Circuit and method for interconnecting stacked integrated circuit dies
    141.
    发明申请
    Circuit and method for interconnecting stacked integrated circuit dies 有权
    用于互连堆叠集成电路管芯的电路和方法

    公开(公告)号:US20080272478A1

    公开(公告)日:2008-11-06

    申请号:US11800472

    申请日:2007-05-04

    IPC分类号: H01L23/02 H01L21/30 H01L23/48

    摘要: Signals are routed to and from identical stacked integrated circuit dies by selectively coupling first and second bonding pads on each of the dies to respective circuits fabricated on the dies through respective transistors. The transistors connected to the first bonding pads of an upper die are made conductive while the transistors connected to the second bonding pads of the upper die are made non-conductive. The transistors connected to the second bonding pads of a lower die are made conductive while the transistors connected to the first bonding pads of the lower die are made non-conductive. The second bonding pads of the upper die are connected to the second bonding pads of the lower die through wafer interconnects extending through the upper die. Signals are routed to and from the circuits on the first and second dies through the first and second bonding pads, respectively.

    摘要翻译: 通过选择性地将每个管芯上的第一和第二接合焊盘与通过相应的晶体管在管芯上制造的各个电路相耦合,将信号路由至相同的堆叠集成电路管芯。 连接到上模的第一接合焊盘的晶体管导通,而连接到上模的第二焊盘的晶体管是不导电的。 连接到下模的第二接合焊盘的晶体管被​​导通,而连接到下模的第一焊盘的晶体管导通。 上模的第二接合焊盘通过延伸穿过上模的晶片互连连接到下模的第二焊盘。 信号分别通过第一和第二接合焊盘被引导到第一和第二裸片上的电路和从第一和第二裸片上的电路。

    Catalyst Composition Comprising Anionic Clay and Rare Earth Metals, Its Preparation and Use in Fcc
    143.
    发明申请
    Catalyst Composition Comprising Anionic Clay and Rare Earth Metals, Its Preparation and Use in Fcc 有权
    催化剂组合物包含阴离子粘土和稀土金属,其制备和用途在Fcc

    公开(公告)号:US20080039314A1

    公开(公告)日:2008-02-14

    申请号:US10582177

    申请日:2004-12-06

    IPC分类号: B01J21/16 B01J23/10

    摘要: The invention relates to a catalyst composition comprising anionic clay, lanthanum (hydr)oxide carbonate, and cerium oxide. This composition can suitably be used in FCC for the reduction of NOx and/or SOx emissions, the reduction of the S and/or N-content in fuels, and as a metal trap. The composition can be prepared by forming a precipitate from a solution comprising a divalent metal salt, a trivalent metal salt, a lanthanum salt, and a cerium salt, calcining the precipitate at 200-800° C., and rehydrating the calcined precipitate in the presence of a carbonate source to form a composition comprising anionic clay, lanthanum (hydr)oxide carbonate, and cerium oxide.

    摘要翻译: 本发明涉及包含阴离子粘土,氧化镧(hydr),碳酸氧化铈和氧化铈的催化剂组合物。 该组合物可以适当地用于FCC中以减少NO x和/或SO x x排放,降低燃料中S和/或N含量,以及 作为金属陷阱。 该组合物可以通过从包含二价金属盐,三价金属盐,镧盐和铈盐的溶液中形成沉淀物来制备,在200-800℃煅烧沉淀物,并将煅烧后的沉淀物再水化 存在碳酸盐源以形成包含阴离子粘土,氧化镧(hydr),碳酸氧化铈和氧化铈的组合物。

    Process For The Preparation Of An Additive-Containing Anionic Clay
    145.
    发明申请
    Process For The Preparation Of An Additive-Containing Anionic Clay 失效
    含添加剂阴离子粘土的制备方法

    公开(公告)号:US20080032883A1

    公开(公告)日:2008-02-07

    申请号:US11587393

    申请日:2005-04-26

    申请人: William Jones

    发明人: William Jones

    IPC分类号: C04B33/00

    摘要: Process for the preparation of an additive-containing anionic clay comprising the steps of (a) preparing a physical mixture of a divalent and a trivalent metal compound, (b) calcining the physical mixture at a temperature in the range 200-800° C. without performing a prior aging or shaping step, thereby forming a product containing at least 5 wt % of a rehydratable compound, and (c) rehydrating the calcined mixture in aqueous suspension containing an additive to form the additive-containing anionic clay. This process provides a simple and cost-effective way of preparing additive-containing anionic clays. The process does neither require aging or reaction steps before calcination, nor does it require precipitation of metal salts or the handling of inhomogeneous slurries.

    摘要翻译: 制备含添加剂的阴离子粘土的方法包括以下步骤:(a)制备二价和三价金属化合物的物理混合物,(b)在200-800℃的温度下煅烧该物理混合物。 从而形成含有至少5重量%的可再水化合物的产品,和(c)将含有添加剂的含水悬浮液中的煅烧混合物再水合以形成含添加剂的阴离子粘土。 该方法提供了制备含添加剂的阴离子粘土的简单和成本有效的方法。 该方法既不需要煅烧前的老化或反应步骤,也不需要沉淀金属盐或处理不均匀的浆料。

    Process for treating steel alloys
    149.
    发明申请
    Process for treating steel alloys 审中-公开
    钢合金处理工艺

    公开(公告)号:US20070068601A1

    公开(公告)日:2007-03-29

    申请号:US11234851

    申请日:2005-09-26

    IPC分类号: C23C8/22 C21D1/773

    CPC分类号: C23C8/02 C23C8/22

    摘要: The process includes heating of steel alloy parts in the presence of hydrogen prior to introduction of, for example, carburizing gas, preferably acetylene, in the presence of a diluent carrier gas. The process uses a continuous cycle involving only one carburizing (boost) step and one diffusion step, and high velocity gas quenching. The process is advantageously carried out in a unique, versatile vacuum furnace (also having high internal pressure capability) that provides very high velocity, continuous flow gas quenching, and a furnace design, including a long, low profile work zone configuration and quench gas recirculation equipment and flow pattern that facilitates high velocity gas flow. The entire process is accomplished in a single self-contained chamber of the furnace.

    摘要翻译: 该方法包括在引入例如渗碳气体(优选乙炔)之前,在稀释剂载体气体的存在下,在氢的存在下加热钢合金部件。 该过程使用仅包括一个渗碳(升压)步骤和一个扩散步骤以及高速气体淬火的连续循环。 该方法有利地在独特的多功能真空炉(也具有高的内部压力能力)中进行,其提供非常高的速度,连续的流动气体淬火和炉设计,其包括长的低轮廓工作区构型和骤冷气体再循环 便于高速气流的设备和流程图。 整个过程在炉的单个独立的室中完成。