摘要:
A process for producing a bumper of synthetic resin for use in an automobile, the bumper including a core and an outer layer covering the core. The process includes the steps of preparing a core forming material that includes a main component and a polyethylene added to the main component, the main component being produced by pulverizing a recovered bumper which has been formed using a polyolefin-based resin composition modified by an olefinic elastomer and which has a thermosetting synthetic resin coating film on its surface, and an outer layer forming material that includes the polyolefin-based resin composition modified by the olefinic elastomer and the polyethylene in a content A.sub.2 which is smaller than a content A.sub.1 of the polyethylene included in the core forming material (A.sub.2
摘要:
A bumper of synthetic resin for use in an automobile includes a core, and an outer layer covering the core. The material for forming the core includes a main component produced by pulverizing a recovered bumper which has been formed using a polyolefin-based resin composition modified by an olefinic elastomer and which has a thermosetting synthetic resin coating film on its surface, and a polyethylene added to the main component. The material for forming the outer layer includes the polyolefin-based resin composition modified by the olefinic elastomer and the polyethylene in a content A.sub.2 which is smaller than a content A.sub.1 of the polyethylene in the core forming material (A.sub.2
摘要:
A resin composition utilizing coated resin moldings, the resin composition comprising 100 parts by weight of a crushed material of coated polyolefin resin moldings compounded with from 3 to 15 parts by weight of an ethylene polymer having a weight average molecular weight of from 50,000 to 180,000.
摘要:
A multilayer resin molding, utilizing coated resin moldings, composed of a core material and a surface layer covering the core material, the core material being composed of a resin composition which comprises 100 parts by weight of a crushed material of coated polyolefin resin moldings compounded with from 3 to 15 parts by weight of an ethylene polymer having a weight average molecular weight of from 50,000 to 180,000 and the surface layer comprising a polypropylene resin composition comprising from 30 to 80% by weight of a propylene polymer, from 3 to 20% by weight of a propylene polymer modified with an unsaturated hydroxy compound, from 15 to 40% by weight of a thermoplastic elastomer, and from 0.1 to 10% by weight of an oligomer having a functional group at the terminal thereof.
摘要:
A polypropylene resin composition comprising: (a) 50 to 90% by weight of polypropylene, (b) 50 to 10% by weight of an ethylene-.alpha.-olefin copolymer elastomer having a Mooney viscosity (ML 1+4 (100.degree. C.)) of 10 to 100, (c) 0.5 to 10 parts by weight per 100 parts by weight of the total of the amounts of the components (a) and (b) of a linear olefinic polymer containing hydroxyl group which is liquid at room temperature, and (d) 0.5 to 15 parts by weight per 100 parts by weight of the total of the amounts of the components (a) and (b) of a linear olefinic polymer having a melting point of about 70.degree. to about 90.degree. C. and a number-average molecular weight of 1500 to 6000 and containing hydroxyl group or carbonyl group; and a protective strip for automobiles using the polypropylene resin composition are disclosed. Coating immediately after degreasing is made possible and excellent property for coating can be provided by using the polypropylene resin composition.
摘要:
A polypropylene resin composition which comprises (A) 100 parts by weight of polypropylene, (B) 20-50 parts by weight of at least one elastomer selected from an ethylenic elastomer, an hydrogenated styrene-butadiene copolymer and a hydrogenated styrene-isoprene block copolymer, (C) 0.3.about.20 parts by weight of polycarbonatediol having a skeleton of aliphatic carbonate with both terminals being a hydroxyl group and (D) 0.about.50 parts by weight of an inorganic filler. The resin composition can provide a molded article having a good adhesive property to a film applied thereon without pretreatment by a halogen-containing solvent.
摘要:
A coated molded article having good adhesion to a coating film and resistance to gasohol as well as excellent appearance can be obtained by applying a primer coating to the surface of a molded article or irradiating the surface with plasma without applying any washing-treatment with a halogen atom-containing organic solvent and then applying a top coat onto the article, if the molded article is formed from a resin composition comprising (A)a polypropylene; (B)a specific ethylene-propylene-diene terpolymer rubber; (C) a specific ethylene-propylene copolymer rubber; and (D) a specific polyhydroxypolyolefin, the amounts of these components (A) to (D) satisfying the following relations:10.ltoreq.[(B)+(C)]/[(A)+(B)+(C)].ltoreq.60 (% by weight)1.ltoreq.(C)/[(B)+(C)].ltoreq.50 (% by weight)0.5.ltoreq.(D)/[(A)+(B)+(C)+(D)].ltoreq.10 (% by weight)
摘要:
Disclosed is a side protective moulding having a decorative section and a rib section. The decorative section has a protruding section protruding most with respect to a door, and a curved section extending aslant from the protruding section toward the door. The rib section has a hollow section formed on the back side of the protruding section and a reinforcing leg section extending from the hollow section toward the door. The side moulding is moulded by a hollow injection moulding process. Adopting this moulding process can improve the outside appearance of the side moulding by eliminating sink marks and wrinkles from the surface of the decorative section if a thick wall section for increasing side moulding rigidity and impact strength is formed on the back side of the decorative section.
摘要:
A molded protective strip for automobiles is prepared by the gas injection molding of a resin composition which comprises (A) 55 to 75% by weight of polypropylene, (B) 18 to 30% by weight of ethylene-propylene copolymer rubber, and (C) 10 to 20% by weight of talc, has a ratio (MI).sub.PP /(MI).sub.EPR of 10 or less, and a polydispersity index of 20 to 100. (MI).sub.PP and (MI).sub.EPR represents melt indices of the polypropylene of component (A) and the ethylene-propylene copolymer rubber of component (B), respectively. The polydispersity index is calculated from a frequency-storage modulus curve obtained with a composition consisting of components (A), (B), and (C) alone at the temperature of 230.degree. C. The molded protective strip can be prepared without using a vinyl chloride resin, shows almost no heat shrinkage, has a small coefficient of linear expansion, is excellent in dimensional stability, and exhibits excellent appearance.
摘要:
A gas diffusion layer (6) is sandwiched between catalyst electrode layers (5) and separators (1, 2), and side faces (6A, 6B) of the gas diffusion layer (6) are arranged so as to face a gas inlet manifold (7) and outlet manifold (8), and partition the inlet manifold (7) and outlet manifold (8). In the gas diffusion layer (6), gas flows from the side face (6A) facing the inlet manifold (7), flows through the interior, and flows out from the side face (6B) facing the outlet manifold (8).