Abstract:
The present disclosure provides a metal compound. The metal compound is represented by a formula (I): Cu2AαB2-αO4-&bgr; (I). A contains at least one element selected from the groups 6 and 8 of the periodic table. B contains at least one element selected from the group 13 of the periodic table, 0
Abstract:
A defroster and a vehicle are provided. The defroster includes: a housing defining an air outlet; a heating device disposed in the housing; an air blower defining a blowing outlet and disposed in the housing; and an air duct defining a duct inlet and a duct outlet, the air duct being disposed between the blowing outlet and the heating device so that air blown out from the blower outlet enters the air duct via the duct inlet and goes out of the air duct via the duct outlet, then passes through the heating device to exchange heat with the heating device, and is discharged out of the housing via the air outlet, wherein an area of the duct inlet is different from that of the duct outlet.
Abstract:
The present disclosure provides a shell, a method of preparing the same and the use of the shell. The shell includes: a base (1) made of ceramic; and a bending part (2) disposed connected with an edge of the base (1) and made of an amorphous alloy.
Abstract:
A method for metallizing a surface of a ceramic substrate includes molding and sintering a ceramic composition to obtain the ceramic substrate, in which the ceramic composition comprises a ceramic powder and a functional powder dispersed in the ceramic powder, radiating a predetermined region of the surface of the ceramic substrate, and performing chemical plating on the ceramic substrate.
Abstract:
The present disclosure discloses an anti-yellowing composition comprising at least a phosphorus-containing compound and at least a pentaerythritol ester, wherein the phosphorus-containing compound is selected from a phosphate salt, which is present in an amount of 100-1600 parts by weight relative to 100 parts by weight of the pentaerythritol ester. The present disclosure also discloses a resin composition containing the anti-yellowing composition, and a metal-resin composite formed with the resin composition and a metal substrate, and preparation method and use thereof. The present disclosure further discloses a electronic product shell formed with the resin composition and a metal shell body.
Abstract:
The present disclosure provides a metal-ceramic composite component and method for preparing the same. The metal-ceramic composite component includes a ceramic substrate having a groove on a surface thereof; a metal member filled in the groove, including a main body made of zirconium base alloy, and a reinforcing material dispersed in the main body and selected from at least one of W, Mo, Ni, Cr, stainless steel, WC, TiC, SiC, ZrC, ZrO 2 , BN, Si 3 N 4 , TiN and Al 2 O 3 ; a luminance value L of the metal member surface is in a range of 36.92-44.07 under the LAB Chroma system.
Abstract:
A metal forming apparatus includes a smelting device, a molding device, an injection device and a vacuumizing device. The smelting device defines a smelting chamber, and includes a rotatable crucible and a heating unit both disposed within the smelting chamber. The molding device defines a molding chamber sealedly communicated with the smelting chamber. The injection device includes a charging barrel assembly sealedly disposed at a joint between the molding device and the smelting device and an injection unit sealedly connected with the smelting device. The vacuumizing device is sealedly connected with the smelting device and the molding device respectively so as to vacuumize the smelting chamber and the molding chamber.
Abstract:
A method for integrally molding a metal and a resin and a metal-resin composite structure obtainable by the same are provided. The method comprises forming a nanopore in a surface of a metal sheet; melting a thermoplastic resin on the surface of the metal sheet formed with the nanopore; and injection molding the thermoplastic resin onto the surface of the metal sheet. The thermoplastic resin is a mixture of a main resin and a polyolefin resin, the main resin is a mixture of polyphenylene oxide and a polyamide, and the polyolefin resin has a melting point of about 65° C. to about 105° C.