Projection resistance welding of superalloys
    4.
    发明授权
    Projection resistance welding of superalloys 有权
    超级合金的防爆焊接

    公开(公告)号:US09273562B2

    公开(公告)日:2016-03-01

    申请号:US13352468

    申请日:2012-01-18

    申请人: Gerald J. Bruck

    发明人: Gerald J. Bruck

    摘要: Superalloy components are joined by mating a recess formed in one component with a corresponding projection formed in another component along a contact surface. The components are compressed along the contact surface and resistance heat welded to each other. Current is passed between the components at a selected flow rate and application time until localized melting occurs along the contact surface, and they are mutually affixed to each other. When repairing a damaged surface portion of a superalloy material component, the damaged portion is removed to form an excavated recess. A repair splice is formed, preferably of a same material with similar mechanical structural properties, having a mating projection with profile conforming to the corresponding recess profile. The splice and substrate are resistance heat welded under compression pressure until localized melting occurs along the contact surface, so that they are mutually affixed.

    摘要翻译: 超合金部件通过将形成在一个部件中的凹部与沿着接触表面形成在另一部件中的相应突起配合而接合。 这些部件沿着接触表面被压缩,并且电阻被热焊接在一起。 电流以选定的流速和施加时间在组分之间通过,直到沿着接触表面发生局部熔融,并且它们彼此相互固定。 当修复超合金材料部件的损坏的表面部分时,损坏的部分被移除以形成挖掘的凹部。 形成具有类似机械结构特性的相同材料的修补接头,其具有符合相应凹槽轮廓的轮廓的配合凸起。 接头和衬底是在压缩压力下进行电阻热焊接,直到沿着接触表面发生局部熔化,使得它们相互贴合。

    PROJECTION RESISTANCE WELDING OF SUPERALLOYS
    6.
    发明申请
    PROJECTION RESISTANCE WELDING OF SUPERALLOYS 有权
    超级合金的耐候性焊接

    公开(公告)号:US20130115480A1

    公开(公告)日:2013-05-09

    申请号:US13352468

    申请日:2012-01-18

    申请人: Gerald J. Bruck

    发明人: Gerald J. Bruck

    IPC分类号: B32B15/00 B23K11/00

    摘要: Superalloy components are joined by mating a recess formed in one component with a corresponding projection formed in another component along a contact surface. The components are compressed along the contact surface and resistance heat welded to each other. Current is passed between the components at a selected flow rate and application time until localized melting occurs along the contact surface, and they are mutually affixed to each other. When repairing a damaged surface portion of a superalloy material component, the damaged portion is removed to form an excavated recess. A repair splice is formed, preferably of a same material with similar mechanical structural properties, having a mating projection with profile conforming to the corresponding recess profile. The splice and substrate are resistance heat welded under compression pressure until localized melting occurs along the contact surface, so that they are mutually affixed.

    摘要翻译: 超合金部件通过将形成在一个部件中的凹部与沿着接触表面形成在另一部件中的相应突起配合而接合。 这些部件沿着接触表面被压缩,并且电阻被热焊接在一起。 电流以选定的流速和施加时间在组分之间通过,直到沿着接触表面发生局部熔融,并且它们彼此相互固定。 当修复超合金材料部件的损坏的表面部分时,损坏的部分被移除以形成挖掘的凹部。 形成具有类似机械结构特性的相同材料的修补接头,其具有符合相应凹槽轮廓的轮廓的配合突起。 接头和衬底是在压缩压力下进行电阻热焊接,直到沿着接触表面发生局部熔化,使得它们相互贴合。

    Process for enhancing the bond strength of resistance welded joints
between titanium alloy articles
    7.
    发明授权
    Process for enhancing the bond strength of resistance welded joints between titanium alloy articles 失效
    提高钛合金制品之间电阻焊接接头的结合强度的方法

    公开(公告)号:US5830289A

    公开(公告)日:1998-11-03

    申请号:US595316

    申请日:1996-02-01

    摘要: A process for enhancing the bond strength of resistance welded joints between titanium alloy articles includes a first step of resistance welding two titanium alloy articles and a second step of heat treating the resistance welded titanium alloy articles in a vacuum or inert environment at temperatures in a range of 1675.degree. F. to 1825.degree. F. for a period of 15 minutes to 4 hours. The process of the present invention is particularly useful in providing efficient joining of face sheets to a honecomb core element.

    摘要翻译: 一种用于提高钛合金制品之间的电阻焊接接头的结合强度的方法包括对两种钛合金制品进行电阻焊接的第一步骤和在真空或惰性环境中在一定范围内的温度下对电阻焊接的钛合金制品进行热处理的第二步骤 为1675°F至1825°F,时间为15分钟至4小时。 本发明的方法特别可用于提供面板到有效核心元件的有效接合。

    Positive displacement casting
    8.
    发明授权
    Positive displacement casting 失效
    正排量铸造

    公开(公告)号:US3908739A

    公开(公告)日:1975-09-30

    申请号:US43515774

    申请日:1974-01-21

    申请人: GOULD INC

    摘要: Methods and apparatus for positive displacement casting and/or for positive displacement bonding and, more particularly, for automatically forming, on a continuous, reproducible basis, fusion bonds devoid of structural and electrical defects between two or more workpieces by moving a heated electrode into the area to be bonded so as to uniformly heat and melt the portions of the workpieces to be bonded while, at the same time, displacing substantially all of the molten material from the area to be bonded into a storage area or reservoir surrounding the heated electrode where such molten material is maintained in its uniformly heated molten state, and then retracting the electrode so as to permit the molten material to return to the cavity formed by the electrode in the workpieces where such molten material is allowed to cool and solidify, thus forming a flawless bond between the workpieces-thermal or fusion bonds are made in accordance with the methods of the invention and with the apparatus of the invention by a combination of (1) elevated temperature levels sufficient to melt the material to be bonded, and (2) displacement of the molten material; as contrasted with more conventional techniques and/or apparatus which combine elevated temperature levels and pressure.

    摘要翻译: 用于正位移铸造和/或用于正位移结合的方法和装置,更具体地,用于在连续的可再现的基础上自动地形成通过将加热的电极移动到所述两个或更多个工件中的结构和电缺陷的熔合键 以便均匀地加热和熔化待接合的工件的部分,同时将基本上所有的熔融材料从待接合的区域移动到围绕加热的电极的储存区域或储存器中,其中, 这种熔融材料保持其均匀加热的熔融状态,然后使电极回缩,以使熔融材料返回到由工件中的电极形成的空腔中,使熔融材料冷却和固化,从而形成 根据本发明的方法和应用,制造工件之间的完美无缺的粘合 - 热或熔合键 通过(1)足以熔化要结合的材料的升高的温度水平和(2)熔融材料的移位的组合来实现本发明; 与组合升高的温度水平和压力的更常规的技术和/或装置形成对比。