Abstract:
A polymer comprises reaction product of (a) one or more diacid, diester thereof, glycolide, and (b) one or more polyol, wherein component (a) comprises glycolide or combinations thereof, and component (b) comprises one or more polyol comprising a mixture of 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol, or 2,2,4,4-tetramethyl-1,3-cyclobutanediol, or combinations thereof.
Abstract:
The instant invention is a composite dispersion, method of producing the same, and articles made therefrom. The composite dispersion according to the instant invention comprises (1) a first seed dispersion comprising (a) a first internal phase; and (b) an external phase, and (2) a second internal phase; wherein the composite dispersion comprises more than 60 percent by the combined weight of the first internal phase and the second internal phase, and the composite dispersion has a viscosity of less than 10,000 cP measured by RV4 spindle at 20 rpm at greater than 60 weight percent total internal phase, and wherein the composite dispersion has a bimodal particle size distribution and a particle size ratio (P2/P1) in the range of 2 to 200.
Abstract:
A shrink film comprising a polyethylene-based film having a top surface, a bottom surface, and comprising one or more layers, wherein at least one layer of the polyethylene-based film comprises a low density polyethylene having a density of from 0.917 g/cc to 0.935 g/cc and melt index, I2, of from 0.1 g/10 min to 5 g/10 min, a linear low density polyethylene having a density of from 0.900 g/cc to 0.965 g/cc and melt index, I2, of from 0.05 g/10 min to 15 g/10 min, or combinations thereof, and optionally, a medium density polyethylene, a high density polyethylene, or combinations thereof, and a coating layer disposed on the top surface of the polyethylene-based film, wherein the coating layer comprises an adhesive and a material that absorbs radiation in the near-infrared, visible, and ultraviolet spectral wavelength ranges.
Abstract:
A polymer comprising reaction product of (a) one or more diacid or diester thereof, and (b) one or more polyol, wherein component (a) comprises 5 to 100 mole %, based on the total amount of component (a), of 2,5-furan dicarboxylic acid (FDCA), or one or more C1 to C10 alkyl diester thereof, and component (b) comprises a mixture of 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol, or 2,2,4,4-tetramethyl-1,3-cyclobutanediol, or combinations thereof.
Abstract:
A polymer comprises reaction product of (a) one or more diacid, diester thereof, glycolide, and (b) one or more polyol, wherein component (a) comprises glycolide or combinations thereof, and component (b) comprises one or more polyol comprising a mixture of 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol, or 2,2,4,4-tetramethyl-1,3-cyclobutanediol, or combinations thereof.
Abstract:
The instant invention is a pressure sensitive adhesive composition comprising an ultra-high solid polyurethane dispersion. The ultra-high solid polyurethane dispersion comprises (1) a first component comprising a first polyurethane prepolymer comprising the reaction product of a polyol and polyisocyanate, (2) a second component comprising a media phase selected from the group consisting of a second polyurethane prepolymer emulsion, a low solid content polyurethane dispersion, a seed latex, and combinations thereof; and (3) optionally a chain extender. The ultra-high solid polyurethane dispersion has at least a solid content of at least 60 percent by weight of solid content, based on the total weight of the ultra-high solid polyurethane dispersion, and a viscosity of less than 5000 cps at 20 rpm at 21° C. using spindle #4 with Brookfield viscometer.
Abstract:
The instant invention is a composite dispersion, method of producing the same, and articles made therefrom. The composite dispersion according to the instant invention comprises (1) a first seed dispersion comprising (a) a first internal phase; and (b) an external phase, and (2) a second internal phase; wherein the composite dispersion comprises more than 60 percent by the combined weight of the first internal phase and the second internal phase, and the composite dispersion has a viscosity of less than 10,000 cP measured by RV4 spindle at 20 rpm at greater than 60 weight percent total internal phase, and wherein the composite dispersion has a bimodal particle size distribution and a particle size ratio (P2/P1) in the range of 2 to 200.
Abstract:
The instant disclosure provides a die assembly for producing an annular microcapillary product. The die assembly is operatively connectable to an extruder having a thermoplastic material passing therethrough. The die assembly includes a shell, an inner manifold, an outer manifold, and a die assembly. The inner and outer manifolds are positionable in the shell with matrix flow channels thereabout to receive the thermoplastic material therethrough such that matrix layers of the thermoplastic material are extrudable therefrom. The die insert is disposable between the inner and the outer manifolds, and has a distribution manifold with a tip at an end thereof defining microcapillary channels to pass a microcapillary material therethrough whereby microcapillaries are formed between the matrix layers.
Abstract:
A barrier film comprising a polyester-based polymer with (a) an O2 gas permeability of 0.25 cc-mil/100 in.2 24 hrs atm (5 cc 20 μm/m2 24 hrs atm) at 80% relative humidity (ASTM D-3985) or less, (b) a moisture permeability of 0.5 g-mil/100 in.2 24 hrs atm (9.8 g 20 μm/m2 24 hrs atm) at 38° C. (ASTM F-1249) or less, (c) haze of 1% or less (ASTM D1003), and (d) a glass transition temperature of 100° C. or higher. The polyester-based polymer may comprise reaction product of (a) one or more diacid or diester thereof, and (b) one or more polyol, wherein component (a) comprises 5 to 100 mole %, based on the total amount of component (a), of 2,5-furan dicarboxylic acid, or one or more C1 to C10 alkyl diester thereof, and component (b) comprises ethylene glycol, a mixture of 1,3-cyclohexanedimethanol and 1,4-cyclohexanedimethanol, or 2,2,4,4-tetramethyl-1,3-cyclobutanediol, or combinations thereof.
Abstract translation:包含聚酯基聚合物的隔离膜,其具有(a)在80%相对湿度下的氧气渗透率为0.25cc密尔/ 100in.2,24小时atm(5cc20μm/ m 2 24小时atm)(ASTM D- 3985)或更小,(b)在38℃下24小时大气压(9.8g20μm/ m 2 24小时atm)下的透湿度为0.5g密耳/ 100(ASTM F-1249)或更低,( c)雾度为1%以下(ASTM D1003),(d)玻璃化转变温度为100℃以上。 基于聚酯的聚合物可以包含(a)一种或多种二酸或二酯的反应产物和(b)一种或多种多元醇,其中组分(a)占组分总量的5-100摩尔% a),2,5-呋喃二羧酸或其一个或多个C1至C10烷基二酯,组分(b)包括乙二醇,1,3-环己烷二甲醇和1,4-环己烷二甲醇的混合物,或2, 2,4,4-四甲基-1,3-环丁二醇或其组合。