摘要:
A high-strength galvanized steel sheet contains C: 0.010% or more and 0.06% or less, Si: more than 0.5% and 1.5% or less, Mn: 1.0% or more and 3.0% or less, P: 0.005% or more and 0.1% or less, S: 0.01% or less, sol.Al: 0.005% or more and 0.5% or less, N: 0.01% or less, Nb: 0.010% or more and 0.090% or less, and Ti: 0.015% or more and 0.15% or less, on a mass percent basis. The Nb and C contents of the steel satisfy the relation of (Nb/93)/(C/12)
摘要翻译:高强度镀锌钢板含有C:0.010%以上且0.06%以下,Si:大于0.5%,1.5%以下,Mn:1.0%以上3.0%以下,P:0.005%以上 和0.1%以下,S:0.01%以下,sol.Al:0.005%以上且0.5%以下,N:0.01%以下,Nb:0.010%以上且0.090%以下,Ti:0.015 %以上且0.15%以下,以质量%计。 钢的Nb和C含量满足(Nb / 93)/(C / 12)<0.20的关系。 C *满足0.005 @ C * @ 0.025。 铁素体构成钢板的70面积比以上。 马氏体构成钢板的3面积比以上。 C * = C-(12/93)Nb-(12/48){Ti-(48/14)N},其中C,Nb,Ti和N表示C,Nb,Ti和N含量 钢。
摘要:
The high strength galvanized steel sheet contains C: more than 0.015% and lower than 0.100%, Si: 0.3% or lower, Mn: lower than 1.90%, P: 0.015% or more and 0.05% or lower, S: 0.03% or lower, sol.Al: 0.01% or more and 0.5% or lower, N: 0.005% or lower, Cr: lower than 0.30%, B: 0.0003% or more and 0.005% or lower, and Ti: lower than 0.014% in terms of mass %, and satisfies 2.2≦[Mneq]≦3.1 and 0.42≦8[% P]+150B*≦0.73. The steel microstructure contains ferrite and a second phase, in which the second phase area ratio is 3 to 15%, the ratio of the area ratio of martensite and retained γ to the second phase area ratio is more than 70%, and 50% or more of the area ratio of the second phase exists in the grain boundary triple point.
摘要:
A high-strength hot-rolled steel sheet has a tensile strength (TS) of 540 to 780 MPa, only small variations in strength, and excellent uniformity in strength using a general-purpose Ti-containing steel sheet, which is inexpensive. The high-strength hot-rolled steel sheet includes, on a mass percent basis, 0.05%-0.12% C, 0.5% or less Si, 0.8%-1.8% Mn, 0.030% or less P, 0.01% or less S, 0.005%-0.1% Al, 0.01% or less N, 0.030%-0.080% Ti, and the balance being Fe and incidental impurities. The microstructure have a volume fraction of polygonal ferrite of 70% or more, and the amount of Ti present in a precipitate having a size of less than 20 nm is 50% or more of the value of Ti* calculated using formula (1): Ti*=[Ti]−48/14×[N] (1) where [Ti] and [N] represent a Ti content (percent by mass) and a N content (percent by mass), respectively, of the steel sheet.
摘要:
A steel slab is rough-rolled into a sheet bar and butt-joined onto a preceding sheet bar and a widthwise end portion of the sheet bar is heated by means of an edge heater and then subjected to a continuous finish rolling through pair-cross rolls rolling on at least 3 stands to provide a hot rolled steel strip having a width of not less than 950 mm, a thickness of 0.5-2 mm and a crown within .+-.40 .mu.m, and the hot rolled steel strip is subjected to cold rolling, continuous annealing, temper rolling and, if necessary, plating treatment on the surface of the cold rolled steel strip, whereby there is obtained a steel sheet having an average thickness of not more than 0.20 mm and a width of not less than 950 mm, a thickness variation quantity in a widthwise direction is within .+-.4% of the average thickness in a region corresponding to not less than 95% of the width of the steel sheet as cold rolled and a hardness (HR30T) variation in the widthwise direction is within .+-.3 of an average hardness.
