Abstract:
A polyethylene composition including the product of the combination of at least one copolymer made from units derived from at least 85 wt % ethylene and a C3 to C10 α-olefin and from 0.10 wt % to 10 wt % of a cyclic-diene terpolymer is provided.
Abstract:
Polymer compositions that include an ethylene-based polymer and a broad molecular weight distribution propylene-based polymer having a melt strength of 20.0 cN to 200.0 cN; and optionally, a propylene-based elastomer are described. The invention also includes articles, such as films, produced from such compositions and methods of making such compositions and methods of improving melt strength.
Abstract:
The present invention relates to a branched modifier and a composition comprising more than 25 wt % (based on the weight of the composition) of one or more linear ethylene polymers having a g′vis of 0.97 or more and an Mw of 20,000 g/mol or more and at least 0.1 wt % of a branched modifier where the modifier has a) a g′vis of 0.70 or less; b) an Mw of 100,000 g/mol or more; c) an Mw/Mn of 4.0 or more; d) a shear thinning ratio of 110 or more, e) a melt strength of 10 cN or more; f) a complex viscosity at 0.1 rad/sec at 190° C. of at least 130,000 Pa·s; and g) a phase angle of Z° or less where Z=138.3 G*(−0.142), where G* is the complex modulus reported in Pascals measured at 190° C. and the phase angle units are reported in degrees, wherein the G* is from 1,000 to 1,000,000 Pa.
Abstract:
The present invention relates to a blown film comprising more than 25 wt % (based on the weight of the composition) of one or more linear ethylene polymers having a g′vis of 0.97 or more and an Mw of 20,000 g/mol or more and at least 0.1 wt % of a branched modifier where the modifier has a) a g′vis of 0.90 or less; b) an Mw of 100,000 g/mol or more; c) an Mw/Mn of 3.0 or more; d) an Mz/Mn of 7.0 or more; e) optionally, an Mz of 2,000,000 g/mol or less; and f) a shear thinning ratio of 40 or more.
Abstract:
The present invention relates to a branched modifier and a composition comprising more than 25 wt % (based on the weight of the composition) of one or more linear ethylene polymers having a g′vis of 0.97 or more and an Mw of 20,000 g/mol or more and at least 0.1 wt % of a branched modifier where the modifier has a) a g′vis of 0.70 or less; b) an Mw of 100,000 g/mol or more; c) an Mw/Mn of 4.0 or more; d) a shear thinning ratio of 110 or more, e) a melt strength of 10 cN or more; f) a complex viscosity at 0.1 rad/sec at 190° C. of at least 130,000 Pa·s; and g) a phase angle of Z° or less where Z=138.3G*(−0.142), where G* is the complex modulus reported in Pascals measured at 190° C. and the phase angle units are reported in degrees, wherein the G* is from 1,000 to 1,000,000 Pa.
Abstract:
A method of forming a blown film comprising extruding a molten composition through a die opening to form a film; wherein the molten composition comprises at least one polyethylene and within the range from 0.10 wt % to 10 wt % of a cyclic-diene terpolymer by weight of the composition; causing the film to progress in a direction away from the die opening; cooling the film at a distance from the die opening, the distance adjusted to effect the properties of the film; and isolating a blown film therefrom.
Abstract:
A method of forming a finished film comprising extruding a molten polyethylene comprising a diene terpolymer modifier through a die opening to form a film, wherein the diene-terpolymer modifier is a terpolymer comprising ethylene-derived units, C3 to C10 α-olefin derived units, and diene-derived units; causing the film to progress in a direction away from the die opening; cooling the film at a distance from the die opening, the distance adjusted to allow relaxation of the molten polyethylene prior to solidification and/or crystallization upon cooling; and isolating a finished film therefrom. Desirably, the polyethylene is a linear low density polyethylene, and the die and cooling is suitable for forming a blown film.
Abstract:
A method of forming a blown film comprising extruding a molten composition through a die opening to form a film; wherein the molten composition comprises at least one polyethylene and within the range from 0.10 wt % to 10 wt % of a cyclic-diene terpolymer by weight of the composition; causing the film to progress in a direction away from the die opening; cooling the film at a distance from the die opening, the distance adjusted to effect the properties of the film; and isolating a blown film therefrom.
Abstract:
The present invention relates to a cast film comprising a composition comprising more than 25 wt % (based on the weight of the composition) of one or more linear ethylene polymers having a g′vis of 0.97 or more and an Mw of 20,000 g/mol or more and at least 0.1 wt % of a branched modifier where the modifier has a) a g′vis of 0.90 or less; b) an Mw of 100,000 g/mol or more; c) an Mw/Mn of 3.0 or more; d) an Mz/Mn of 7.0 or more; e) a shear thinning ratio of 40 or more; and f) an I21 of 20 dg/min or less; where the film has at least a 10% reduction in neck-in as compared to the same composition formed into a film under the same conditions, except that the branched modifier is absent.
Abstract:
The present invention relates to polyethylene compositions comprising one or more ethylene polymers and one or more HDPE modifiers, in particular, this invention further relates to polyethylene blends comprising one or more ethylene polymers and one or more HDPE modifiers, wherein the modifier has: 1) a density of greater than 0.94 g/cc; 2) a Mw/Mn greater than 5; 3) a melt index (ASTM 1238, 190° C., 2.16 kg) of less than 0.7 dg/min; and 4) a g′vis of 0.96 or less.