摘要:
A method of manufacturing a reflection type mask blank by forming a multilayer reflection film reflecting exposure light on a substrate and forming an absorber layer absorbing the exposure light on the multilayer reflection film includes a step of forming, between the substrate and the multilayer reflection film, a stress correction film opposite in direction to film stress of the multilayer reflection film and smaller in absolute value than the film stress of the multilayer reflection film, a step of heat-treating the stress correction film, and a step of heat-treating the multilayer reflection film.
摘要:
A multilayer-reflection-film-coated substrate includes a substrate, a multilayer reflection film formed on the substrate and reflecting an exposure light, and a conductive film formed on an opposite side of the substrate from the multilayer reflection film in a region excluding at least a peripheral portion of the substrate. The conductive film is made of a material containing chromium (Cr). The conductive film contains nitrogen (N) on a substrate side and at least one of oxygen (O) and carbon (C) on a surface side. A reflection type mask blank for exposure is obtained by forming an absorber film for absorbing the exposure light on the multilayer reflection film of the multilayer-reflection-film-coated substrate. A reflection type mask is obtained by forming a pattern on the absorber film of the reflection type mask blank for exposure.
摘要:
A method of manufacturing a reflection type mask blank by forming a multilayer reflection film reflecting exposure light on a substrate and forming an absorber layer absorbing the exposure light on the multilayer reflection film includes a step of forming, between the substrate and the multilayer reflection film, a stress correction film opposite in direction to film stress of the multilayer reflection film and smaller in absolute value than the film stress of the multilayer reflection film, a step of heat-treating the stress correction film, and a step of heat-treating the multilayer reflection film.
摘要:
A reflective mask blank and a reflective mask each have, on a multilayer reflective film, a protective film that protects the multilayer reflective film from etching during pattern formation of an absorber layer or a buffer layer formed on the protective film. The protective film is formed by a ruthenium compound containing ruthenium (Ru) and at least one selected from the group consisting of molybdenum (Mo), niobium (Nb), zirconium (Zr), yttrium (Y), boron (B), titanium (Ti), and lanthanum (La). A reflection enhancement film of Ru may be further formed on the surface of the protective film.
摘要:
A reflective mask blank has a substrate (11) on which a reflective layer (12) for reflecting exposure light in a short-wavelength region including an extreme ultraviolet region and an absorber layer (16) for absorbing the exposure light are successively formed. The absorber layer (16) has an at least two-layer structure including as a lower layer an exposure light absorbing layer (14) formed by an absorber for the exposure light in the short-wavelength region including the extreme ultraviolet region and as an upper layer a low-reflectivity layer (15) formed by an absorber for inspection light used in inspection of a mask pattern. The upper layer is made of a material containing tantalum (Ta), boron (B), and nitrogen (N). The content of B is 5 at % to 30 at %. The ratio of Ta and N (Ta:N) falls within a range of 8:1 to 2:7. Alternatively, the reflective mask blank has a substrate on which a multilayer reflective film and an absorber layer are successively formed. In this case, the absorber layer is made of a material containing tantalum (Ta), boron (B), and nitrogen (N). The content of B is 5 at % to 25 at %. The ratio of Ta and N (Ta:N) falls within a range of 8:1 to 2:7.
摘要:
A reflective mask blank and a reflective mask each have, on a multilayer reflective film, a protective film that protects the multilayer reflective film from etching during pattern formation of an absorber layer or a buffer layer formed on the protective film. The protective film is formed by a ruthenium compound containing ruthenium (Ru) and at least one selected from the group consisting of molybdenum (Mo), niobium (Nb), zirconium (Zr), yttrium (Y), boron (B), titanium (Ti), and lanthanum (La). A reflection enhancement film of Ru may be further formed on the surface of the protective film.
摘要:
A reflective mask blank has a substrate (11) on which a reflective layer (12) for reflecting exposure light in a short-wavelength region including an extreme ultraviolet region and an absorber layer (16) for absorbing the exposure light are successively formed. The absorber layer (16) has an at least two-layer structure including as a lower layer an exposure light absorbing layer (14) formed by an absorber for the exposure light in the short-wavelength region including the extreme ultraviolet region and as an upper layer a low-reflectivity layer (15) formed by an absorber for inspection light used in inspection of a mask pattern. The upper layer is made of a material containing tantalum (Ta), boron (B), and nitrogen (N). The content of B is 5 at % to 30 at %. The ratio of Ta and N (Ta:N) falls within a range of 8:1 to 2:7. Alternatively, the reflective mask blank has a substrate on which a multilayer reflective film and an absorber layer are successively formed. In this case, the absorber layer is made of a material containing tantalum (Ta), boron (B), and nitrogen (N). The content of B is 5 at % to 25 at %. The ratio of Ta and N (Ta:N) falls within a range of 8:1 to 2:7.
摘要:
A reflective mask blank has a substrate (11) on which a reflective layer (12) for reflecting exposure light in a short-wavelength region including an extreme ultraviolet region and an absorber layer (16) for absorbing the exposure light are successively formed. The absorber layer (16) has an at least two-layer structure including as a lower layer an exposure light absorbing layer (14) formed by an absorber for the exposure light in the short-wavelength region including the extreme ultraviolet region and as an upper layer a low-reflectivity layer (15) formed by an absorber for inspection light used in inspection of a mask pattern. The upper layer is made of a material containing tantalum (Ta), boron (B), and nitrogen (N). The content of B is 5 at % to 30 at %. The ratio of Ta and N (Ta:N) falls within a range of 8:1 to 2:7. Alternatively, the reflective mask blank has a substrate on which a multilayer reflective film and an absorber layer are successively formed. In this case, the absorber layer is made of a material containing tantalum (Ta), boron (B), and nitrogen (N). The content of B is 5 at % to 25 at %. The ratio of Ta and N (Ta:N) falls within a range of 8:1 to 2:7.
摘要:
In a reflection type mask blank for EUV exposure, a multilayer film is formed on a substrate to reflect EUV light. An intermediate layer is formed on the multilayer film. An absorber layer is formed on the intermediate layer to absorb the EUV light. The intermediate layer is formed by a material containing Cr and at least one element selected from the group consisting of N, O, and C.
摘要:
In a reflection type mask blank for EUV exposure with a substrate, a multilayer film is formed on the substrate so as to reflect an EUV light ray. A light absorber layer is formed on the multilayer film so as to absorb the EUV light ray. The multilayer film has flatness with respect to a surface thereof, and the flatness is 100 nm or less.