摘要:
A high-strength galvanized steel sheet contains C: 0.010% or more and 0.06% or less, Si: more than 0.5% and 1.5% or less, Mn: 1.0% or more and 3.0% or less, P: 0.005% or more and 0.1% or less, S: 0.01% or less, sol.Al: 0.005% or more and 0.5% or less, N: 0.01% or less, Nb: 0.010% or more and 0.090% or less, and Ti: 0.015% or more and 0.15% or less, on a mass percent basis. The Nb and C contents of the steel satisfy the relation of (Nb/93)/(C/12)
摘要:
A vehicle collision energy absorbing member is excellent in collision energy absorbing performance in the axial direction upon collision. The vehicle collision energy absorbing member is formed of a high strength thin steel sheet having TS of at least 980 MPa and having an n-value and a limit bending radius Rc satisfying the following Formula: Rc/t≦1.31×ln(n)+5.21.
摘要:
A high strength hot-dip galvanized steel sheet has TS of 440 MPa or more and an average r value of 1.30 or more, where the absolute value of the planar anisotropy of the r value (Δr) is 0.20 or less. A chemical composition contains C: 0.010% or more and 0.04% or less, Si: more than 1.0% and 1.5% or less, Mn: 1.0% or more and 3.0% or less, P: 0.005% or more and 0.1% or less, S: 0.01% or less, sol. Al: 0.005% or more and 0.5% or less, N: 0.01% or less, Nb: 0.010% or more and less than 0.05%, Ti: 0.015% or more and 0.120% or less, and the remainder composed of Fe and incidental impurities, wherein (Nb/93)/(C/12) 0.20 and 0.005
摘要:
A high-strength hot-rolled steel sheet has a tensile strength (TS) of 540 to 780 MPa, only small variations in strength, and excellent uniformity in strength using a general-purpose Ti-containing steel sheet, which is inexpensive. The high-strength hot-rolled steel sheet includes, on a mass percent basis, 0.05%-0.12% C, 0.5% or less Si, 0.8%-1.8% Mn, 0.030% or less P, 0.01% or less S, 0.005%-0.1% Al, 0.01% or less N, 0.030%-0.080% Ti, and the balance being Fe and incidental impurities. The microstructure have a bainitic ferrite fraction of 70% or more, and the amount of Ti present in a precipitate having a size of less than 20 nm is 50% or more of the value of Ti* calculated using formula (1): Ti*=[Ti]−48/14×[N] (1) where [Ti] and [N] represent a Ti content (percent by mass) and a N content (percent by mass), respectively, of the steel sheet.
摘要:
A high-strength galvanized steel sheet has a low YP, good stretch flangeability, and excellent corrosion resistance and contains, on a percent by mass basis, more than 0.015% to less than 0.10% of C, 0.5% or less of Si, 1.0% to 1.9% of Mn, 0.015% to 0.050% of P, 0.03% or less of S, 0.01% to 0.5% of sol. Al, 0.005% or less of N, less than 0.40% of Cr, 0.005% or less of B, less than 0.15% of Mo, 0.4% or less of V, and less than 0.020% of Ti, in which 2.2≦[Mneq]≦3.1 and [% Mn]+3.3[% Mo]≦1.9, and [% Mn]+3.3 [% Mo])/(1.3[% Cr]+8[% P]+150B*)
摘要:
A high-strength hot-dip galvanized steel sheet that even on the premise of ordinary CGL heat cycle, has a low yield stress and excels in resistance to natural aging and baking hardenability without reliance on the use of expensive Mo; and a process for producing the same. The constituent composition thereof comprises 0.01 to less than 0.08% C, 0.2% or less Si, more than 1.0 to 1.8% Mn, 0.10% or less P, 0.03% or less S, 0.1% or less Al, 0.008% or less N and more than 0.5% Cr so that the relationship 1.95≦Mn(mass %)+1.3Cr(mass %)≦2.8 is satisfied and comprising the balance iron and unavoidable impurities. The structure thereof has a ferrite phase and a martensite phase of 2 to 15% area ratio, and the cumulative area ratio of pearlite phase and/or bainite phase is 1.0% or less. In the production of this hot-dip galvanized steel sheet, the temperature and cooling rate are controlled during the annealing/plating operation subsequent to cold rolling.