摘要:
An optical film, is provided, the optical film including: a support; and at least one antiglare layer having a surface that has asperities, wherein the at least one antiglare layer contains at least one kind of light transmitting particles including first light transmitting particles in an amount of 0.01 to 1 mass % based on a total solid content in the antiglare layer, the first light transmitting particles have an average particle size that is 0.1 to 4.0 μm greater than an average thickness of the antiglare layer, and a region θ(0.5) in which slope angles θ of the asperities of the surface of the antiglare layer lie within a range of 0°
摘要:
An antiglare film is provided and includes: a transparent support; and an antiglare layer containing a binder and a light-transmitting fine particle. The light-transmitting fine particle has an average particle diameter of 3 to 15 μm, the antiglare layer has an average thickness smaller than the average particle diameter of the light-transmitting fine particle by 0.1 to 2.0 μm, the antiglare layer contains the light-transmitting fine particle in an amount of 1.0 to 3.0 weight % based on all solid contents of the antiglare layer. The antiglare layer has a surface having a θ(1) of 60 to 98.5%, wherein the θ(1) is a ratio of a surface region of 0°≦θ≦1° in the surface when θ represents a tilt angle of an irregularity on the surface.
摘要:
An optical film, includes: a transparent support; and at least one low refractive index layer, wherein the at least one low refractive index layer is a layer formed from a coating composition containing: (A) an inorganic fine particle; (B) a fluorine-containing copolymer; and (C) a polyfunctional fluorine-containing acrylate, and the polyfunctional fluorine-containing acrylate (C) is represented by the following structural formula: wherein Rf represents a (p+q)-valent perfluoro saturated hydrocarbon group having a carbon number of 1 to 20, which may have an ether bond; p represents an integer of 2 to 10; q represents an integer of 0 to 8, provided that (p+q) represents an integer of 2 to 10; r represents an integer of 0 to 100; and R represents a hydrogen atom, a methyl group, a fluorine atom or a trifluoromethyl group.
摘要:
Providing is an antistatic hard-coat-layer forming composition including a nonvolatile component containing a conductive polymer (a) a compound (b) and a photo-polymerization initiator (c); and a volatile component containing a solvent (d) having a hydroxyl group, and a solvent (e) having no hydroxyl group where the boiling point is 120° C. or less, wherein the solvent (d) contains a solvent (d2) with 4 or more carbon atoms having a hydroxyl group where the boiling point is 90° C. or more and the SP value is 22.0 to 35.0, the proportion of the polymer (a) in the nonvolatile component is 1 to 20 mass %, the proportion of the solvent (d) in the volatile component is 0.5 to 25 mass %, and the proportion of the component (d2) in the component (d) is 80 to 100 mass %.
摘要:
A production method of an antireflection film comprises, in order, a step of applying a coating composition obtained by mixing the following components (A) to (D) on a base material to form a coating film, a step of drying the coating film to volatilize the solvent therefrom, and a step of curing the coating film to form a cured layer, wherein a multilayer structure having different refractive indexes is formed from the coating composition: (A) a compound having at least one structure selected from a fluorine-containing hydrocarbon structure and a polysiloxane structure and at least one basic functional group, (B) an inorganic fine particle, (C) a curable binder containing no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.
摘要:
The method for producing an antireflection film is provided. The method includes, a step of coating a coating composition including the following components (A) to (D) on a base material to form a coating film, a step of volatilizing the solvent from the coating film for drying the coating film, and a step of curing the coating film to form a cured layer, in which a multilayer structure having different refractive indices from the coating composition is formed: (A) a fluorine-containing polymer with a specific structure, having a polyalkylene oxide group in the molecule, (B) non-surface-modified inorganic fine particles, or inorganic fine particles that are surface-treated with a silane coupling agent having a molecular weight of 600 or less, (C) a curable binder having no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.
摘要:
The method for producing an antireflection film is provided. The method includes, a step of coating a coating composition including the following components (A) to (D) on a base material to form a coating film, a step of volatilizing the solvent from the coating film for drying the coating film, and a step of curing the coating film to form a cured layer, in which a multilayer structure having different refractive indices from the coating composition is formed: (A) a fluorine-containing polymer with a specific structure, having a polyalkylene oxide group in the molecule, (B) non-surface-modified inorganic fine particles, or inorganic fine particles that are surface-treated with a silane coupling agent having a molecular weight of 600 or less, (C) a curable binder having no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.
摘要:
A production method of an antireflection film comprises, in order, a step of applying a coating composition obtained by mixing the following components (A) to (D) on a base material to form a coating film, a step of drying the coating film to volatilize the solvent therefrom, and a step of curing the coating film to form a cured layer, wherein a multilayer structure having different refractive indexes is formed from the coating composition: (A) a compound having at least one structure selected from a fluorine-containing hydrocarbon structure and a polysiloxane structure and at least one isocyanate group; (B) an inorganic fine particle; (C) a curable binder containing no fluorine atom in the molecule; and (D) a solvent; provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.
摘要:
An antireflective film is provided, the antireflective film including: a transparent support; and at least one low refractive index layer, wherein the low refractive index layer is formed from a composition containing at least following (A) to (C): (A) a fluorine-containing antifouling agent having at least one polymerizable unsaturated group; (B) a fluorine-containing copolymer having at least one polymerizable unsaturated group; and (C) inorganic fine particles.
摘要:
An antireflective film includes: a transparent substrate film; and at least one low refractive index layer, the low refractive index layer is formed with a composition containing: a fluorine-containing antifouling agent having a weight average molecular weight of less than 10,000 and a structure represented by the following formula (F); a polyfunctional monomer having a polymerizable unsaturated group; and (C) an inorganic particle, and a content of the fluorine-containing antifouling agent is 1% by weight or more and less than 25% by weight based on a total solid content of the coating composition: (Rf)-[(W)-(RA)n]m Formula (F) wherein, Rf represents a (per)fluoroalkyl group or a (per)fluoropolyether group, W represents a connecting group, RA represents a functional group having a polymerizable unsaturated group, n represents an integer of from 1 to 3, and m represents an integer of from 1 to 3.