Healing agent for self-healing cementious material
    2.
    发明授权
    Healing agent for self-healing cementious material 有权
    自愈愈合剂治愈剂

    公开(公告)号:US08911549B2

    公开(公告)日:2014-12-16

    申请号:US13639840

    申请日:2011-04-06

    摘要: The invention provides a process for the production of a cementious material. The process comprises mixing cement starting materials and a particulate healing agent to provide the cementious material. The healing agent comprises coated particles, wherein the coated particles comprise bacterial material and additive. The bacterial material is selected from the group consisting of a bacterium, a lyophilized bacterium and a bacterial spore of a bacterium. The present invention solves these problems, as (substantially leakage-proof) tablets containing the actual healing agent may neither interfere with either the workability of the liquid mixture (“cementious material”) nor negatively affect properties of either mixture or final material (hardened concrete), even when applied in large quantities. During crack formation in cementious based constructions, the particles also crack, and healing agent is released.

    摘要翻译: 本发明提供一种生产胶结材料的方法。 该方法包括混合水泥起始材料和颗粒愈合剂以提供粘结材料。 愈合剂包括涂覆的颗粒,其中涂覆的颗粒包括细菌材料和添加剂。 细菌材料选自细菌,冻干细菌和细菌的细菌孢子。 本发明解决了这些问题,因为含有实际愈合剂的(基本上防漏的)片剂既不会干扰液体混合物(“胶结材料”)的可加工性,也不影响混合物或最终材料(硬化混凝土 ),即使大量应用。 在水泥基结构裂缝形成过程中,颗粒也开裂,释放愈合剂。

    Highly porous ceramic material for absorption and adsorption purposes,
particularly for animal litter/bedding, process for the production
thereof and the use thereof
    7.
    发明授权
    Highly porous ceramic material for absorption and adsorption purposes, particularly for animal litter/bedding, process for the production thereof and the use thereof 失效
    用于吸收和吸附目的的高度多孔陶瓷材料,特别是用于动物垫料/床上用品,其制备方法及其用途

    公开(公告)号:US4824810A

    公开(公告)日:1989-04-25

    申请号:US71539

    申请日:1987-07-08

    摘要: Highly porous ceramic material for adsorption and absorption purposes, particularly for animal litter, characterized by a porosity of 50 to 300%, preferably 200 to 250%; a water absorption capacity of 50 to 200%, preferably 100 to 150%, a pH-value in the range 5 to 9, preferably 7 to 8; a bulk density of 400 to 700 g/1; an internal surface (BET-N.sub.2) between 20 and 200 m.sup.2 /g, preferably between 80 and 150 m.sup.2 /g; which can be produced by firing a foamed mixture of clay or clays, optionally aggregate or aggregates, anionic or cationic surfactant or surfactants and deflocculant or deflocculants, process for the production thereof and use thereof.

    摘要翻译: PCT No.PCT / DE85 / 00035 Sec。 371日期1985年12月17日第 102(e)日期1985年12月17日PCT提交1985年2月9日PCT公布。 出版物WO85 / 04862 日期:1985年11月7日。用于吸收和吸收目的的多孔陶瓷材料,特别是用于动物垫料,其特征在于孔隙率为50-300%,优选为200-250%。 吸水量为50〜200%,优选为100〜150%,pH值为5〜9,优选为7〜8; 堆积密度为400至700g / l; 介于20和200m2 / g之间的内表面(BET-N2),优选在80和150m2 / g之间; 其可以通过煅烧粘土或粘土的泡沫混合物,任选的聚集体或聚集体,阴离子或阳离子表面活性剂或表面活性剂和抗絮凝剂或抗絮凝剂,其制备方法和用途来制备。

    PRODUCTION OF THERMAL ENERGY STORAGE SYSTEMS
    10.
    发明申请

    公开(公告)号:US20200290926A1

    公开(公告)日:2020-09-17

    申请号:US16630280

    申请日:2018-07-12

    摘要: The invention relates to a method for producing thermal energy storage components comprising phase change material embedded into porous components, in particular for use in cement-based compositions. The method comprises: an impregnation step (10) comprising introducing phase change material into porous components inside a main vessel (102) by vacuum impregnation; an injection step (12) at a temperature within a melting temperature range of said phase change material and under an overpressure, in order vacuuming to force the phase change material into the porous components; and an entrapment step (14) comprising reducing the temperature inside the main vessel, while maintaining an the overpressure, in order to lower the viscosity of said phase change material.