摘要:
An oxide superconducting thin film wherein nanoparticles functioning as flux pins are dispersed in the film is provided. The oxide superconducting thin film wherein the nanoparticles in the oxide superconducting thin film have a dispersing density of 1020 particles/m3 to 1024 particles/m3 is provided. The oxide superconducting thin film wherein the nanoparticles have a particle diameter of 5 nm to 100 nm is provided. A method of manufacturing an oxide superconducting thin film wherein a predetermined amount of a solution obtained by dissolving nanoparticles functioning as flux pins in a solvent is added to a solution obtained by dissolving an organometallic compound in a solvent to prepare a source material solution for an oxide superconducting thin film, and the source material solution is used to manufacture the oxide superconducting thin film through a coating-pyrolysis process is provided.
摘要翻译:提供了其中作为磁通引脚的纳米颗粒分散在膜中的氧化物超导薄膜。 提供氧化物超导薄膜中的氧化物超导薄膜的分散密度为1020粒子/ m 3至1024个/ m3的氧化物超导薄膜。 提供其中纳米颗粒具有5nm至100nm的粒径的氧化物超导薄膜。 一种制造氧化物超导薄膜的方法,其中将通过将用作助熔剂针的纳米颗粒溶解在溶剂中而获得的预定量的溶液加入到通过将有机金属化合物溶解在溶剂中而获得的溶液中,以制备用于氧化物的源材料溶液 超导薄膜和源材料溶液用于通过涂层热解制备氧化物超导薄膜。
摘要:
A process for forming a dense, epitaxial metal oxide film on a single crystal substrate, including cleaning the surface of the single crystal substrate, contacting the cleaned surface with a polar organic compound such as a small molecular weight alcohol, so that the cleaned surface adsorbs the polar organic compound, then applying a hydrocarbon solvent solution containing at least one organic group-containing metal compound on the polar organic compound-adsorbed surface, and then heating the substrate to decompose the organic group-containing metal compound and to form a dense epitaxial metal oxide film on the substrate.
摘要:
Provided is a coating solution where, upon producing a rare-earth superconductive composite metal oxide film by means of a coating-pyrolysis method, cracks are not generated in the heat treatment process for eliminating organic components, even when the thickness of the rare-earth superconductive film produced in a single coating is 500 nm or more, and without having to repeat the coating and annealing process. A solution for producing a rare-earth superconductive film which is made into a homogeneous solution by dissolving, in a solvent formed by adding a polyhydric alcohol to a univalent linear alcohol having a carbon number of 1 to 8 and/or water, a metal complex coordinated, relative to metal ions of a metallic species containing rare-earth elements, barium and copper, with pyridine and/or at least one type of tertiary amine, at least one type of carboxylic acid having a carbon number of 1 to 8, and, as needed, an acetylacetonato group.
摘要:
Provided is a coating solution where, upon producing a rare-earth superconductive composite metal oxide film by means of a coating-pyrolysis method, cracks are not generated in the heat treatment process for eliminating organic components, even when the thickness of the rare-earth superconductive film produced in a single coating is 500 nm or more, and without having to repeat the coating and annealing process. A solution for producing a rare-earth superconductive film which is made into a homogeneous solution by dissolving, in a solvent formed by adding a polyhydric alcohol to a univalent linear alcohol having a carbon number of 1 to 8 and/or water, a metal complex coordinated, relative to metal ions of a metallic species containing rare-earth elements, barium and copper, with pyridine and/or at least one type of tertiary amine, at least one type of carboxylic acid having a carbon number of 1 to 8, and, as needed, an acetylacetonato group.
摘要:
A metal complex composition containing complexes having metal species of a rare earth element, barium and copper and ligands of a trifluoroacetic acid or pentafluoropropionic acid ligand, a pyridine ligand and an acetylacetone ligand. A superconductive film may be obtained by applying an organic solvent solution of the above metal complex composition to a substrate and by heat treating the coating.
摘要:
There is disclosed a method for producing a metal oxide, which comprises the steps of: dissolving a metal organic compound (e.g. a metal organic acid salt, a metal acetylacetonato complex, and a metal alkoxide having an organic group with 6 or more carbon atoms) in a solvent to provide a state of solution, applying the solution onto a substrate, drying the solution, and subjecting the resultant substrate to irradiation with a laser light of a 400 nm or less wavelength, to form a metal oxide on the substrate. According to that method, a metal oxide can be produced without applying a heat treatment at a high temperature of the degree adopted in the conventionally known application thermal decomposition method.
摘要:
An oxide superconducting thin film includes a substrate having a single crystal structure, the main face of the substrate and a crystal face of the single crystal structure having an angle therebetween; an intermediate layer formed on the main face of the substrate and having an axis oriented in a direction perpendicular to the crystal face; and a superconducting layer formed on the intermediate layer and containing, as a main component, an oxide superconductor having a c-axis oriented in a direction perpendicular to the surface of the intermediate layer. A superconducting fault current limiter and a method of manufacturing an oxide superconducting thin film are also provided.
摘要:
An oxide superconducting thin film includes a substrate, and an intermediate layer and a superconducting layer provided in this order on the substrate. The intermediate layer has an average thickness of from 10 nm to 20 nm and a surface roughness Ra of 0.5 nm or less. The superconducting layer is formed on a surface of the intermediate layer and includes an oxide superconductor as a main component. A superconducting fault current limiter including the oxide superconducting thin film is also provided.
摘要:
Provided is a resistor film comprising vanadium oxide as a main component, wherein metal-to-insulator transition is indicated in the vicinity of room temperature in temperature variations of electric resistance, there is no hysteresis in a resistance change in response to temperature variations or the temperature width is small at less than 1.5K even if there is hysteresis, and highly accurate measurement can be provided when used in a bolometer.Upon producing the resistor film comprising vanadium oxide as a main component by treating a coating film of an organovanadium compound via laser irradiation or the like, a crystalline phase and a noncrystalline (amorphous) phase are caused to coexist in the resistor film.
摘要:
An oxide superconducting thin film includes a substrate, and an intermediate layer and a superconducting layer provided in this order on the substrate. The intermediate layer has an average thickness of from 10 nm to 20 nm and a surface roughness Ra of 0.5 nm or less. The superconducting layer is formed on a surface of the intermediate layer and includes an oxide superconductor as a main component. A superconducting fault current limiter including the oxide superconducting thin film is also provided.