Cationic fiberglass size
    111.
    发明申请
    Cationic fiberglass size 审中-公开
    阳离子玻璃纤维尺寸

    公开(公告)号:US20090162609A1

    公开(公告)日:2009-06-25

    申请号:US12004875

    申请日:2007-12-21

    IPC分类号: E04D3/06 B32B27/02

    摘要: A sizing composition for reinforcement fibers that includes a cationic modified polyurethane dispersion, one or more silane coupling agents, and at least one lubricant is provided. The cationic modified polyurethane dispersion includes a dual end-capped polyurethane selected from a silane-terminated polyurethane, a ketoxime-terminated polyurethane, or a hybrid silane/ketoxime-terminated polyurethane where one end of the polyurethane is terminated with a silane group and the opposing end is terminated with a ketoxime group. The size composition is applied to reinforcement fibers and formed into chopped strand, wet-laid mats that can be used for a variety of purposes, including roofing products. Chopped strand mats formed from fibers sized with the inventive sizing composition maintains or improves the dry tear strengths and wet strengths compared to chopped strand mats made from fibers sized with a commercial sizing composition that does not contain a modified cationic polyurethane dispersion (e.g., SPUD).

    摘要翻译: 提供了包含阳离子改性聚氨酯分散体,一种或多种硅烷偶联剂和至少一种润滑剂的增强纤维用施胶组合物。 阳离子改性聚氨酯分散体包括选自硅烷封端的聚氨酯,酮肟封端的聚氨酯或混合硅烷/酮肟封端的聚氨酯的双端封聚氨酯,其中聚氨酯的一端用硅烷基团终止, 末端用酮肟组终止。 尺寸组合物用于增强纤维并形成短切纤维,可用于各种目的的湿敷垫,包括屋顶产品。 由使用本发明的施胶组合物尺寸的纤维形成的切断的丝网垫与由不含改性阳离子聚氨酯分散体(例如SPUD)的商业施胶组合物尺寸的纤维制成的短切丝网垫相比,保持或改善干燥撕裂强度和湿强度, 。

    SYSTEM AND METHOD FOR PREVENTING USER O.S. IN VMM SYSTEM FROM DEENERGIZING DEVICE BEING USED BY SERVICE O.S.
    112.
    发明申请
    SYSTEM AND METHOD FOR PREVENTING USER O.S. IN VMM SYSTEM FROM DEENERGIZING DEVICE BEING USED BY SERVICE O.S. 有权
    用于防止用户的系统和方法 在由服务使用的设备使用的VMM系统中

    公开(公告)号:US20090144570A1

    公开(公告)日:2009-06-04

    申请号:US11949983

    申请日:2007-12-04

    IPC分类号: G06F1/32

    摘要: A call from a user operating system (UOS) to BIOS to configure a connected device into a reduced energy consumption mode is routed through a virtual machine monitor (VMM). The VMM determines whether a service O.S. (SOS) is in need of the device and if so the VMM informs the UOS that the device has been configured as ordered, while allowing the SOS to complete its task with the device. If the SOS is not in need of the device, or at the completion of the SOS task with the device, the VMM passes the call to ACPI/BIOS to configure the device in the demanded energy consumption mode.

    摘要翻译: 通过虚拟机监视器(VMM)路由从用户操作系统(UOS)到BIOS的将连接的设备配置为降低的能量消耗模式的呼叫。 VMM确定一个服务O.S. (SOS)需要该设备,如果是这样,则VMM通知UOS设备已被配置为有序,同时允许SOS完成其与该设备的任务。 如果SOS不需要设备,或者在使用设备完成SOS任务时,VMM会将呼叫传递给ACPI / BIOS,以将设备配置为所需能量消耗模式。

    SEMICONDUCTOR PHOTODETECTORS
    113.
    发明申请
    SEMICONDUCTOR PHOTODETECTORS 有权
    SEMICONDUCTOR PHOTODETEORS

    公开(公告)号:US20090101909A1

    公开(公告)日:2009-04-23

    申请号:US12253497

    申请日:2008-10-17

    IPC分类号: H01L31/0368 H01L31/18

    摘要: In one aspect, a method includes forming a pit in a top surface of a substrate by removing a portion of the substrate and growing a semiconductor material with a bottom surface on the pit, the semiconductor material different than the material of the substrate. The pit has a base recessed in the top surface of the substrate. In another aspect, a structure includes a substrate having a top surface, the substrate including at least one pit having a base lower than the top surface of the substrate, and a semiconductor material having a bottom surface formed on the base of the pit.

