiffness
    6.
    发明授权
    Process for producing moldings with an increase in the melt stiffness 有权
    具有增加熔体刚度的生产模制品的方法

    公开(公告)号:US08647551B2

    公开(公告)日:2014-02-11

    申请号:US11354114

    申请日:2006-02-15

    摘要: A process for producing moldings with condensing-up of a polyamide molding composition whose polyamide component contains, as a result of the method of preparation, at least 5 ppm of phosphorus in the form of an acidic compound by means of a compound having at least two carbonate units, wherein a) from 0.001 to 10% by weight, based on the polyamide, of a salt of a weak acid is added to the polyamide molding composition prior to compounding or during compounding, b) a mixture of the finished composition and the compound having at least two carbonate units is prepared, c) the mixture is, if appropriate, stored and/or transported and d) the mixture is subsequently processed to produce the molding, with the condensing-up occurring only in this step, effects a significant increase in the melt stiffness combined with moderate processing pressures, which considerably simplifies, in particular, the production of hollow bodies and hollow profiles having large diameters.

    摘要翻译: 一种聚酰胺成型组合物的制造用模制品的制造方法,其聚酰胺成分作为制备方法的结果,含有至少5ppm的酸性化合物形式的磷,该化合物具有至少两个 碳酸酯单元,其中a)基于聚酰胺的0.001至10重量%的弱酸盐在配混之前或在配混期间加入到聚酰胺模塑组合物中,b)成品组合物和 制备具有至少两个碳酸酯单元的化合物,c)如果合适的话,该混合物被储存和/或运输,以及d)随后将该混合物加工以产生模制物,其中仅在该步骤中发生冷凝, 结合中等加工压力的熔体刚度的显着增加,这特别地简化了具有大直径的中空体和中空型材的生产。