摘要:
A thermoplastic resin composition having well-balanced properties which comprises 95-5 weight % of polycarbonate, 5-95 weight % of polyolefin and a particular combination of additional components selected from a styrene-ethylene.propylene copolymer, a styrene-ethylene. butyrene-styrene block copolymer, an AES resin, a styrene-olefin block copolymer, an unsaturated carboxylic acid-modified polyolefin, polybutylene terephthalate, a styrene-maleic anhydride copolymer, an oxazoline ring-containing styrene copolymer a saponified olefin-vinyl ester copolymer and an epoxy group-containing styrene copolymer.
摘要:
A modified polyolefin-polyester graft copolymer includes (a) 10-90 parts by weight of a polyester having an intrinsic viscosity [.eta.] of 0.30-1.20 and an end carboxyl group content of 15-200 milliequivalent/kg, and (b) 90-10 parts by weight of a modified polyolefin having 0.2-5 mol % of an epoxy group or carboxyl group content and a weight-average molecular weight of 8,000-140,000.A thermoplastic resin composition includes (a) 5-95 weight % of an aromatic polycarbonate, (b) 95-5 weight % of a polyolefin, and (c) 1-30 parts by weight, per 100 parts by weight of (a)+(b), of the graft copolymer.
摘要:
A resin composition having excellent paint coatability containing (a) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, (b) 20-40 weight % of an ethylene-.alpha.-olefin copolymer elastomer, and (c) 20 weight % or less of an inorganic filler, components in the components (a) and (b), which are soluble in p-xylene at a room temperature, having a number-average molecular weight of 4.times.10.sup.4 or more and a weight-average molecular weight of 20.times.10.sup.4 or more.
摘要:
A resin composition having excellent paint coatability containing (a) 50-80 weight % of a multi-stage polymerized propylene-ethylene block copolymer consisting essentially of (i) a propylene homopolymer portion, (ii) a propylene-ethylene random copolymer portion, and (iii) an ethylene homopolymer portion, (b) 20-40 weight % of an ethylene-.alpha.-olefin copolymer elastomer, and (c) 20 weight % or less of an inorganic filler, components in the components (a) and (b), which are soluble in p-xylene at a room temperature, having a number-average molecular weight of 4.times.10.sup.4 or more and a weight-average molecular weight of 20.times.10.sup.4 or more.
摘要:
A polypropylene thermoplastic resin composition comprising (a) a modified crystalline polypropylene of a crystalline polypropylene comprising said modified crystalline polypropylene and (b) a modified polyamide obtained by partially or wholly grafting a polyamide with a clay mineral. A polypropylene thermoplastic resin composition comprising, in addition to the above polypropylene thermoplastic resin composition comprising the components (a) and (b), one or any combination of the following components (c), (d) and (e): (c) an ethylene-.alpha.-olefin copolymer rubber or a modified ethylene-.alpha.-olefin copolymer rubber, (d) a block copolymer between a monovinyl-substituted aromatic hydrocarbon and a conjugated diene, a hydrogenation product of said block copolymer, or a modification product of said block copolymer, and (e) an inorganic filler. The modified polyamide as the component (b), obtained by modifying a polyamide with a clay mineral has good compatibility with or good dispersibility in the component (a), i.e. the modified crystalline polypropylene or the crystalline polypropylene comprising the modified crystalline polypropylene. Therefore, the polypropylene thermoplastic resin composition comprising these components (a) and (b) has excellent heat resistance and excellent impact resistance.
摘要:
The polypropylene resin composition of the present invention can be obtained by melt mixing:(a) a modified polypropylene obtained by grafting a crystalline propylene-ethylene block copolymer with an unsaturated carboxylic acid, or a crystalline polypropylene containing the modified polypropylene,(b) a polyamide, and(c) a modified ethylene-.alpha.-olefin copolymer rubber obtained by grafting an ethylene-.alpha.olefin copolymer rubber with an unsaturated carboxylic acid. This composition is superior in low temperature impact resistance, rigidity, heat resistance and oil resistance.
