Non-aqueous electrolyte secondary battery
    1.
    发明授权
    Non-aqueous electrolyte secondary battery 有权
    非水电解质二次电池

    公开(公告)号:US09023530B2

    公开(公告)日:2015-05-05

    申请号:US11371286

    申请日:2006-03-09

    摘要: To improve high temperature storage characteristic of a non-aqueous electrolyte secondary battery suitable for high input/output application, the structure of a positive electrode active material is optimized. The non-aqueous electrolyte secondary battery includes a positive electrode; a negative electrode; a separator interposed between the positive and negative electrodes; and a non-aqueous electrolyte. The positive electrode active material includes secondary particles, each formed of an aggregate of primary particles. A value (VPr) defined by the formula: VPr=(1−C/D)/(A2×B3) is not less than 0.0005 and not greater than 0.04, where an average particle size of the primary particles is A μm, an average particle size of the positive electrode active material is B μm, a tap density of the positive electrode active material is C g/ml, and a true specific gravity of the positive electrode active material is D g/ml.

    摘要翻译: 为了提高适用于高输入/输出应用的非水电解质二次电池的高温储存特性,优化了正极活性物质的结构。 非水电解质二次电池包括正极; 负极; 插入在正极和负极之间的隔膜; 和非水电解质。 正极活性物质包括由一次粒子的聚集体形成的二次粒子。 由VPr =(1-C / D)/(A2×B3)定义的值(VPr)不小于0.0005且不大于0.04,其中初级粒子的平均粒径为Aμm, 正极活性物质的平均粒径为Bμm,正极活性物质的振实密度为C g / ml,正极活性物质的真比例为D g / ml。

    Non-aqueous electrolyte secondary battery
    2.
    发明申请
    Non-aqueous electrolyte secondary battery 有权
    非水电解质二次电池

    公开(公告)号:US20060204849A1

    公开(公告)日:2006-09-14

    申请号:US11371286

    申请日:2006-03-09

    IPC分类号: H01M4/48 H01M4/52 H01M4/50

    摘要: To improve high temperature storage characteristic of a non-aqueous electrolyte secondary battery suitable for high input/output application, the structure of a positive electrode active material is optimized. The non-aqueous electrolyte secondary battery includes a positive electrode; a negative electrode; a separator interposed between the positive and negative electrodes; and a non-aqueous electrolyte. The positive electrode active material includes secondary particles, each formed of an aggregate of primary particles. A value (VPr) defined by the formula: VPr=(1−C/D)/(A2×B3) is not less than 0.0005 and not greater than 0.04, where an average particle size of the primary particles is A μm, an average particle size of the positive electrode active material is B μm, a tap density of the positive electrode active material is C g/ml, and a true specific gravity of the positive electrode active material is D g/ml.

    摘要翻译: 为了提高适用于高输入/输出应用的非水电解质二次电池的高温储存特性,优化了正极活性物质的结构。 非水电解质二次电池包括正极; 负极; 插入在正极和负极之间的隔膜; 和非水电解质。 正极活性物质包括由一次粒子的聚集体形成的二次粒子。 由以下公式定义的值(V Pr Pr Pr> Pr Pr Pr Pr Pr Pr Pr Pr Pr Pr Pr Pr>>>>>>>>>>>>>>>>>>>>>>>>>>>>>> 3)不小于0.0005且不大于0.04,其中一次颗粒的平均粒径为A mum,正极活性物质的平均粒径为B mum,振实密度为正 电极活性物质为C g / ml,正极活性物质的真比重为D g / ml。

    Production method of positive electrode active material for non-aqueous electrolyte secondary battery and positive electrode active material
    3.
    发明授权
    Production method of positive electrode active material for non-aqueous electrolyte secondary battery and positive electrode active material 有权
    非水电解质二次电池用正极活性物质和正极活性物质的制造方法

    公开(公告)号:US07410511B2

    公开(公告)日:2008-08-12

    申请号:US10636642

    申请日:2003-08-08

    IPC分类号: H01M6/14 H01M4/52

    摘要: A positive electrode active material, which gives a non-aqueous electrolyte secondary battery capable of high input/output where resistance due to a battery reaction in a low temperature environment is suppressed, is produced by a method comprising: (a)providing a nickel hydroxide which is represented by the general formula Ni1−(x+y)CoxMy(OH)2, (b)heating the nickel hydroxide at a temperature not lower than 600° C. and not higher than 1000° C. to produce a nickel oxide which is represented by the general formula Ni1−(x+y)CoxMyO; and (c)mixing the nickel oxide and a lithium compound to obtain a mixture and heating the mixture at a temperature not lower than 700° C. and not higher than 850° C. to produce a lithium-containing composite oxide which is represented by the general formula LiNi1−(x+y)CoxMyO2, where 0.1≦x≦0.35 and 0.03≦y≦0.2 are satisfied and M is at least one selected from the group consisting of Al, Ti and Sn.

