公开(公告)号:US20220212991A1
公开(公告)日:2022-07-07
申请号:US17609091
申请日:2020-05-28
Applicant: SIKA TECHNOLOGY AG
Inventor: Thomas MOSER , Jürg STURZENEGGER , Fabio WÜRMLI , Steffen KELCH
Abstract: Methods including preparing a mixture including a binder composition containing at least one binder and at least one mineral filler, and curing the mixture to produce a material having improved electrical conductivity at 20° C., where at least 20% by weight of the at least one mineral filler is iron-containing slag.
-
公开(公告)号:US20170292050A1
公开(公告)日:2017-10-12
申请号:US15511340
申请日:2015-09-25
Applicant: SIKA TECHNOLOGY AG
Inventor: Urs BURCKHARDT , Steffen KELCH , Ursula STADELMANN
IPC: C09J175/08 , C08L75/08 , C08G18/71 , C08G18/48 , C08G18/75 , C08G18/83 , C08L63/00 , C09J163/00
CPC classification number: C09J175/08 , C08G18/4866 , C08G18/718 , C08G18/755 , C08G77/458 , C08G77/46 , C08G2190/00 , C08K5/5415 , C08K5/548 , C08L63/00 , C08L71/02 , C08L75/08 , C08L2205/03 , C09D175/08 , C09J163/00 , C09J183/12 , C08G18/10 , C08G18/289
Abstract: A two-component composition, containing at least one silane-group-containing polymer that is liquid at room temperature, at least one epoxide liquid resin, at least one polyetheramine, and at least one aminosilane or mercaptosilane. The composition has low odor, cures quickly and without blistering at room temperature, and, when cured, forms a tough elastic material of high strength, high adhesive force, and good thermal resistance that has no tendency toward yellowing or substrate discoloration. The composition is excellently suitable as a tough elastic adhesive for structural adhesive joints in the field of construction and in industrial production.
-
公开(公告)号:US20170240686A1
公开(公告)日:2017-08-24
申请号:US15518057
申请日:2015-10-13
Applicant: SIKA TECHNOLOGY AG
Inventor: Steffen MAIER , Dominik HUBER , Steffen KELCH
IPC: C08G18/50 , C08G18/76 , C08G18/73 , B29C73/02 , C08G18/10 , C09J175/02 , C09J5/00 , C08G18/79 , C08G18/48
CPC classification number: C08G18/5027 , B29C73/02 , B29K2075/02 , C08G18/10 , C08G18/12 , C08G18/324 , C08G18/482 , C08G18/4854 , C08G18/5024 , C08G18/6681 , C08G18/73 , C08G18/7664 , C08G18/797 , C09J5/00 , C09J175/02 , C09J2400/226 , C08G18/48
Abstract: The invention relates to compositions comprising at least one first and one second component; —the first component K1 comprising at least one di(aminobenzoate) ester A1 of formula (I) with an average molecular weight of 500 g/mol to 2000 g/mol, preferably 600 g/mol to 1500 g/mol and particularly preferred between 650 g/mol and 1300 g/mol, G being a divalent group derived from poly(tetramethylene oxide) diol, and —the second component K2 comprising at least one aromatic polyisocyanate B1 with an average molecular weight of 160 g/mol to 1100 g/mol, preferably 500 g/mol to 800 g/mol.
-
公开(公告)号:US20250162194A1
公开(公告)日:2025-05-22
申请号:US18835150
申请日:2023-01-25
Applicant: SIKA TECHNOLOGY AG , EMPA
Inventor: Steffen KELCH , Urs BURCKHARDT , Tim MAMIE , Ingo BURGERT , Philippe GRÖNQUIST , Sandro STUCKI , Andrea FRANGI , Stefan VÖGTLI
Abstract: A method of producing a laminate, wherein a wood body is provided, a curable composition in the liquid state is applied thereto, and the composition cures, wherein the composition contains at least one organic binder and at least 80% by weight of mineral fillers, based on the overall composition. The method enables permanent bonding of wood bodies and compositions that are based on organic binder and have a high content of mineral fillers. The laminates obtained from the method are comparatively lightweight, stable and durable, and are particularly suitable as sustainable components in building construction, especially as a roof element.
-
5.
