BISPHENOL POLYETHER OLIGOMERS, METHODS OF MANUFACTURE, AND POLYCARBONATES MADE THEREFROM
    4.
    发明申请
    BISPHENOL POLYETHER OLIGOMERS, METHODS OF MANUFACTURE, AND POLYCARBONATES MADE THEREFROM 审中-公开
    双酚聚醚低聚物,制造方法和其制备的聚碳酸酯

    公开(公告)号:US20150183929A1

    公开(公告)日:2015-07-02

    申请号:US14143361

    申请日:2013-12-30

    CPC classification number: C08G64/06 C08G64/081 C08G64/12 C08G65/40 C08K5/524

    Abstract: A bisphenol polyether oligomer composition comprising greater than 90 wt. % of an oligomer of the formula wherein Ra, Rb, and Rc are each independently a C1-12 alkyl, C1-12 alkoxy, or C1-12 alkylarylene, each Xa is independently a single bond, —O—, —S—, —S(O)—, —S(O)2—, —C(O)—, or a C1-18 organic group, G is H or p, q, and t are each independently integers of 0 to 4, n is 1 to 10; and wherein the bisphenol polyether oligomer composition comprises: a total halide content of less than 1000 ppm, less than 1000 ppm of —CH2OH groups, less than 5 wt. % cyclic oligomers, and less than 100 ppm of a bisphenol of the formula wherein Ra, Rb, Xa, p and q are the same as in the oligomer.

    Abstract translation: 一种双酚聚醚低聚物组合物,其包含大于90wt。 %的下式的低聚物其中Ra,Rb和Rc各自独立地为C1-12烷基,C1-12烷氧基或C1-12烷基亚芳基,每个Xa独立地为单键,-O - , - S - , - -S(O) - , - S(O)2 - , - C(O) - 或C 1-18有机基团,G为H或p,q和t各自独立地为0至4的整数,n 是1到10; 并且其中所述双酚聚醚低聚物组合物包含:总卤化物含量小于1000ppm,小于1000ppm的-CH 2 OH基团,小于5wt。 %环状低聚物和小于100ppm的下式的双酚其中Ra,Rb,Xa,p和q与低聚物中相同。

    POLYARYL ETHER KETONE - POLYCARBONATE COPOLYMER BLENDS
    5.
    发明申请
    POLYARYL ETHER KETONE - POLYCARBONATE COPOLYMER BLENDS 审中-公开
    聚醚醚酮 - 聚碳酸酯共聚物共混物

    公开(公告)号:US20140024787A1

    公开(公告)日:2014-01-23

    申请号:US14035573

    申请日:2013-09-24

    Abstract: A polymer composition comprising a mixture of a) a first resin component comprising a polyaryl ether ketone, a polyaryl ketone, a polyether ketone, a polyether ether ketone, or a combination of two or more of the foregoing, and b) a second resin component comprising a specific type of copolycarbonate, wherein the mixture has at least two glass transition temperatures, as measured by ASTM method D5418, wherein the first glass transition temperature is from 120 to 160° C. and the second glass transition temperature is from 170 to 280° C. is disclosed. The compositions have improved properties such as improved load bearing capability at high temperature, better impact strength, and a high crystallization temperature.

    Abstract translation: 一种聚合物组合物,其包含a)包含聚芳基醚酮,聚芳基酮,聚醚酮,聚醚醚酮或两种或多种前述物质的组合的第一树脂组分的混合物,和b)第二树脂组分 包括特定类型的共聚碳酸酯,其中所述混合物具有通过ASTM方法D5418测量的至少两个玻璃化转变温度,其中第一玻璃化转变温度为120至160℃,第二玻璃化转变温度为170-280℃ °C。 组合物具有改进的性能,例如在高温下改善的承载能力,更好的冲击强度和高结晶温度。

    BLENDS OF POLYPHENYLENE ETHER SULFONE AND SILICONE POLYESTER CARBONATE
    8.
    发明申请
    BLENDS OF POLYPHENYLENE ETHER SULFONE AND SILICONE POLYESTER CARBONATE 有权
    聚苯乙烯醚和硅酮聚碳酸酯的混合物

    公开(公告)号:US20140039103A1

    公开(公告)日:2014-02-06

    申请号:US14047508

    申请日:2013-10-07

    CPC classification number: C08L81/06 C08L27/18 C08L71/08

    Abstract: Disclosed herein is a composition comprising a polyphenylene ether sulfone and a resorcinol based silicone aryl polyester carbonate copolymer wherein greater than or equal to 50 mol % of copolymer repeating units are ester units derived from resorcinol, based on the total molar amount of all repeating units in the polymer and wherein the blend has less than 1 weight percent polycarbonate, based on the total weight of the composition, has FAR 25.853 peak heat release of less than 60 KW/m2 and time to peak heat release of greater than or equal to 120 seconds.

    Abstract translation: 本文公开了包含聚苯醚砜和间苯二酚基硅酮芳基聚酯碳酸酯共聚物的组合物,其中大于或等于50摩尔%的共聚物重复单元是源自间苯二酚的酯单元,基于所有重复单元的总摩尔量 聚合物,其中共混物具有小于1重量%的聚碳酸酯,基于组合物的总重量,具有小于60KW / m 2的FAR 25.853峰值热释放和大于或等于120秒的时间到峰值热释放 。