摘要:
A high strength cold rolled steel sheet includes a chemical composition containing, by mass %, C: 0.010% or more and 0.060% or less, Si: more than 0.5% and 1.5% or less, Mn: 1.0% or more and 3.0% or less, P: 0.005% or more and 0.100% or less, S: 0.010% or less, sol.Al: 0.005% or more and 0.500% or less, N: 0.0100% or less, Nb: 0.010% or more and 0.100% or less, Ti: 0.015% or more and 0.150% or less and the balance comprising Fe and inevitable impurities. The microstructure includes, in area fraction, 70% or more of a ferrite phase and 3% or more of a martensite phase. The tensile strength is 440 MPa or more and an average r value is 1.20 or more.
摘要:
A steel sheet has the chemical composition containing, by mass %, C: 0.04 to 0.13%, Si: 0.9 to 2.3%, Mn: 0.8 to 1.8%, P: 0.1% or less, S: 0.01% or less, Al: 0.1% or less, N: 0.008% or less, the remainder being Fe and the inevitable impurities and a microstructure including, in terms of area ratio, a ferrite phase of 80% or more, a bainitic ferrite phase of 1.0% or more, a pearlite phase of 1.0 to 10.0%, and a martensite phase of 1.0% or more and less than 5.0%, wherein the mean grain size of ferrite is 14 μm or less, the mean grain size of martensite is 4 μm or less, the mean free path of martensite is 3 μm or more, the Vickers hardness of ferrite is 140 or more, and the relationship area ratio of martensite/(area ratio of bainitic ferrite+area ratio of pearlite) 0.6 is satisfied.
摘要:
The invention provides a high strength cold rolled steel sheet comprising ferrite phases and second phases, in which the mean grain size of the ferrite phases is 20 μm or less, the volume fraction of the second phase is 0.1% or more to less than 10%, the absolute value |Δr| of in-plane anisotropy of r value is less than 0.15, and the thickness is 0.4 mm or more. The high strength cold rolled steel sheet of the present invention has a tensile strength of 370 to 590 MPa, and has excellent stretchability, dent resistance, surface precision, secondary working embrittlement, anti-aging, and surface appearance, therefore it is suitable for outer panels of automobile.
摘要:
The present invention relates to a high strength steel sheet consisting essentially of 0.04 to 0.1% C, 0.5% or less Si, 0.5 to 2% Mn, 0.05% or less P, 0.005% or less O, 0.005% or less S, by weight, having 10 μm or less of average ferritic grain size, and 20 mm/mm2 or less of generation frequency A, which generation frequency A is defined as the total length of a banded secondary phase structure observed per 1 mm2 of steel sheet cross section along the rolling direction thereof. The steel sheet is manufactured by, for example, a method comprising the steps of: hot-rolling a continuously cast slab having the composition described above at temperatures of Ar3 transformation point or above directly or after reheating thereof; and cooling the hot-rolled steel sheet within 2 seconds down to the temperatures of from 600 to 750° C. at cooling speeds of from 100 to 2,000° C./sec, followed by coiling the cooled steel sheet at temperatures of from 450 to 650° C. The present invention provides a high strength steel sheet having strengths of 340 MPa or more and having excellent stretch flanging performance, ductility, and shock resistance, providing a sufficient coil shape with good surface properties, even when hot dip zinc-coating is applied.
摘要:
The present invention relates to a high strength cold rolled steel sheet consisting of 0.015% or less of C, 1.5% or less of Si, 0.4 to 3% of Mn, 0.15% or less of P, 0.02% or less of S, 0.1 to 1% of sol.Al, 0.01% or less of N, 0.2% or less of Ti, by mass %, and the balance of Fe and inevitable impurities. In this steel sheet, 1≦([Ti]/48)/([C]/12+[N]/14) is satisfied, in which [M] represents the content of the element M. Since having the superior deep drawability and the TS of 340 to 590 MPa, the high strength cold rolled steel sheet of the present invention is preferably used for automobiles parts difficult to be press formed, such as a side outer panel and a door inner panel.
摘要:
Provided are a high-strength hot-dip galvanized steel sheet having excellent formability and a tensile strength of 440 MPa or more and a method for manufacturing the same. A steel sheet has a microstructure containing a ferrite phase having an area fraction of 60% or more, a pearlite phase having an area fraction of 20% to 30%, and a bainite phase having an area fraction of 1% to 5%, the area fraction of a cementite phase present in a grain of the ferrite phase being 5% or less. Upon manufacture, a hot-rolled sheet or a cold-rolled sheet is heated to a temperature of 650° C. or higher at an average heating rate of 10° C./s or more, is held at a temperature of 700° C. to (Ac3-5)° C. for ten seconds or more, is cooled to a temperature of 300° C. to 500° C. at an average cooling rate of 10° C./s to 200° C./s, is held at a temperature of 300° C. to 500° C. for 30 seconds to 300 seconds, and is then hot-dip galvanized.
摘要:
A method of manufacturing a high strength galvanized steel sheet has a first heating step including heating to 400° C. to 750° C. in an atmosphere containing O2: 0.1 to 20 percent and H2O: 1 to 50 percent and heating to 600° C. to 850° C. in an atmosphere containing O2: 0.01 to less than 0.1 percent and H2O: 1 to 20 percent is applied to a steel sheet, a second heating step includes holding the steel sheet in an atmosphere containing H2: 1 to 50 percent and having a dew point of 0° C. or lower at 750° C. to 900° C. for 15 to 600 s, cooling to a temperature of 450° C. to 550° C., and holding is performed at that temperature for 10 to 200 s, and a galvanization treatment is applied.
摘要:
A galvanized steel sheet has a composition containing, by mass %, C: 0.05% or more and 0.5% or less, Si: 0.01% or more and 2.5% or less, Mn: 0.5% or more and 3.5% or less, P: 0.003% or more and 0.100% or less, S: 0.02% or less, Al: 0.010% or more and 0.5% or less, B: 0.0002% or more and 0.005% or less, Ti: 0.05% or less, a relationship of Ti>4N being satisfied, and the balance comprising Fe and inevitable impurities, and a microstructure containing 60% or more and 95% or less of tempered martensite in terms of area ratio and 5% or more and 20% or less of retained austenite in terms of area ratio.
摘要:
A high-strength galvanized steel sheet with excellent formability and shape fixability and a method for manufacturing the high-strength galvanized steel sheet.
摘要:
A galvannealed steel sheet includes a zinc coating layer containing 7 to 15% Fe on the surface of steel sheet including, C: 0.02% to 0.30%, Si: 0.01% to 2.5%, Mn: 0.1% to 3.0%, P: 0.003% to 0.08%, S: not more than 0.01%, Al: 0.001% to 0.20%, one or more selected from Ti: 0.03% to 0.40%, Nb: 0.001% to 0.2%, V: 0.001% to 0.2%, Mo: 0.01% to 0.5% and W: 0.001% to 0.2%. In the zinc coating layer, carbides with average particle size of 1 nm to 20 nm including one or more selected from titanium, niobium, vanadium, molybdenum and tungsten are present with a density of five or more particles per segment that is defined by the thickness of the coating layer and also by dividing a cross section of the coating layer at intervals of 1 μm in a direction perpendicular to the thickness of the coating layer.