Electron-conductive high polymer and electroconductive material having
the same
    2.
    发明授权
    Electron-conductive high polymer and electroconductive material having the same 失效
    具有导电性高聚合物和电子导电材料

    公开(公告)号:US5115057A

    公开(公告)日:1992-05-19

    申请号:US548648

    申请日:1990-07-05

    IPC分类号: C08F246/00 H01B1/12 H01M4/60

    摘要: Disclosed is an electron-conductive high polymer, which has at least (1) an ethylenic repeating unit having an electron-conductive site comprising at least one of aniline compounds and heterocyclic compounds as the repeating unit in the side chain and (2) an ethylenic repeating unit having an anionic group in the side chain and/or an ethylenic repeating unit having a repeating unit of an oxyalkylene group in the side chain. As having excellent electroconductivity, mechanical strength and shapability, the high polymer is laminated with a solid polyelectrolyte or with a separator to prepare an electroconductive material usable as a battery material.

    Screw for in-line screw type thermosetting resin injection molding
machine
    4.
    发明授权
    Screw for in-line screw type thermosetting resin injection molding machine 失效
    螺旋式螺旋式热固性树脂注塑机

    公开(公告)号:US5957576A

    公开(公告)日:1999-09-28

    申请号:US673206

    申请日:1996-06-27

    申请人: Eiji Funatsu

    发明人: Eiji Funatsu

    IPC分类号: B29C45/60 B29B7/14

    CPC分类号: B29C45/60

    摘要: A screw for an in-line screw type thermosetting resin injection molding machine comprises a resin kneading portion in a front end portion of a full-flighted screw. In the resin kneading portion, a groove having a crest portion and a trough portion formed spirally in a circumferential direction, and a step portion. A difference between a radial dimension of the step portion and an outermost radial dimension of the crest portion is 10% to 60% of a difference between the outermost radial dimension of the crest portion and an innermost radial dimension of the trough portion. The axial length of the resin kneading portion is 0.5 to 2 times as long as the outer diameter of the full-flighted screw, or 0.5 to 2 times as long as the pitch of the full-flighted screw.

    摘要翻译: 用于直列螺杆型热固性树脂注射成型机的螺杆包括在全螺纹螺钉的前端部分中的树脂捏合部分。 在树脂捏合部分中,具有沿圆周方向螺旋形成的波峰部分和谷部分的槽和台阶部分。 台阶部分的径向尺寸与波峰部分的最外径向尺寸之间的差别在波峰部分的最外侧径向尺寸与凹槽部分的最内侧径向尺寸之差为10%至60%。 树脂捏合部的轴向长度为全螺纹螺杆的外径的0.5〜2倍,即全螺纹螺杆的间距的0.5〜2倍。

    Process for injection molding of phenolic resin molding material
    5.
    发明授权
    Process for injection molding of phenolic resin molding material 失效
    酚醛树脂成型材料注塑成型工艺

    公开(公告)号:US5679305A

    公开(公告)日:1997-10-21

    申请号:US508993

    申请日:1995-07-28

    IPC分类号: B29C45/00 B29C45/60

    CPC分类号: B29C45/0001

    摘要: The present invention provides a process for injection molding a phenolic resin molding material which includes injection molding a phenolic resin molding material having a melt viscosity of 10.sup.4 Pa.cndot.s or lower, preferably 10.sup.3 Pa.cndot.s or lower at 100.degree. C. by an injection molding machine having a screw of 1.5 or higher in compression ratio and/or provided with a back-flow stopping ring at the tip portion of the screw. According to the present invention, it is possible to carry out injection molding of phenolic resin molding materials with injection molding machines generally used for molding of thermoplastic resins by employing phenolic resin molding materials which are low in viscosity in molten state. Furthermore, the injection molding can be carried out under relatively low pressure and thus, occurrence of flash can be inhibited.

    摘要翻译: 本发明提供了一种酚醛树脂成型材料的注射成型方法,该方法包括通过注射在100℃注射成型熔体粘度为104Pa·s或更低,优选为103Pa.s或更低的酚醛树脂成型材料 成型机具有1.5或更高的压缩比的螺杆和/或在螺杆的尖端部分设置有回流止动环。 根据本发明,通过使用在熔融状态下粘度低的酚醛树脂成型材料,可以通过使用通常用于模塑热塑性树脂的注射成型机来进行酚醛树脂成型材料的注射成型。 此外,注射成型可以在相对低的压力下进行,因此可以抑制闪光的发生。

    Catalyst for hydrotreating coal liquefaction and circulation solvent
    7.
    发明授权
    Catalyst for hydrotreating coal liquefaction and circulation solvent 失效
    用于加氢处理煤液化和循环溶剂的催化剂