公开(公告)号:US20190169354A1
公开(公告)日:2019-06-06
申请号:US16321072
申请日:2017-07-28
Applicant: SIKA TECHNOLOGY AG
Inventor: Steffen KELCH , Urs BURCKHARDT
IPC: C08G18/69 , C08G18/76 , C08G18/20 , C08G18/32 , C09J175/14
Abstract: A two-component polyurethane composition containing at least 55% by weight of polybutadiene polyols based on the total amount of all polyols having an average molecular weight of at least 500 g/mol, and at least one latent hardener, where the ratio of the number of reactive groups in the latent hardener to the number of OH groups present is in the range from 0.02 to 0.4. The composition has a long open time, blister-free curing, a very low glass transition temperature, high elasticity and surprisingly high strength which is very constant over a wide temperature range. Furthermore, it has very good adhesion to metallic and nonmetallic substrates, causing barely any stress cracks on glassy thermoplastics.
-
公开(公告)号:US20160090515A1
公开(公告)日:2016-03-31
申请号:US14891240
申请日:2014-05-14
Applicant: SIKA TECHNOLOGY AG
Inventor: Wolfgang ROOCK , Steffen KELCH , Andrea THOMAS
IPC: C09J175/08 , C08G18/69 , B32B37/12 , C09J175/12 , C09J5/00 , B32B7/12 , C08G18/76 , C08G18/66
CPC classification number: C09J175/08 , B32B7/12 , B32B37/12 , C08G18/3206 , C08G18/4812 , C08G18/482 , C08G18/4829 , C08G18/4879 , C08G18/5021 , C08G18/6674 , C08G18/69 , C08G18/698 , C08G18/7671 , C09J5/00 , C09J175/04 , C09J175/12 , C09J2475/00
Abstract: The invention relates to a polyurethane composition comprising one first component and one second component, said first component comprising an alkoxylated aromatic diol, a low molecular aliphatic or cycloaliphatic diol, a specific polybutadiene polyol and a specific polyetherpolyol, in specific ratios. The hardened composition is characterized by having good adhesion characteristics, a resistance which is only slightly dependent on the temperature, in the temperature range of −35 to +85° C. and also very high resistances. It is particularly suitable as a structural adhesive for bonding two substrates.
Abstract translation: 本发明涉及包含一种第一组分和一种第二组分的聚氨酯组合物,所述第一组分以特定比例包含烷氧基化芳族二醇,低分子脂族或脂环族二醇,特定聚丁二烯多元醇和特定聚醚多元醇。 硬化组合物的特征在于在-35至+ 85℃的温度范围内具有良好的粘附特性,仅稍微取决于温度的电阻,并且还具有非常高的电阻。 特别适用于粘合两种基材的结构粘合剂。
-
公开(公告)号:US20160068724A1
公开(公告)日:2016-03-10
申请号:US14785098
申请日:2014-05-14
Applicant: SIKA TECHNOLOGY AG
Inventor: Wolfgang ROOCK , Steffen KELCH , Matthias HEIDTMANN
IPC: C09J175/14 , B32B7/12 , C09D175/14
CPC classification number: C09J175/14 , B32B7/12 , B32B2250/02 , B32B2255/26 , C08G18/3206 , C08G18/3215 , C08G18/6588 , C08G18/69 , C09D175/14 , C09J175/04
Abstract: The present invention relates to a polyurethane composition consisting of a first and a second component, wherein the first component comprises an alkoxylated aromatic diol, a low molecular weight aliphatic or cycloaliphatic diol and a specific polybutadiene polyol in specific ratios. The cured composition is characterized by having good adhesive characteristics, a strength that is only slightly dependent upon the temperature in the temperature range of −35 to +85° C. and high strength and elasticity. It is particularly suitable as a structural adhesive for bonding two substrates.