    摘要翻译: 一方面,一种方法包括通过去除衬底的一部分并在凹坑上生长具有底表面的半导体材料,半导体材料与衬底的材料不同,在衬底的顶表面中形成凹坑。 凹坑具有凹陷在基板的顶表面中的基部。 在另一方面,一种结构包括具有顶表面的基底,该基底包括至少一个具有低于基底顶表面的基底的凹坑,以及在凹坑底部形成有底表面的半导体材料。

    Auto-discovery and management of base station neighbors in wireless networks
    114.
    发明申请
    Auto-discovery and management of base station neighbors in wireless networks 有权
    无线网络中基站邻居的自动发现和管理

    公开(公告)号:US20090052350A1

    公开(公告)日:2009-02-26

    申请号:US12221951

    申请日:2008-08-08

    IPC分类号: H04W48/16 H04L12/28

    摘要: Systems and methods are disclosed that include determining a local node configuration for a local network node. The local network node configuration can include a local range and a local location. In addition, these systems and methods can include receiving a remote network node configuration for a remote network node via a communications link. The remote network node configuration can include a remote range and a remote location. Also these systems and methods can further include generating a neighbor list that includes the remote network node and the local network node. The neighbor list can be determined using the local network node configuration and the remote network node configuration.

    摘要翻译: 公开了包括确定本地网络节点的本地节点配置的系统和方法。 本地网络节点配置可以包括本地范围和本地位置。 另外,这些系统和方法可以包括经由通信链路为远程网络节点接收远程网络节点配置。 远程网络节点配置可以包括远程范围和远程位置。 而且这些系统和方法还可以包括生成包括远程网络节点和本地网络节点的邻居列表。 可以使用本地网络节点配置和远程网络节点配置来确定邻居列表。

    Process for Refining Ganoderma Spore Polysacchoride
    116.
    发明申请
    Process for Refining Ganoderma Spore Polysacchoride 审中-公开
    精制灵芝孢子多糖的工艺

    公开(公告)号:US20080112967A1

    公开(公告)日:2008-05-15

    申请号:US11563769

    申请日:2006-11-28

    IPC分类号: A61K36/06 C12P19/04

    CPC分类号: A61K36/074

    摘要: The present invention discloses a process for refining Ganoderma spore polysacchoride. The process comprise the step of: Remove the impurity in the Ganoderma spores, warm water extraction, alcohol precipitation, separate precipitate, obtain the impure polysacchoride, adjust pH to 7.5-8.5, centrifuge to removal deposit, take out supernatent, add H2O2 to decolor, deproteined by sevag method, dialyses, alcohol precipitation, wash the precipitate, dry in the vacuum to get the pure Ganoderma spore polysacchoride.

    摘要翻译: 本发明公开了一种精制灵芝孢子多糖的方法。 该过程包括以下步骤:去除灵芝孢子中的杂质,温水萃取,酒精沉淀,分离沉淀,得到不纯多糖,调pH至7.5-8.5,离心去除沉淀物,取出上清液,加入H

    Apparatus and method for fiber batt foam encapsulation
    117.
    发明授权
    Apparatus and method for fiber batt foam encapsulation 失效
    纤维絮泡泡沫包封装置及方法

    公开(公告)号:US07083693B2

    公开(公告)日:2006-08-01

    申请号:US10789208

    申请日:2004-02-27

    IPC分类号: B32B5/20 B32B5/28 B32B31/12

    摘要: Disclosed is an apparatus and a method for at least partially encapsulating a fiber batt or other highly porous substrate by applying a polymeric foam layer to one or more surfaces of the fiber batt. The foam application assemblies are arranged and configured to extrude a polymeric foam or a foaming mixture onto the surface(s) of the fiber batt to be coated. A combination of foam application assemblies may be provided in either fixed or moveable configurations for coating one or more sides of the fiber batt. The encapsulation of the fiber batt may also include a premanufactured material layer on one or more surfaces that may be exposed or may also be encapsulated below the polymeric foam layer.

