Self-Bonding Polypridobismidazole Pulp and a Process for Making Same
    43.
    发明申请
    Self-Bonding Polypridobismidazole Pulp and a Process for Making Same 审中-公开
    自粘多吡啶并吡喃浆及其制备方法

    公开(公告)号:US20090101295A1

    公开(公告)日:2009-04-23

    申请号:US12084024

    申请日:2006-12-19

    CPC classification number: D21H13/20

    Abstract: The invention concerns a fibrous pulp comprising polypyridobisimidazole fiber, the pulp having a Canadian Standard Freeness (CSF) of no more than about 650 ml, a specific surface area of from 0.5 to 50 square meters per gram, a length-weighted average length of from 0.5 to 2.0 mm, and a equilibrium moisture content of greater than 10 percent by weight. Also provided are papers made from such pulp and processes for making the pulp.

    Abstract translation: 本发明涉及包含聚吡啶并二咪唑纤维的纤维纸浆,该纸浆具有不超过约650ml的加拿大标准游离度(CSF),比表面积为0.5至50平方米/克,长度加权平均长度为 0.5〜2.0mm,平衡含水量大于10重量%。 还提供了由这种纸浆制造的纸张和用于制造纸浆的方法。

    Processes for making shaped honeycomb and honeycombs made thereby
    44.
    发明申请
    Processes for making shaped honeycomb and honeycombs made thereby 审中-公开
    由此制成成形蜂窝和蜂窝的方法

    公开(公告)号:US20080145602A1

    公开(公告)日:2008-06-19

    申请号:US11640046

    申请日:2006-12-15

    Abstract: This invention relates to processes for making a honeycomb comprising cells having edges forming a face of the honeycomb, the face defined by a plurality of points and having an area of curvature wherein at least two of the points are located in different tangential planes, comprising the steps of: a) bonding a plurality of sheets along parallel lines of adhesive, the sheets comprising 5 to 50 parts by weight thermoplastic material having a melting point of from 120° C. to 350° C., and 50 to 95 parts by weight high modulus fiber having a modulus of 600 grams per denier (550 grams per dtex) or greater, based on the total amount of thermoplastic material and high modulus fiber in the walls; b) pulling the bonded sheets apart in directions perpendicular to the plane of the sheets to form a honeycomb having cells; c) heating the honeycomb to soften the thermoplastic material; d) bending, molding, or forming the honeycomb in a mold or over a form having an area of curvature; and e) cooling the honeycomb to retain the shape of the area of curvature of the mold or form. Other processes for making a honeycomb include steps for impregnation, b-staging, and/or curing of the honeycomb with resin.This invention also relates to a shaped honeycomb made by this processes wherein less than 25 percent of the honeycomb cells in the area of curvature have a re-entrant angle of greater than 180°.

    Abstract translation: 本发明涉及一种制造蜂窝体的方法,该蜂窝体包括具有形成蜂窝表面的边缘的蜂窝体,所述蜂窝体的表面由多个点限定并且具有曲率区域,其中至少两个点位于不同的切向平面中,包括 步骤:a)沿着平行的粘合剂线粘合多个片材,所述片材包含5至50重量份的熔点为120℃至350℃的热塑性材料和50至95重量份 基于热塑性材料的总量和壁中的高模量纤维,具有600克/旦尼尔(550克/分特)或更高的模量的高模量纤维; b)沿垂直于片材平面的方向拉动粘合片材以形成具有细胞的蜂窝体; c)加热蜂窝以软化热塑性材料; d)在模具中或在具有曲率面积的形式上弯曲,模制或形成蜂窝体; 和e)冷却蜂窝体以保持模具或形式的曲率区域的形状。 制造蜂窝的其它方法包括用树脂浸渍,b阶段化和/或固化蜂窝的步骤。 本发明还涉及通过该方法制造的成形蜂窝体,其中在曲率区域中小于25%的蜂窝电池具有大于180°的重入角度。

    Honeycomb from paper having a high melt point thermoplastic fiber
    45.
    发明申请
    Honeycomb from paper having a high melt point thermoplastic fiber 有权
    具有高熔点热塑性纤维的纸的蜂窝状

    公开(公告)号:US20080145598A1

    公开(公告)日:2008-06-19

    申请号:US11639548

    申请日:2006-12-15

    Abstract: This invention relates to a honeycomb comprising matrix resin and paper, the paper comprising 50 to 80 parts by weight fibrous material having a modulus of 600 grams per denier (550 grams per dtex) or greater, 0 to 50 parts by weight powdered inorganic material, and 20 parts by weight or greater thermoplastic fiber, the improvement comprising the thermoplastic fiber is a binder for the paper and has a melting temperature above the curing temperature of the matrix resin; a glass transition temperature of greater than 100° C., and the weight average molecular weight of the thermoplastic polymer in the thermoplastic fibers changes 20% or less after being maintained for 10 minutes at the melting temperature.One embodiment of this invention includes an article comprising the aforesaid honeycomb, with such articles including a panel or an aerodynamic structure.

    Abstract translation: 本发明涉及一种包含基质树脂和纸的蜂窝体,该纸包含50至80重量份的纤维材料,其模量为600克/旦(550克/分)或更大,0至50重量份粉末状无机材料, 和20重量份以上的热塑性纤维,包括热塑性纤维的改进是用于纸的粘合剂,其熔融温度高于基体树脂的固化温度; 玻璃化转变温度大于100℃,热塑性纤维中的热塑性聚合物的重均分子量在熔融温度下保持10分钟后变化20%以下。 本发明的一个实施例包括一种包含上述蜂窝体的制品,其中包括面板或空气动力学结构的制品。

    Paper comprising PIPD floc and process for making the same
    48.
    发明授权
    Paper comprising PIPD floc and process for making the same 失效
    包含PIPD絮凝剂的纸张及其制造方法

    公开(公告)号:US08444814B2

    公开(公告)日:2013-05-21

    申请号:US12084007

    申请日:2006-12-19

    Inventor: Mikhail R. Levit

    CPC classification number: D21H13/26 D21H15/02 D21H21/18

    Abstract: The invention concerns a paper comprising polypyridobisimidazole floc having a length of from 1.0 to 15 mm, where the apparent density of the paper is from 0.1 to 0.4 g/cm3 and the tensile strength of the paper in N/cm is at least 0.000052X*Y, where X is the volume portion of polypyridobisimidazole in the total solids of the paper in % and Y is basis weight of the paper in g/m2.

    Abstract translation: 本发明涉及包含长度为1.0至15mm的聚吡啶二咪唑絮凝物的纸,其中纸张的表观密度为0.1至0.4g / cm 3,纸张的拉伸强度为N / cm至少为0.000052X * Y,其中X是聚酰胺二咪唑在纸的总固体中的体积百分比,Y是纸的单位面积重量/ g。