Abstract translation: 本发明涉及由第一和第二组分组成的聚氨酯组合物,其中第一组分包含烷氧基化芳族二醇,低分子量脂族或脂环族二醇和特定比例的特定聚丁二烯多元醇。 固化的组合物的特征在于具有良好的粘合特性,强度仅在-35至+ 85℃的温度范围内的温度稍微取决于高强度和弹性。 特别适用于粘合两种基材的结构粘合剂。
-
公开(公告)号:US20160053147A1
公开(公告)日:2016-02-25
申请号:US14779847
申请日:2014-05-14
Applicant: SIKA TECHNOLOGY AG
Inventor: Steffen KELCH , Wolfgang ROOCK , Florian ITTRICH
IPC: C09J175/12 , B32B37/12 , B32B43/00 , B32B27/38 , B32B9/00 , B32B17/06 , B32B27/18 , B32B7/12 , B32B15/04
CPC classification number: C09J175/12 , B32B7/12 , B32B9/005 , B32B15/04 , B32B17/06 , B32B27/18 , B32B27/38 , B32B37/12 , B32B43/006 , B32B2037/1253 , B32B2037/1269 , B32B2255/26 , B32B2260/04 , B32B2311/00 , B32B2315/02 , B32B2315/08 , B32B2363/00 , B32B2398/00 , B65D81/325 , C08G18/10 , C08G18/2081 , C08G18/324 , C08G18/4812 , C08G18/4841 , C08G18/4854 , C08G18/724 , C08G18/792 , C08G18/797 , C09J5/00 , C09J175/08 , C09J2475/00 , C09J2475/003 , C08G18/12 , C08G18/6685
Abstract: The present invention relates to a two-component polyurethane adhesive consisting of a polyol component and a polyisocyanate component, wherein the polyol component comprises a triol with a molar mass of 1,000 to 10,000 g/mol, a diol having two primary hydroxy groups and a molar mass of 60 to 150 g/mol, a poly(trimethylene oxide) diol or a poly(tetramethylene oxide) diol with a molar mass of 200 to 3,000 g/mol and an aliphatic polyamine. The adhesive is characterized by high early strength, a low temperature dependence of the mechanical properties, good adhesion and the possibility of controlled thermally induced release of adhesion.
Abstract translation: 本发明涉及由多元醇组分和多异氰酸酯组分组成的双组分聚氨酯粘合剂,其中多元醇组分包括摩尔质量为1,000至10,000g / mol的三醇,具有两个伯羟基的二醇和摩尔 质量为60〜150g / mol,聚(三亚甲基氧化物)二醇或摩尔质量为200〜3,000g / mol的聚(四氢呋喃)二醇和脂族多胺。 粘合剂的特征在于高的早期强度,机械性能的低温依赖性,良好的粘合性和受控的热诱导的粘附释放的可能性。
-
公开(公告)号:US20250019558A1
公开(公告)日:2025-01-16
申请号:US18714284
申请日:2022-11-23
Inventor: Urs BURCKHARDT , Ingo BURGERT , Fabien CHOFFAT , Philippe GRÖNQUIST , Steffen KELCH , Sanja KOSTIC , Tim MAMIE , Klaas MENNECKE , Ursula STADELMANN , Stefan VÖGTLI , Andrea FRANGI , Sandro STUCKI
IPC: C09D15/00 , C04B28/04 , C04B111/00 , C09D5/00 , C09D163/00
Abstract: A method for producing a laminate, wherein a wooden element is provided, the wooden element is coated on the top side with a an adhesive that is applied in liquid form and includes at least one polymer that is liquid at room temperature and contains silane groups, at least one liquid epoxy resin and at least one amine hardener, the applied adhesive is covered with a layer of a liquid cementitious composition while still wet, and the liquid cementitious composition and the adhesive each cure. The method enables the durable joining of wooden elements and cementitious elements in an easy-to-implement, wet-on-wet method. The laminates obtained from the method are comparatively light, stable and robust and are especially suitable as sustainable components in above-ground construction.
-
公开(公告)号:US20230339813A1
公开(公告)日:2023-10-26
申请号:US18026712
申请日:2021-11-22
Applicant: SIKA TECHNOLOGY AG
Inventor: Steffen KELCH , Tim MAMIE
CPC classification number: C04B26/16 , C04B14/047 , C04B14/28 , C04B22/142 , C04B14/06 , C04B40/065 , C04B38/10 , C04B38/0051 , C04B2103/465
Abstract: The use of a desiccant for influencing the density of a curable binder composition including a) at least one organic binder including a polyisocyanate and a polyol, and b) at least 50% by weight of an inorganic filler F, more particularly in the form of quartz aggregates and/or slag, the proportions by weight being based on 100% by weight of the binder composition.
-
-
-
-
-
-
-
-
-