Propylene block copolymer and propylene resin composition
    1.
    发明授权
    Propylene block copolymer and propylene resin composition 有权
    丙烯嵌段共聚物和丙烯树脂组合物

    公开(公告)号:US06825280B1

    公开(公告)日:2004-11-30

    申请号:US09485189

    申请日:2000-02-07

    IPC分类号: C08L2310

    摘要: Disclosed are a propylene polymer composition possessing excellent balance among rigidity and low warpage, resistance to deterioration caused by thermal oxidation during processing, weathering resistance, antistatic properties, and low bleeding properties, and a propylene resin composition which can easily produce molded products having excellent balance between rigidity and impact resistance (particularly low-temperature impact resistance) or heat resistance. The propylene polymer composition and the propylene resin composition comprise a propylene block copolymer consisting essentially of the following blocks (a) and (b) and having a melt flow rate of 0.1 to 200 g/10 min: block (a): a polymer block of a homopolymer of propylene or a random copolymer of propylene with a comonomer selected from the group consisting of ethylene and C4-C20 &agr;-olefins, the content of the comonomer being not more than 10% by mole; and block (b): a polymer block of a random copolymer of propylene with at least one comonomer selected from the group consisting of ethylene and C4-C20 &agr;-olefins, the content of the comonomer being 10 to 80% by mole, the average chain length of the comonomer block and the gross average chain length of the comonomer having a relationship represented by formula (I) nb≦n+1.5  (I) wherein nb represents the average chain length of the comonomer block; and n represents the gross average chain length of the comonomer.

    摘要翻译: 公开了在刚性和低翘曲之间具有优异的平衡性,耐加工中的热氧化,耐候性,抗静电性和低渗透性的耐劣化性的丙烯聚合物组合物,以及可以容易地制备具有优异平衡性的模塑产品的丙烯树脂组合物 刚性和抗冲击性(特别是低温耐冲击性)或耐热性。 丙烯聚合物组合物和丙烯树脂组合物包含基本上由以下嵌段(a)和(b)组成并且熔体流动速率为0.1至200g / 10min的丙烯嵌段共聚物:嵌段(a):聚合物嵌段 的丙烯均聚物或丙烯与选自乙烯和C 4 -C 20α-烯烃的共聚单体的无规共聚物,共聚单体的含量不超过10摩尔% 和嵌段(b):丙烯与至少一种选自乙烯和C 4 -C 20α-烯烃的共聚单体的无规共聚物的聚合物嵌段,共聚单体的含量为10〜80摩尔%,平均链 共聚单体嵌段的长度和由式(I)表示的关系的共聚单体的总平均链长,其中nb表示共聚单体嵌段的平均链长; n表示共聚单体的总平均链长。

    Propylene block copolymer and resin composition
    2.
    发明授权
    Propylene block copolymer and resin composition 有权
    丙烯嵌段共聚物和树脂组合物

    公开(公告)号:US06469100B2

    公开(公告)日:2002-10-22

    申请号:US09325384

    申请日:1999-06-04

    IPC分类号: C08L5300

    摘要: A block copolymer is provided comprising one or more blocks of a propylene polymer (PP) and one or more blocks of an ethylene-propylene copolymer (EPR) having the properties: (1) the interface thickness of the PP block with EPR block is from 20-1000 nm; (2) the weight average molecular weight of the PP block is 10,000-1,000,000; (3) the proportion of mesopentad chain in the PP block is not less than 95%; (4) the particle diameter of the disperse phase in EPR block is 0.2-3 microns; (5) the weight average molecular weight of the EPR block is 50,000-1000,000; (6) the propylene content in the EPR block is 20-80 mole %; (7) the composition fluctuation in molecular weight in EPR block is within +/−5% from the average composition.

    摘要翻译: 提供一种包含一个或多个丙烯聚合物(PP)嵌段和一个或多个乙烯 - 丙烯共聚物嵌段(EPR)的嵌段共聚物,其具有以下性质:(1)PP嵌段与EPR嵌段的界面厚度为 20-1000nm;(2)PP块的重均分子量为10,000-1,000,000;(3)PP嵌段中的美链的比例不低于95%;(4)分散体的粒径 EPR嵌段的相为0.2-3微米;(5)EPR嵌段的重均分子量为50,000-1000,000;(6)EPR嵌段中的丙烯含量为20-80摩尔%;(7) EPR块中分子量的组成波动在平均组成的+/- 5%以内。

    Process for producing propylene block copolymers
    3.
    发明授权
    Process for producing propylene block copolymers 失效
    制备丙烯嵌段共聚物的方法

    公开(公告)号:US5623022A

    公开(公告)日:1997-04-22

    申请号:US502141

    申请日:1995-07-13

    摘要: A propylene block copolymer having a high impact resistance is prepared without the generation of finely divided particles or the adhesion to the reactor, which propylene block copolymer having a weight ratio of 5/95-70/30 (process (1)/process (2)) is obtained by carrying out the particular polymerization processes (1) and (2) in this sequence under the action of the catalyst comprising the following A and B.A: particular transition metal compound.B: an alumoxane, the reaction product of an alkylboronic acid with an organoAl, a Lewis acid or ionic compound.Process (1): process for copolymerizing propylene and a specified comonomer in a ratio of 0/100-80/20.Process (2): process for producing a propylene polymer having a specified comonomer in an amount of 10% by weight or less.

    摘要翻译: 制备具有高耐冲击性的丙烯嵌段共聚物,而不产生细碎颗粒或与反应器的粘附性,该丙烯嵌段共聚物的重量比为5 / 95-70 / 30(工艺(1)/工艺(2) ))是通过在包含以下A和B的催化剂的作用下以该顺序进行特定的聚合方法(1)和(2)得到的。A:特定的过渡金属化合物。 B:铝氧烷,烷基硼酸与有机铝的反应产物,路易斯酸或离子化合物。 方法(1):以0 / 100-80 / 20的比例共聚丙烯和特定共聚单体的方法。 方法(2):制备具有10重量%以下的特定共聚单体的丙烯聚合物的方法。

    Catalyst component for olefin polymerization, catalyst for alpha-olefin polymerization and process for the production of alpha-olefin polymer
    8.
    发明申请
    Catalyst component for olefin polymerization, catalyst for alpha-olefin polymerization and process for the production of alpha-olefin polymer 有权
    用于烯烃聚合的催化剂组分,用于α-烯烃聚合的催化剂和用于生产α-烯烃聚合物的方法

    公开(公告)号:US20050070426A1

    公开(公告)日:2005-03-31

    申请号:US10940769

    申请日:2004-09-15

    摘要: To develop a catalyst component for olefin polymerization, a metallocene catalyst for olefin polymerization and a process for the production of an olefin polymer capable of producing an olefin polymer having a high molecular weight and a high melting point which can be extruded or injection-molded in a high yield and a novel transition metal compound to be used in these catalyst components a catalyst component for olefin polymerization is made of a transition metal compound represented by formula (I) defined in the specification; a metallocene catalyst for olefin polymerization comprises the catalyst component for olefin polymerization; and a process for the production of an olefin polymer is performed in the presence of the metallocene catalyst for olefin polymerization: