Method of Making a Trihalosilane
    1.
    发明申请
    Method of Making a Trihalosilane 有权
    制备三氯硅烷的方法

    公开(公告)号:US20130251617A1

    公开(公告)日:2013-09-26

    申请号:US13877909

    申请日:2011-12-13

    IPC分类号: C01B33/107

    CPC分类号: C01B33/1071 C01B33/107

    摘要: A method of making a trihalosilane comprising contacting an organotrihalosilane according to the formula RS1X3 (I), wherein R is C1-C10 hydrocarbyl and each X independently is halo, with hydrogen, wherein the mole ratio of the organotrihalosilane to hydrogen is from 0.009:1 to 1:2300, in the presence of a catalyst comprising a metal selected from (i) Re, (ii) a mixture comprising Re and at least one element selected from Pd, Ru, Mn, Cu, and Rh, (iii) a mixture comprising Ir and at least one element selected from Pd and Rh, (iv) Mn, (v) a mixture comprising Mn and Rh, (vi) Ag, (vii) Mg, and (viii) Rh at from 300 to 800° C. to form a trihalosilane.

    摘要翻译: 一种制备三卤代硅烷的方法,其包括使式RS1X3(Ⅰ)的有机三卤硅烷与其中R为C1-C10烃基并且每个X独立地为卤素与有机三卤代硅烷与氢的摩尔比为0.009:1 在包含选自(i)Re,(ii)包含Re和至少一种选自Pd,Ru,Mn,Cu和Rh的元素的混合物的催化剂存在下,(iii)a 包含Ir和选自Pd和Rh中的至少一种元素的混合物,(iv)Mn,(v)包含Mn和Rh的混合物,(vi)Ag,(vii)Mg和(viii)Rh在300至800℃ C.形成三卤硅烷。

    Method of making a trihalosilane
    2.
    发明授权
    Method of making a trihalosilane 有权
    制备三卤代硅烷的方法

    公开(公告)号:US08697022B2

    公开(公告)日:2014-04-15

    申请号:US13877909

    申请日:2011-12-13

    IPC分类号: C01B33/08

    CPC分类号: C01B33/1071 C01B33/107

    摘要: A method of making a trihalosilane comprising contacting an organotrihalosilane according to the formula RS1X3 (I), wherein R is C1-C10 hydrocarbyl and each X independently is halo, with hydrogen, wherein the mole ratio of the organotrihalosilane to hydrogen is from 0.009:1 to 1:2300, in the presence of a catalyst comprising a metal selected from (i) Re, (ii) a mixture comprising Re and at least one element selected from Pd, Ru, Mn, Cu, and Rh, (iii) a mixture comprising Ir and at least one element selected from Pd and Rh, (iv) Mn, (v) a mixture comprising Mn and Rh, (vi) Ag, (vii) Mg, and (viii) Rh at from 300 to 800° C. to form a trihalosilane.

    摘要翻译: 一种制备三卤代硅烷的方法,其包括使式RS1X3(Ⅰ)的有机三卤硅烷与其中R为C1-C10烃基并且每个X独立地为卤素与有机三卤代硅烷与氢的摩尔比为0.009:1 在包含选自(i)Re,(ii)包含Re和至少一种选自Pd,Ru,Mn,Cu和Rh的元素的混合物的催化剂存在下,(iii)a 包含Ir和选自Pd和Rh中的至少一种元素的混合物,(iv)Mn,(v)包含Mn和Rh的混合物,(vi)Ag,(vii)Mg和(viii)Rh在300至800℃ C.形成三卤硅烷。

    Method for forming activated copper oxide catalysts
    4.
    发明申请
    Method for forming activated copper oxide catalysts 有权
    形成活性氧化铜催化剂的方法

    公开(公告)号:US20070014711A1

    公开(公告)日:2007-01-18

    申请号:US11370843

    申请日:2006-03-09

    IPC分类号: B01D53/86 A24D3/00

    摘要: A method for forming a copper oxide catalyst includes forming a precipitate of copper hydroxide from a copper salt solution; forming dried particles of copper hydroxide by drying the precipitate at a temperature of less than 30° C.; heating the copper hydroxide particles to form copper oxide; and activating the copper oxide. The copper oxide catalyst includes particles of copper oxide. Copper oxide catalyst particles can preferably include a metastable form of copper oxide. The copper oxide catalyst particles are useful for low-temperature and near-ambient temperature catalysis and/or oxidation of carbon monoxide to carbon dioxide.

    摘要翻译: 形成氧化铜催化剂的方法包括由铜盐溶液形成氢氧化铜沉淀物; 通过在低于30℃的温度下干燥沉淀物来形成氢氧化铜的干燥颗粒; 加热氢氧化铜颗粒形成氧化铜; 并激活氧化铜。 氧化铜催化剂包括氧化铜颗粒。 氧化铜催化剂颗粒可以优选包括亚稳态形式的氧化铜。 氧化铜催化剂颗粒可用于低温和近环境温度的催化和/或一氧化碳氧化成二氧化碳。

    Method for forming activated copper oxide catalysts
    6.
    发明授权
    Method for forming activated copper oxide catalysts 有权
    形成活性氧化铜催化剂的方法

    公开(公告)号:US07744846B2

    公开(公告)日:2010-06-29

    申请号:US11370843

    申请日:2006-03-09

    IPC分类号: C01G3/02 B01J23/72

    摘要: A method for forming a copper oxide catalyst includes forming a precipitate of copper hydroxide from a copper salt solution; forming dried particles of copper hydroxide by drying the precipitate at a temperature of less than 30° C.; heating the copper hydroxide particles to form copper oxide; and activating the copper oxide. The copper oxide catalyst includes particles of copper oxide. Copper oxide catalyst particles can preferably include a metastable form of copper oxide. The copper oxide catalyst particles are useful for low-temperature and near-ambient temperature catalysis and/or oxidation of carbon monoxide to carbon dioxide.

    摘要翻译: 形成氧化铜催化剂的方法包括由铜盐溶液形成氢氧化铜沉淀物; 通过在低于30℃的温度下干燥沉淀物来形成氢氧化铜的干燥颗粒; 加热氢氧化铜颗粒形成氧化铜; 并激活氧化铜。 氧化铜催化剂包括氧化铜颗粒。 氧化铜催化剂颗粒可以优选包括亚稳态形式的氧化铜。 氧化铜催化剂颗粒可用于低温和近环境温度的催化和/或一氧化碳氧化成二氧化碳。