ANTIFOULING COMPOSITION, ANTIFOULING SHEET AND METHOD FOR PRODUCING ANTIFOULING SHEET

    公开(公告)号:US20180298231A1

    公开(公告)日:2018-10-18

    申请号:US15569602

    申请日:2016-04-26

    Abstract: Provided are an antifouling composition including a tetrafunctional silane-based compound (A) having a specified structure, a trifunctional silane-based compound (B) having a specified structure, and a metal catalyst (C) containing one or more metal atoms selected from titanium, aluminum, and zinc, which does not require light irradiation for revealing a catalytic action; an antifouling sheet including an antifouling layer formed of the antifouling composition; and a method for producing the same.

    METHOD FOR STICKING A FORMED PRODUCT OF AN ADHESIVE TO AN ADHEREND
    9.
    发明申请
    METHOD FOR STICKING A FORMED PRODUCT OF AN ADHESIVE TO AN ADHEREND 审中-公开
    用于粘贴胶粘剂的成型产品的方法

    公开(公告)号:US20150190993A1

    公开(公告)日:2015-07-09

    申请号:US14661086

    申请日:2015-03-18

    Abstract: A method for sticking a formed product of an adhesive composition to an adherend composed of a metal, which includes: (a) holding the formed product to the adherend with a magnetic force, (b) heating the resultant formed article at 110° C. to 200° C. to decrease the magnetic force and to generate adhesion, thereby sticking the formed product to the adherend by the adhesion, wherein the adhesive composition comprises a mixture of a hot-melt adhesive and a ferromagnetic material, the adhesive composition exhibiting a surface magnetic force of not less than 20 mT to be operable to be held to the adherend having a surface magnetic force of less than 5 mT after a heating at 50° C. for 40 minutes, and the adhesive composition having a shear force of not less than 20 N after a hot bonding at 150° C. for 10 minutes.

    Abstract translation: 将粘合剂组合物的成形物粘贴到由金属构成的被粘物上的方法,该方法包括:(a)以磁力将所形成的产品保持在被粘物上,(b)在110℃下加热所得的成型体。 至200℃以降低磁力并产生粘附,从而通过粘合将成形产品粘贴到被粘物上,其中粘合剂组合物包含热熔粘合剂和铁磁材料的混合物,所述粘合剂组合物显示出 表面磁力不小于20mT,可在50℃加热40分钟后可操作地保持表面磁力小于5mT的被粘物,并且粘合剂组合物的剪切力不为 在150℃热粘合10分钟后小于20N。