Abstract:
An aqueous dispersion and an aqueous coating composition comprising the aqueous dispersion, and the aqueous coating composition providing coatings made therefrom with improved anti-corrosion property and good water resistance and block resistance.
Abstract:
The present invention provides two-component polyurethane compositions that are substantially free of VOCs and comprising, as one component, polyisocyanate compositions and, as a second component, a polyol which is chosen from a cycloaliphatic diol or polyol having a molecular weight of from 100 to 500 and containing one or more 4 to 7 member aliphatic ring and an oligomeric diol or polyol comprising the condensation reaction product of from 30 wt. % to 78 wt. %, based on the total weight of reactants used to make the oligomer, and an acrylic or vinyl emulsion polymer.
Abstract:
The present invention provides two-component polyurethane compositions that are substantially free of VOCs and comprising, as one component, polyisocyanate compositions and, as a second component, a polyol which is chosen from a cycloaliphatic diol or polyol having a molecular weight of from 100 to 500 and containing one or more 4 to 7 member aliphatic ring and an oligomeric diol or polyol comprising the condensation reaction product of from 30 wt. % to 78 wt. %, based on the total weight of reactants used to make the oligomer, and an acrylic or vinyl emulsion polymer.
Abstract:
A two-component polyurethane composition comprising: an aqueous dispersion comprising an emulsion polymer and a specific sulphate and/or sulfonate surfactant, and a water-dispersible polyisocyanate; the emulsion polymer with a weight average molecular weight of 70,000 g/mol or less comprising, by weight based on the weight of the emulsion polymer, greater than 0.25% of structural units of a phosphorous-containing acid monomer and/or salts thereof, greater than 15% of structural units of a hydroxy-functional alkyl (meth)acrylate, structural units of an monoethylenically unsaturated nonionic monomer, and from zero to 10% of structural units of an additional acid monomer and/or salts thereof; and a process of preparing the two-component polyurethane composition.
Abstract:
A stable two-component waterborne coating composition comprising an epoxy component A comprising a waterborne epoxy resin, a polymeric dispersant, and pigments and/or extenders; and a component B comprising a curing agent; providing coatings made therefrom with improved anti-corrosion properties; and a method of preparing the coating composition.
Abstract:
A two-component polyurethane composition comprising (A) an aqueous dispersion comprising an emulsion polymer and from 2% to 20% of an alcohol alkoxylate of formula (I), by weight based on the weight of the emulsion polymer, and (B) a polyisocyanate; the two-component polyurethane composition can provide coatings with a high distinctness of image.
Abstract:
An aqueous dispersion comprising a multistage polymer comprising a first polymer and a second polymer that comprises structural units of an ethylenically unsaturated siloxane monomer, the multistage polymer comprising, by weight based on the weight of the multistage polymer, 4.5% or more of structural units of the ethylenically unsaturated siloxane monomer, and the coagulum content of the aqueous dispersion is less than 2,000 ppm after filtration through a 44 micron sieve.
Abstract:
An aqueous polymer dispersion and an aqueous coating composition comprising the aqueous polymer dispersion, and the aqueous coating composition providing the resulting coatings with good anti-corrosion property.