METHOD FOR PREPARING A BENZOPHENONE DERIVATIVE

    公开(公告)号:US20220033580A1

    公开(公告)日:2022-02-03

    申请号:US17298103

    申请日:2019-12-02

    Abstract: The present invention is method comprising the steps of a) contacting 4-hydroxyphenone and a salt thereof with propylene oxide in a reactor heated to a temperature in the range of from 100° C. to 200° C. to form a poly(propylene oxide)-benzophenone intermediate; then b) contacting the intermediate with ethylene oxide in the heated reactor to form an alkoxylated benzophenone substituted with propylene oxide groups and ethylene oxide groups. The method of the present invention is useful for preparing a non-volatile alkoxylated benzophenone photoinitiator that gives long lasting gloss retention in an exterior architectural coating.

    CARBOXYL GROUP CONTAINING ACRYLIC RDP AND DRY MIX CEMENT FORMULATIONS CONTAINING THEM
    26.
    发明申请
    CARBOXYL GROUP CONTAINING ACRYLIC RDP AND DRY MIX CEMENT FORMULATIONS CONTAINING THEM 有权
    包含丙烯酸RDP和含有它们的干混合水泥配方的羧基

    公开(公告)号:US20150111995A1

    公开(公告)日:2015-04-23

    申请号:US14383586

    申请日:2013-03-05

    Abstract: The present invention provides water redispersible polymer powder (RDP) compositions that perform well even when redispersibility is fair comprising carboxyl group containing multi-stage acrylic copolymers having an alkali-soluble resin outer stage and one or more inner stage acrylic (co)polymer having a glass transition temperature (Tg) of from −40 to 50° C., one or more nucleating agent having a boiling point of 150° C. to 500° C., and a water solubility of 3.5% or less, preferably, an alkyl isobutyrate and a branched alkyl isobutyrate, and one or more colloidal stabilizer. Also provided are dry mix cement tile adhesive compositions comprising the water redispersible polymer powder an ordinary Portland cement, an alumina rich cement with an alumina content of from 30 wt. % to 85 wt. %, and calcium sulfate. The invention enables a broad range of the claimed acrylic polymers in useful RDPs.

    Abstract translation: 本发明提供了即使再分散性显着地包含具有碱溶性树脂外层的含羧基多级丙烯酸共聚物和一种或多种内层丙烯酸(共)聚合物)的水可再分散性聚合物粉末(RDP)组合物,其表现良好, 玻璃化转变温度(Tg)为-40至50℃,一种或多种沸点为150℃至500℃,水溶性为3.5%以下的成核剂,优选烷基 异丁酸酯和支链烷基异丁酸酯,以及一种或多种胶体稳定剂。 还提供了干混合水泥瓦粘合剂组合物,其包含水可再分散聚合物粉末,普通波特兰水泥,氧化铝富含水泥,氧化铝含量为30重量% %〜85重量% %和硫酸钙。 本发明使得所需要的丙烯酸类聚合物的范围广泛,在有用的RDP中。