    摘要: A process for regenerating a zeolite catalyst comprises the following stages: (I) Heating a partially or completely deactivated catalyst to 250-600° C. in an atmosphere which contains less than 2% by volume of oxygen, (II) treating the catalyst at from 250 to 800° C., preferably from 350 to 600° C., with a gas stream which contains from 0.1 to 4% by volume of an oxygen-donating substance or of oxygen or of a mixture of two or more thereof, and (III) treating the catalyst at from 250 to 800° C., preferably from 350 to 600° C., with a gas stream which contains from more than 4 to 100% by volume of an oxygen-donating substance or of oxygen or of a mixture of two or more thereof.

    摘要翻译: 再生沸石催化剂的方法包括以下步骤:(I)在含有少于2体积%氧气的气氛中将部分或完全失活的催化剂加热至250-600℃,(II)将催化剂处理 250至800℃,优选350至600℃,含有0.1至4体积%的供氧物质或氧气或其两种或多种的混合物的气流和 (III)在250至800℃,优选350至600℃下处理催化剂,其中气流含有超过4至100体积%的供氧物质或氧气或 其两种或更多种的混合物。

    Method for regenerating a zeolitic catalyst
    6.
    发明授权
    Method for regenerating a zeolitic catalyst 有权
    再生沸石催化剂的方法

    公开(公告)号:US06710002B2

    公开(公告)日:2004-03-23

    申请号:US10061282

    申请日:2002-02-04

    IPC分类号: B01L2990

    摘要: A process for regenerating a zeolite catalyst comprises the following stages: (I) Heating a partially or completely deactivated catalyst to 250-600° C. in an atmosphere which contains less than 2% by volume of oxygen, (II) treating the catalyst at from 250 to 800° C., preferably from 350 to 600° C., with a gas stream which contains from 0.1 to 4% by volume of an oxygen-donating substance or of oxygen or of a mixture of two or more thereof, and (III) treating the catalyst at from 250 to 800° C., preferably from 350 to 600° C., with a gas stream which contains from more than 4 to 100% by volume of an oxygen-donating substance or of oxygen or of a mixture of two or more thereof.

    摘要翻译: 再生沸石催化剂的方法包括以下步骤:(I)在含有少于2体积%氧气的气氛中将部分或完全失活的催化剂加热至250-600℃,(II)将催化剂处理 250至800℃,优选350至600℃,含有0.1至4体积%的供氧物质或氧气或其两种或多种的混合物的气流和 (III)在250至800℃,优选350至600℃下处理催化剂,其中气流含有超过4至100体积%的供氧物质或氧气或 其两种或更多种的混合物。