Comminution process
    1.
    发明授权
    Comminution process 失效
    服务流程

    公开(公告)号:US4265406A

    公开(公告)日:1981-05-05

    申请号:US44161

    申请日:1979-05-31

    IPC分类号: B02C23/06 C05C1/02 B02C19/00

    摘要: A process is described for the comminution of a solid material in the presence of a saturated solution of the solid in a liquid in which the solid has a solubility greater than 1%, and also in the presence of an additive dissolved in the saturated solution which can at least partially inhibit regrowth at crystal surfaces of the solid material. The process is of particular interest for the comminution of water-soluble salts in the presence of their saturated aqueous solutions and may be employed to make, inter alia, improved slurry explosives and fluid fertilizer compositions.

    摘要翻译: 描述了一种在固体在固体溶解度大于1%的液体中的固体的饱和溶液存在下粉碎固体材料的方法,以及溶解在饱和溶液中的添加剂的存在下, 可以至少部分地抑制固体材料的晶体表面的再生长。 该方法在其饱和水溶液存在下粉碎水溶性盐是特别有意义的,并且可用于特别改进的浆料炸药和流体肥料组合物。

    Ammonium nitrate slurry compositions
    2.
    发明授权
    Ammonium nitrate slurry compositions 失效
    硝酸铵浆料组合物

    公开(公告)号:US4331490A

    公开(公告)日:1982-05-25

    申请号:US227413

    申请日:1981-01-22

    IPC分类号: B02C23/06 C05C1/02 C06B31/28

    摘要: A slurry composition based essentially on ammonium nitrate, prepared by a process which comprises comminuting solid substance containing ammonium nitrate by grinding in the presence of a saturated solution of solid in a liquid in which the solid has a solubility greater than 1% by weight, the mixture of the solution and the solid being in fluid condition with the solid being a separate phase during grinding and the solution having dissolved therein an additive which is a crystal growth inhibitor for the solid whereby crystal growth is inhibited at both existing crystal surfaces and new crystal surfaces created by the breaking down of relatively coarse particles.

    摘要翻译: 基于硝酸铵的浆料组合物,其通过以下方法制备,该方法包括在固体溶解度大于1重量%的液体中的固体饱和溶液存在下研磨,粉碎含有硝酸铵的固体物质, 溶液和固体的混合物处于流体状态,固体在研磨过程中是分离相,溶液中溶解有作为固体的晶体生长抑制剂的添加剂,从而在现有晶体表面和新晶体上晶体生长被抑制 通过破碎比较粗糙的颗粒产生的表面。

    Fluid fertilizer composition
    3.
    发明授权
    Fluid fertilizer composition 失效
    流体肥料组成

    公开(公告)号:US4482372A

    公开(公告)日:1984-11-13

    申请号:US452497

    申请日:1982-12-23

    IPC分类号: B02C23/06 C05C1/02 C05B7/00

    摘要: A fluid fertilizer composition based essentially on potassium chloride and an ammonium phosphate prepared by a process which comprises comminuting a solid substance containing potassium chloride and ammonium phosphate by grinding in the presence of a saturated solution of solid in a liquid in which the solid has a solubility greater than 1% by weight, the mixture of the solution and the solid being in fluid condition with the solid being a separate phase during grinding and the solution having dissolved therein an additive which is a crystal growth inhibitor for the solid whereby crystal growth is inhibited at both existing crystal surfaces and new crystal surfaces created by the breaking down of relatively coarse particles.

