THERMOPLASTIC COMPOSITIONS AND ARTICLES FORMED FROM THE SAME
    1.
    发明申请
    THERMOPLASTIC COMPOSITIONS AND ARTICLES FORMED FROM THE SAME 审中-公开
    热塑性组合物及其形成的制品

    公开(公告)号:US20130203939A1

    公开(公告)日:2013-08-08

    申请号:US13643178

    申请日:2011-05-19

    IPC分类号: C08L27/24

    摘要: The invention provides a composition comprising the following: A) a chlorinated ethylene-based polymer; and B) an ethylene-based polymer; and wherein the total chlorine content of the composition is greater than, or equal to, 13 weight percent, based on the total weight of polymers in the composition.

    摘要翻译: 本发明提供了包含以下物质的组合物:A)氯化乙烯类聚合物; 和B)乙烯类聚合物; 并且其中组合物的总氯含量基于组合物中聚合物的总重量大于或等于13重量%。

    Monovinylidene aromatic polymers with improved toughness and rigidity and a process for their preparation
    3.
    发明授权
    Monovinylidene aromatic polymers with improved toughness and rigidity and a process for their preparation 失效
    具有改善韧性和刚性的单亚乙烯基芳族聚合物及其制备方法

    公开(公告)号:US06444752B1

    公开(公告)日:2002-09-03

    申请号:US09852198

    申请日:2001-05-09

    IPC分类号: C08F27902

    摘要: Disclosed are rubber-modified monovinylidene aromatic polymers with improved toughness and rigidity as well as a process for the preparation thereof. The polymer comprises: a) a monovinylidene aromatic polymer matrix, b) rubber particles dispersed therein, characterized in that the rubber particles are produced from a diene rubber having I) from 20 to 80 percent, based on the total weight of said rubber particles, of a high solution viscosity component having a viscosity value ranging from 110 to 500 centipoise and II) from 80 to 20 percent, based on the total weight of said rubber particles, of a low solution viscosity component having a viscosity value ranging from 1 to 100 centipoise, further characterized in that the ratio of solution viscosity of high solution viscosity component to the solution viscosity of low solution viscosity ranges from 1.1 to 500, wherein both components I and II have a 1,4 cis content of greater than 30 percent, and III) the rubber is grafted with monovinylidene aromatic polymer to the extent that there is at least 30 percent monovinylidene aromatic polymer present as grafts on the rubber.

    摘要翻译: 公开了具有改进的韧性和刚性的橡胶改性的单亚乙烯基芳族聚合物以及其制备方法。 聚合物包括:a)单亚乙烯基芳族聚合物基体,b)分散在其中的橡胶颗粒,其特征在于,所述橡胶颗粒由二烯橡胶制成,所述二烯橡胶的I)为20-80重量%,基于所述橡胶颗粒的总重量, 具有粘度值为110-500厘泊的高溶液粘度组分和II。基于所述橡胶颗粒总重量的80%至20%的粘度值范围为1至100的低溶液粘度组分 其特征在于,高溶液粘度组分的溶液粘度与低溶液粘度的溶液粘度的比例为1.1至500,其中组分I和II均具有大于30%的1,4-顺式含量,以及 III)橡胶用单亚乙烯基芳族聚合物接枝至至少30%的单亚乙烯基芳族聚合物作为橡胶上的接枝物存在的程度。

    Compositions, Methods of Making the Same, and Articles Prepared from the Same
    5.
    发明申请
    Compositions, Methods of Making the Same, and Articles Prepared from the Same 审中-公开
    组合,制作方法及其制备方法

    公开(公告)号:US20130316111A1

    公开(公告)日:2013-11-28

    申请号:US13991545

    申请日:2011-12-29

    IPC分类号: C08L47/00

    摘要: A composition comprising at least the following components: (A) a first composition comprising the following: i) a first interpolymer comprising, in polymerized form, ethylene, an α-olefin, and a nonconjugated polyene; ii) a second interpolymer comprising, in polymerized form, ethylene, an α-olefin and a nonconjugated polyene; and wherein the first composition has an MWD less than, or equal to, 3.5, a Mooney Viscosity (ML (1+4 @125° C.)) greater than, or equal to, 80, and an [(ML(1+4 @125° C.))/Mw(conv)]*1000 greater than 0.429 mole/g; (B) a thermoplastic polymer; and (C) a vulcanization agent is provided. A crosslinked composition made by heating one or more of the inventive compositions is also provided. Articles made from one or more of the inventive compositions are also provided.

    摘要翻译: 至少包含以下组分的组合物:(A)包含以下物质的第一组合物:i)以聚合形式包含乙烯,α-烯烃和非共轭多烯的第一共聚体; ii)以聚合形式包含乙烯,α-烯烃和非共轭多烯的第二共聚体; 并且其中第一组合物的MWD小于或等于3.5,大于或等于80的门尼粘度(ML(1 + 4 @ 125℃))和[(ML(1+ 4 @ 125℃))/ Mw(conv)] * 1000大于0.429摩尔/ g; (B)热塑性聚合物; 和(C)硫化剂。 还提供了通过加热一种或多种本发明组合物制备的交联组合物。 还提供了由一种或多种本发明组合物制成的制品。

    HIGH FREQUENCY WELDABLE POLYOLEFIN COMPOSITIONS INCLUDING POLAR POLYMERS
    9.
    发明申请
    HIGH FREQUENCY WELDABLE POLYOLEFIN COMPOSITIONS INCLUDING POLAR POLYMERS 审中-公开
    高频焊接聚烯烃组合物,包括极性聚合物

    公开(公告)号:US20140364572A1

    公开(公告)日:2014-12-11

    申请号:US14367660

    申请日:2012-12-21

    IPC分类号: C08L23/14 B29C65/14 C08L23/20

    摘要: A polyolefin-based composition showing improved weldability using high frequency (HF) includes (1) a base polymer selected from (a) a homogeneously branched, linear or substantially linear ethylene/α-olefin copolymer; (b) a homogeneously branched propylene/α-olefin copolymer; or (c) a combination thereof; and (2) at least one secondary component selected from (a) an ethylene vinyl acetate copolymer having from 5 to 40 wt % vinyl acetate; (b) an ethylene-ethyl acrylate having from 5 to 25 wt % ethyl acrylate; and (c) a combination thereof. The combination of the specified polyolefin with the specified secondary component, which is a polar polymer, makes these formulations HF weldable, with a cohesive welding failure, a weld strength for 10 mil thick film greater than 7 lb/in (1.23 N/mm) at a weld time of less than or equal to 6 seconds. The formulations may also exhibit good calendering processability and mechanical properties.

    摘要翻译: 使用高频(HF)显示出改进的焊接性的聚烯烃基组合物包括(1)选自(a)均匀支化的,直链的或基本上线性的乙烯/α-烯烃共聚物的基础聚合物; (b)均匀支化的丙烯/α-烯烃共聚物; 或(c)其组合; 和(2)至少一种选自(a)乙烯 - 乙酸乙烯酯共聚物的次要组分,其具有5至40重量%的乙酸乙烯酯; (b)具有5至25重量%丙烯酸乙酯的乙烯 - 丙烯酸乙酯; 和(c)其组合。 指定的聚烯烃与作为极性聚合物的规定的次要组分的组合使得这些配方HF可焊接,具有内聚焊接故障,10密耳厚膜的焊接强度大于7lb / in(1.23N / mm) 在焊接时间小于或等于6秒。 制剂还可以表现出良好的压延加工性能和机械性能。