Weld bonding method
    1.
    发明授权
    Weld bonding method 失效
    焊接方法

    公开(公告)号:US6146488A

    公开(公告)日:2000-11-14

    申请号:US954966

    申请日:1997-10-21

    摘要: The present invention is a weld bonding method providing adhesion by both an adhesive and resistance spot welding, and includes application of an adhesive including a thermosetting epoxy resin, a latent curing agent and 1 to 15 vol % of one or more additives selected from the group consisting of conductive metals, metal oxides, metal carbides, metal nitrides, metal borides, and metal silicides, which are in the from of powder having a particle size of 10 .mu.m or less, or in the form of fragments or flakes having a thickness of 0.5 .mu.m or more and a size of 30 .mu.m or less.

    摘要翻译: 本发明是通过粘合剂和电阻点焊两者提供粘合的焊接方法,包括使用包含热固性环氧树脂,潜在性固化剂和1〜15体积%的一种或多种添加剂的粘合剂的应用,所述添加剂选自 由来自具有10μm或更小的粒度的粉末的导电金属,金属氧化物,金属碳化物,金属氮化物,金属硼化物和金属硅化物组成,或者具有厚度的片状或薄片形式 为0.5μm以上,尺寸为30μm以下。

    Method of manufacturing full face vehicle wheel
    2.
    发明授权
    Method of manufacturing full face vehicle wheel 有权
    全面车轮制造方法

    公开(公告)号:US07509739B2

    公开(公告)日:2009-03-31

    申请号:US10537232

    申请日:2004-10-18

    IPC分类号: B23P11/00 B21K1/32 B60B3/00

    摘要: A method of manufacturing a full face vehicle wheel having a high durability performance, in which the back surface of a wheel disk is provided in advance with an annular joining groove. A peripheral joining end of a wheel rim is provided in advance with an inside slope end surface. The peripheral joining end is seated and positioned on the bottom surface of the annular joining groove. A welding heat confining annular region is produced between the inside groove wall of the annular joining groove and the inside slope end surface. The annular joining groove and the peripheral joining end are joined by welding.

    摘要翻译: 一种制造具有高耐久性的全面车轮的方法,其中轮盘的后表面预先设置有环形接合槽。 轮缘的周边连接端部预先设置有内侧倾斜端面。 周边连接端位于环形接合槽的底面上并定位。 在环形接合槽的内侧槽壁和内侧倾斜端面之间产生焊接热限制环状区域。 环形接合槽和周边接合端通过焊接接合。

    Resistance welding process for aluminum and aluminum alloy materials
    3.
    发明授权
    Resistance welding process for aluminum and aluminum alloy materials 失效
    铝和铝合金材料的电阻焊接工艺

    公开(公告)号:US5552573A

    公开(公告)日:1996-09-03

    申请号:US167396

    申请日:1993-12-08

    摘要: A resistance welding process for aluminum and aluminum alloy materials for enabling the remarkable improvement of the electrode life comprises the steps of preparing an insert material having the overall thickness of 0.02 to 1 mm including a sheet-like core material consisting of iron, steel, copper or copper alloy and coated layers each having the thickness of 1 to 100 .mu.m, consisting of any one of Ni, Ni alloy, Ti, Ti alloy, Nb, Nb alloy, Mo, Mo alloy, W, W alloy, Cr, Cr alloy, Co and Co alloy and formed on both surfaces of the core material, or an insert material consisting of Ti foil or Ni foil; interposing the insert material between each of upper and under electrodes and each portion of overlapped materials to be welded consisting of aluminum or aluminum alloy; pressurizing the materials to be welded by the upper and under electrodes to join the materials to be welded together. The coated layers on both surfaces of the core material may consist of the same metal or different metals from each other. When the core material of the insert material consists of iron or steel, the insert material having the coated layer consisting of Ti and formed on one surface is interposed between each electrode and each portion of the materials to be welded in such a state that the coated layer faces each material to be welded, and the materials to be welded are pressurized and jointed together.

    摘要翻译: 用于铝和铝合金材料的电阻焊接方法能够显着提高电极寿命包括以下步骤:制备总厚度为0.02至1mm的插入材料,包括由铁,钢,铜组成的片状芯材 或者由Ni,Ni合金,Ti,Ti合金,Nb,Nb合金,Mo,Mo合金,W,W合金,Cr,Cr中的任一种构成的厚度为1〜100μm的铜合金和涂层 合金,Co和Co合金,并形成在芯材的两个表面上,或由Ti箔或Ni箔组成的插入材料; 将插入材料插入每个上电极和下电极之间,并且每个重叠焊接材料部分由铝或铝合金构成; 通过上部和下部电极对要焊接的材料进行加压,以将待焊接的材料结合在一起。 芯材的两个表面上的涂层可以由相同的金属或彼此不同的金属组成。 当插入材料的芯材料由铁或钢组成时,具有由Ti构成的涂层的一个表面上形成的插入材料以这样的状态插入每个电极和待焊接材料的每个部分之间, 层面对每个待焊接的材料,并且待焊接的材料被加压并接合在一起。