    摘要翻译: 一种基本上基于氯化钾和一种磷酸铵的流体肥料组合物,其通过以下方法制备,所述方法包括在固体在其中具有溶解度的液体中的固体的饱和溶液存在下,研磨含有氯化钾和磷酸铵的固体物质 大于1重量%,溶液和固体的混合物处于流体状态,固体在研磨期间是分离相,并且溶液中溶解有作为固体的晶体生长抑制剂的添加剂,从而晶体生长被抑制 在现有的晶体表面和通过相对粗糙的颗粒的分解产生的新的晶体表面。

    Production of ceramic materials
    6.
    发明授权
    Production of ceramic materials 失效
    生产陶瓷材料

    公开(公告)号:US4861735A

    公开(公告)日:1989-08-29

    申请号:US112890

    申请日:1987-10-27

    CPC分类号: C08G79/00 C01B33/06 C01B35/04

    摘要: A process for the production of a refractory boride or silicide which comprises producing an oxygen-containing polymeric product by reacting a compound of the metallic or non-metallic element having two or more groups reactive with hydroxyl groups and a compound of boron or silicon having two or more groups reactive with hydroxyl groups with an organic compound having two or more hydroxyl groups and heating the polymeric product in an inert atmosphere to pyrolyse the polymeric product and produce a refractory boride or silicide of the metallic or non-metallic element.

    摘要翻译: 一种用于生产耐火硼化物或硅化物的方法,其包括通过使具有两个或多个与羟基反应的基团的金属或非金属元素的化合物和具有两个或两个以上的羟基的硼或硅化合物反应制备含氧聚合物 或更多个与具有两个或更多个羟基的有机化合物与羟基反应的基团,并在惰性气氛中加热聚合产物以热解聚合产物并产生金属或非金属元素的耐火硼化物或硅化物。

    Hydraulic cement composition
    7.
    发明授权
    Hydraulic cement composition 失效
    水泥水泥组成

    公开(公告)号:US4353747A

    公开(公告)日:1982-10-12

    申请号:US160370

    申请日:1980-06-17

    IPC分类号: C04B7/02 C04B7/52 C04B28/02

    CPC分类号: C04B7/527 C04B28/02

    摘要: A hydraulic cement composition comprising a mixture of at least one particulate hydraulic cement and water in which the weight average mean particle size of the particles of the cement is less than 20 microns and in which the proportion of water is not greater than 30% by weight of the hydraulic cement in the composition, the cement being preferably substantially free of particles having a size above 20 microns and the proportion of water being preferably not greater than 20% by weight.

    摘要翻译: 一种水硬性水泥组合物,其包含至少一种水泥水泥和水的混合物,其中所述水泥颗粒的重均粒度平均粒径小于20微米,并且其中水的比例不大于30重量% 组合物中的水硬性水泥的水泥优选基本上不含大于20微米的颗粒,水的比例优选不大于20重量%。

    Cement composition and product
    10.
    发明授权
    Cement composition and product 失效
    水泥组成和产品

    公开(公告)号:US4410366A

    公开(公告)日:1983-10-18

    申请号:US330585

    申请日:1981-12-14

    摘要: A cementitious composition comprising hydraulic cement, not more than 25% of water by weight of the composition, and water soluble or dispersible (co)polymer in a proportion of 1 to 15% by weight of the hydraulic cement in the composition, the cement and (co)polymer being selected such that a test composition comprising 100 parts by weight of cement, 5 parts by weight of (co)polymer, and 16 parts by weight of water when extruded in a capillary rheometer undergoes an increase of at least 25% in shear stress when a ten-fold increase in the shear rate of the test composition from the capillary of the rheometer is effected. Also a cementitious product produced by setting of the composition. The (co)polymer is preferably a partially hydrolyzed poly (vinyl acetate). The cementitious product may have a flexural strength in excess of 100 MPa.

    摘要翻译: 一种胶结组合物,其包含水硬性水泥,不超过组合物重量的25%的水,以及组合物中水硬性水泥的1至15重量%的水溶性或可分散(共)聚合物,水泥和 (共)聚合物,使得当在毛细管流变仪中挤出时,包含100重量份水泥,5重量份(共)聚合物和16重量份水的测试组合物经历增加至少25重量% 当来自流变仪的毛细管的试验组合物的剪切速率增加十倍时,在剪切应力下。 也是通过设定组合物生产的水泥制品。 (共)聚合物优选为部分水解的聚(乙酸乙烯酯)。 胶结产物的弯曲强度可以超过100MPa。