摘要:
There is disclosed a thermoplastic resin composition comprising a blend of100 parts by weight of a resin composition composed of 1 to 99% by weight of a polypropylene type resin (C) selected from the group consisting of a modified polypropylene (A) obtained by graft copolymerizing an unsaturated carboxylic acid or a derivative thereof and an unsaturated aromatic monomer onto polypropylene, and a composition composed of the modified polypropylene (A) and a polypropylene (B), and 99 to 1% by weight of at least one saturated polyester resin (D),0.1 to 300 parts by weight of an epoxy group containing copolymer (E),0.1 to 300 parts by weight of a modified ethylenic copolymer rubber (F) obtained by graft copolymerizing an unsaturated carboxylic acid or a derivative thereof and an unsaturated aromatic monomer onto ethylenic copolymer rubber, andup to 5 parts by weight of a basic compound (G) optionally added as reaction accelerator, the content of the saturated polyester resin in the thermoplastic polyester resin being less than 50% by weight.The thermoplastic resin composition of the present invention has high heat resistance and high impact resistance, in particular, high low-temperature impact resistance and is advantageously used in automobile parts, electric and electronic parts, etc.
摘要:
A polypropylene thermoplastic resin composition comprising (a) a modified crystalline polypropylene of a crystalline polypropylene comprising said modified crystalline polypropylene and (b) a modified polyamide obtained by partially or wholly grafting a polyamide with a clay mineral. A polypropylene thermoplastic resin composition comprising, in addition to the above polypropylene thermoplastic resin composition comprising the components (a) and (b), one or any combination of the following components (c), (d) and (e): (c) an ethylene-.alpha.-olefin copolymer rubber or a modified ethylene-.alpha.-olefin copolymer rubber, (d) a block copolymer between a monovinyl-substituted aromatic hydrocarbon and a conjugated diene, a hydrogenation product of said block copolymer, or a modification product of said block copolymer, and (e) an inorganic filler. The modified polyamide as the component (b), obtained by modifying a polyamide with a clay mineral has good compatibility with or good dispersibility in the component (a), i.e. the modified crystalline polypropylene or the crystalline polypropylene comprising the modified crystalline polypropylene. Therefore, the polypropylene thermoplastic resin composition comprising these components (a) and (b) has excellent heat resistance and excellent impact resistance.
摘要:
A process for reclaiming waste plastics having a paint film which includes subjecting the paint film to a hydrolysis treatment by immersing the waste plastics having a urethane paint film or an amino resin paint film in a treating liquid, or contacting the waste plastics with the vapor of a treating liquid, to decompose the paint into lower molecular weight compounds. The resulting waste plastics are then heated and kneaded to disperse the products of the hydrolysis in the waste plastics, and there is recovered a reclaimed waste plastics product having good mechanical properties.
摘要:
A polypropylene resin composition having excellent rigidity, impact resistance and formability (moldability) and thus useful for the interior parts of automobile, includes (A) a crystalline E/P block copolymer containing a fraction Ac soluble in p-xylene at room temperature and having an ethylene content of 18 to 22%; (B) a crystalline E/P block copolymer containing a fraction Bc soluble in p-xylene at room temperature and having an ethylene content of 27 to 40% and (C) talc particles having an average size of 3 to 5 .mu.m and largest size less than 20 .mu.m, in which composition, (a) the p-xylene-soluble fractions Ac and Bc are in contents As and Bs based on the total weight of the copolymers (A) and (B) and satisfying As+Bs=7 to 17% by weight and As/(A +Bs)=0.1 to 0.6; (b) an isotactic pentad fraction of propylene in each of copolymers (A) and (B) is 96% or more, and the mixture of the copolymers (A) and (B) has a MFR of 20 to 35 g/10 min at 230.degree. C. under 2160 g load; and (c) the copolymers (A) and (B) are in a total weight content of 50 to 95% and talc (C) is in a weight content of 5 to 50%.