    公开(公告)号:US4950633A

    公开(公告)日:1990-08-21

    申请号:US422428

    申请日:1989-10-17

    摘要: Disclosed is a catalyst for hydrotreating a coal liquefaction and circulation solvent, in which .gamma.-alumina carrier carries at least one metal of Group VI of the Periodic Table in an amount of from 15 to 15% by weight as the oxide thereof and at least one metal of Group VIII of the same Table in an amount of from 3 to 10% by weight as the oxide thereof and the pore distribution as measured by mercury pressure porosimetry satisfies the conditions that the pores having a diameter of from 40 to 600 .ANG. have a mean diameter of from 9 to 150 .ANG. and the capacty of the pores having a diameter falling within the range of the mean diametr plus/minus 10 .ANG. is 65% or more of the capacity of the pores having a diameter of from 40 to 600 .ANG.. The catalyst is highly active for both hydrogenation and denitrogenation of coal-liquefying solvents.

    摘要翻译: 公开了用于加氢处理煤液化和循环溶剂的催化剂,其中γ-氧化铝载体携带至少一种元素周期表第VI族金属,其量为其15至15重量%的氧化物和至少一种 相同表的VIII族金属的氧化物的量为3〜10重量%,通过汞压孔率法测定的孔分布满足直径40〜600的孔具有 平均直径为9至150安培角,直径在平均直径加/减10安培范围内的孔的角度为直径为40至600埃的孔的容量的65%或更多 。 该催化剂对于煤液化溶剂的氢化和脱氮均具有高度的活性。

    Nonaqueous secondary battery
    8.
    发明授权
    Nonaqueous secondary battery 失效
    非水二次电池

    公开(公告)号:US5478673A

    公开(公告)日:1995-12-26

    申请号:US110951

    申请日:1993-08-24

    申请人: Eiji Funatsu

    发明人: Eiji Funatsu

    IPC分类号: H01M4/48 H01M10/40

    CPC分类号: H01M10/0566 H01M4/485

    摘要: A nonaqueous secondary battery comprises an anode active material, a cathode active material and an electrolytic solution. The anode active material comprises a transition metal oxide, and the electrolytic solution is prepared by dissolving a fluorine-containing lithium salt in a mixed solvent comprising ethylene carbonate and at least one selected from the group consisting of chain carbonic acid esters, cyclic carbonic acid esters, cyclic esters, chain ethers and cyclic ethers.

    摘要翻译: 非水二次电池包括负极活性物质,正极活性物质和电解液。 所述负极活性物质包含过渡金属氧化物,所述电解液是通过将含氟锂盐溶解在含有碳酸亚乙酯和选自链碳酸酯,环状碳酸酯中的至少一种的混合溶剂中来制备的 ,环酯,链醚和环醚。

    Protein-starch binary molding composition and shaped articles obtained
therefor
    9.
    发明授权
    Protein-starch binary molding composition and shaped articles obtained therefor 失效
    蛋白质 - 淀粉二元成型组合物和获得的成型制品

    公开(公告)号:US4076846A

    公开(公告)日:1978-02-28

    申请号:US631405

    申请日:1975-11-12

    摘要: An edible, water-soluble, thermoplastic molding composition comprising a starch material, a neutral inorganic alkali salt of protein material, water, an edible plasticizer, an edible lubricant, and other additives. This composition shows excellent moldability and processability when subjected to various constomery dry processes for molding and processing customary plastics, such as compression molding, transfer molding, extrusion molding, blow molding, inflation molding, injection molding, vacuum forming, pressure forming, heat sealing, etc. Transparent or translucent shaped articles obtained from the above composition have unique properties such as gas impermeability, solubility in water, edibility, biodegradability, etc., and may be utilized with favorable results in various fields such as food industry, feedstuff industry, agriculture, fisheries, etc. The shaped articles, if necessary, can be allowed to have any balance between its water resistance and its water-solubility by ultraviolet irradiation or by the incorporation of a protein-coagulating agent.

    摘要翻译: 一种可食用的水溶性热塑性模塑组合物,其包含淀粉材料,蛋白质材料的中性无机碱金属盐,水,可食用增塑剂,可食用润滑剂和其它添加剂。 当进行各种常规的塑料成型加工,例如压缩成型,传递成型,挤出成形,吹塑成型,吹塑成型,注射成型,真空成形,加压成型,热封等常规塑料的干法时,该组合物显示优异的成型性和加工性, 由上述组合物得到的透明或半透明成型制品具有独特的性能,例如气体不渗透性,在水中的溶解性,可溶性,生物降解性等,并且可以在食品工业,饲料工业,农业等各个领域得到有利的结果 ,渔业等。如果需要,成形制品可以通过紫外线照射或通过掺入蛋白质凝结剂在其耐水性和其水溶性之间具有任何平衡。