    摘要翻译: 通过以下方法制造正极活性物质,该正极活性物质通过以下方法制备能够抑制由于电池反应在低温环境中引起的电阻而具有高输入/输出能力的非水电解质二次电池:(a)提供氢氧化镍 其由下列通式表示:Ni 1 - (x + y)2(x)y(x)y(OH)2&lt; >,(b)在不低于600℃且不高于1000℃的温度下加热氢氧化镍以产生由通式Ni 1-(x + y)表示的氧化镍, Co x;;;;;;;;;;;;;;;;;;;;;;;;;;;;; 和(c)将氧化镍和锂化合物混合以获得混合物,并在不低于700℃且不高于850℃的温度下加热该混合物,以制备由下式表示的含锂复合氧化物: 通式为LiNi 1 - (x + y)2 O x O 2 O 2,其中0.1 <= x <= 0.35和0.03 <= y <= 0.2,M为选自Al,Ti和Sn中的至少一种。

    Positive electrode active material for non-aqueous electrolyte secondary battery, production method thereof, and non-aqueous electrolyte secondary battery using the same
    4.
    发明授权
    Positive electrode active material for non-aqueous electrolyte secondary battery, production method thereof, and non-aqueous electrolyte secondary battery using the same 失效
    非水电解质二次电池用正极活性物质及其制造方法以及使用其的非水电解质二次电池

    公开(公告)号:US07666551B2

    公开(公告)日:2010-02-23

    申请号:US11097280

    申请日:2005-04-04

    IPC分类号: H01M4/58 H01M4/52

    摘要: A positive electrode active material for a non-aqueous electrolyte secondary battery of this invention includes: a lithium nickel composite oxide containing lithium, nickel, and at least one metal element other than lithium and nickel; and a layer containing lithium carbonate, aluminum hydroxide, and aluminum oxide, the layer being carried on the surface of the lithium nickel composite oxide. The lithium nickel composite oxide is composed such that the ratio of the nickel to the total of the nickel and the at least one metal element is 30 mol % or more. The layer is composed such that the amount of the lithium carbonate is 0.5 to 5 mol per 100 mol of the lithium nickel composite oxide. The total of aluminum atoms contained in the aluminum hydroxide and the aluminum oxide is 0.5 to 5 mol per 100 mol of the lithium nickel composite oxide.

    摘要翻译: 本发明的非水电解质二次电池用正极活性物质,其特征在于,含有锂,镍,锂和镍以外的至少一种金属元素的锂镍复合氧化物, 和含有碳酸锂,氢氧化铝和氧化铝的层,该层承载在锂镍复合氧化物的表面上。 锂镍复合氧化物的组成使得镍与镍和至少一种金属元素的总量的比例为30摩尔%以上。 该层的组成使得碳酸锂的量相对于每100摩尔锂镍复合氧化物为0.5〜5摩尔。 铝氢氧化物和氧化铝中所含的铝原子总量相对于每100摩尔锂镍复合氧化物为0.5〜5摩尔。

    Negative electrode for non-aqueous electrolyte secondary battery, manufacturing method therefor, and non-aqueous electrolyte secondary battery
    9.
    发明授权
    Negative electrode for non-aqueous electrolyte secondary battery, manufacturing method therefor, and non-aqueous electrolyte secondary battery 失效
    非水电解质二次电池用负极及其制造方法以及非水电解质二次电池

    公开(公告)号:US07638239B2

    公开(公告)日:2009-12-29

    申请号:US11289681

    申请日:2005-11-30

    IPC分类号: H01M4/58

    摘要: In a negative electrode for a non-aqueous electrolyte secondary battery including an active material portion capable of electrochemically absorbing and desorbing Li, a current collector carrying the active material portion, and a buffer interposed between the active material portion and the current collector, the active material portion includes at least one selected from the group consisting of a Si simple substance, a Si alloy, and a Si compound, the current collector includes Cu, and the buffer has a first layer contacting the current collector and including a group A element which is at least one selected from the group A consisting of Sn, Al, and In, and a second layer contacting the active material portion and including a group B element which is at least one selected from the group B consisting of transition metal elements other than Cu.

    摘要翻译: 在含有能够电化学吸收和解吸Li的活性物质部分的非水电解质二次电池用负极中,携带有活性物质部分的集电体和介于活性物质部分和集电体之间的缓冲剂,活性物质 材料部分包括选自由Si单质,Si合金和Si化合物组成的组中的至少一种,集电体包括Cu,并且缓冲层具有与集电体接触的第一层,并且包括A族元素, 是选自由Sn,Al和In构成的组A中的至少一种,第二层与活性物质部分接触,并且包含B族元素,该B族元素是选自除B以外的过渡金属元素的组B中的至少一种 铜。