    摘要翻译: 公开了一种用于通过将聚合物泡沫层施加到纤维絮垫的一个或多个表面来至少部分地包封纤维絮垫或其它高度多孔的基材的装置和方法。 泡沫施加组件被布置和构造成将聚合物泡沫或发泡混合物挤出到待涂覆的纤维絮垫的表面上。 泡沫施加组件的组合可以以固定的或可移动的构造提供,用于涂覆纤维絮垫的一个或多个侧面。 纤维絮垫的包封还可以包括在一个或多个表面上的预制材料层,其可以被暴露或也可以包封在聚合物泡沫层的下面。

    Method for determining cure in a polycarboxylic acid bindered material

    公开(公告)号:US07063983B2

    公开(公告)日:2006-06-20

    申请号:US10160775

    申请日:2002-05-31

    申请人: Liang Chen

    发明人: Liang Chen

    IPC分类号: G01N33/00

    摘要: By utilizing a pH indicator having known color change characteristics, an accurate determination of the pH of a binder surface, and hence the amount of cure of a polycarboxylic acid based binder on the fiberglass fibers, can be easily determined for polycarboxylic binder based fiberglass materials used in insulation and composite applications. Based on these results, the manufacturing line used to make these bindered materials may be adjusted to ensure adequate curing at maximum efficiency while minimizing operating costs and reducing waste.

    Low odor insulation binder from phosphite terminated polyacrylic acid
    119.
    发明授权
    Low odor insulation binder from phosphite terminated polyacrylic acid 有权
    来自亚磷酸酯封端的聚丙烯酸的低气味绝缘粘合剂

    公开(公告)号:US06933349B2

    公开(公告)日:2005-08-23

    申请号:US09814034

    申请日:2001-03-21

    摘要: A binder composition, obtained by polymerizing acrylic acid monomer in water in the presence of a cure accelerator comprising an alkali metal salt of a phosphorous-containing inorganic acid to form a low molecular weight polyacrylic acid and subsequently reacting said low molecular weight polyacrylic acid with a polyhydroxy crosslinking agent in a crosslinking step to make a composition suitable for use as a component in a binder for fiberglass. A significant improvement involves conducting the crosslinking step in the absence of added catalyst. Moreover, satisfactory results are obtained in the absence of conventional undesirable sulfur odors.

    摘要翻译: 一种粘合剂组合物,其通过在包含含磷无机酸的碱金属盐的固化促进剂存在下在水中聚合以形成低分子量聚丙烯酸,随后使所述低分子量聚丙烯酸与 多羟基交联剂在交联步骤中制备适于用作玻璃纤维粘合剂中组分的组合物。 显着的改进包括在不加入催化剂的情况下进行交联步骤。 此外,在没有常规的不希望的硫气味的情况下,可获得令人满意的结果。

    Cosmetic composition
    120.
    发明申请
    Cosmetic composition 失效
    化妆品组成

    公开(公告)号:US20050142086A1

    公开(公告)日:2005-06-30

    申请号:US10748945

    申请日:2003-12-29

    CPC分类号: A61K8/28 A61K8/86 A61Q15/00

    摘要: A composition comprising an antiperspirant or deodorant active and which is substantially free of alcohol and has a viscosity of less than 100 centipoise and a contact angle less than 90°. A product comprising the composition marketed in a porous dome applicator.

    摘要翻译: 一种组合物,其包含止汗剂或除臭剂活性物质,其基本上不含醇,并且具有小于100厘泊的粘度和小于90°的接触角。 一种产品,其包含在多孔圆顶涂敷器中销售的组合物。