公开(公告)号:US10062851B2
公开(公告)日:2018-08-28
申请号:US15375187
申请日:2016-12-12
Applicant: FUJIFILM CORPORATION
Inventor: Toshihiro Kariya , Kensuke Masui , Takafumi Nakayama , Shuji Kanayama , Hiroyuki Takahashi
CPC classification number: H01L51/0071 , C09D11/037 , C09D11/322 , C09D11/52 , H01L51/0004 , H01L51/0005 , H01L51/004 , H01L51/0043 , H01L51/0068 , H01L51/0074 , H01L51/0094 , H01L51/0533 , H01L51/0545 , H01L51/0558
Abstract: An object of the present invention is to provide a composition for forming an organic semiconductor film that makes it possible to obtain an organic semiconductor film having excellent mobility and heat stability, an organic semiconductor element including an organic semiconductor film having excellent mobility and heat stability, and a method for manufacturing the organic semiconductor element.The composition for forming an organic semiconductor film of the present invention contains an organic semiconductor having a condensed polycyclic aromatic group and a polymer, in which the number of rings in the condensed polycyclic aromatic group is equal to or greater than 4, at least two rings in the condensed polycyclic aromatic group contain at least one atom selected from the group consisting of a sulfur atom, a nitrogen atom, a selenium atom, and an oxygen atom, the condensed polycyclic aromatic group contains, as a partial structure, at least any one structure selected from the group consisting of a benzene ring, a naphthalene ring, and a phenanthrene ring, and the polymer has a glass transition temperature of equal to or higher than −100° C. and equal to or less than −30° C. and an elastic recovery of equal to or less than 30%.
-
公开(公告)号:US10053587B2
公开(公告)日:2018-08-21
申请号:US14807654
申请日:2015-07-23
Applicant: FUJIFILM CORPORATION
Inventor: Misato Sasada , Yuuichi Hayata , Yushi Hongo , Toshihiro Kariya
IPC: H01B1/22 , C09D5/24 , C09D5/00 , C09D139/06 , C09D171/02 , C09D201/00 , C08L39/06 , H01B13/00 , C08K3/20 , C08L71/02 , C09D7/40
CPC classification number: C09D5/24 , C08K3/20 , C08K2201/005 , C08K2201/011 , C08L39/06 , C08L71/02 , C09D5/00 , C09D7/40 , C09D7/61 , C09D7/66 , C09D139/06 , C09D171/02 , C09D201/00 , H01B1/22 , H01B13/0026 , C08K3/22 , C08K2003/2248
Abstract: In a conductive film-forming composition including copper oxide particles, water and a dispersant selected from the group consisting of a water-soluble polymer and a surfactant, the copper oxide particles have a volume average secondary particle size of 20 to 240 nm, and the copper oxide particles are contained in an amount of 10 to 70 wt % with respect to a total weight of the conductive film-forming composition.
-
公开(公告)号:US20240199900A1
公开(公告)日:2024-06-20
申请号:US18588456
申请日:2024-02-27
Applicant: FUJIFILM Corporation
Inventor: Ayato SATO , Toshihiro Kariya , Takeshi Miyato
IPC: C09D11/322 , C09D11/54
CPC classification number: C09D11/322 , C09D11/54
Abstract: Provided are an ink jet ink capable of recording an image with excellent adhesiveness to a base material or the like (for example, lamination strength between an image and a base material for lamination which is disposed on an image surface of an image recorded material), and applications thereof. The ink jet ink contains water, a white pigment, and at least two kinds of resins, and the ink jet ink has an acid value of 8.0 mgKOH/g or less.
-
公开(公告)号:US10457823B2
公开(公告)日:2019-10-29
申请号:US15696188
申请日:2017-09-06
Applicant: FUJIFILM Corporation
Inventor: Koji Yasuda , Toshihiro Kariya , Atsushi Kaeriyama
IPC: B41J2/01 , C09D11/30 , C08F12/22 , C08F20/28 , C08F20/58 , C09D11/106 , B41M5/00 , C08F212/08 , C08F220/14 , C08F220/18 , C08F220/28 , C08F12/26 , C09D11/322 , C09D11/54
Abstract: An aqueous ink composition includes an aqueous medium and resin microparticles formed from a resin, in which the resin has a structural unit represented by General Formula (1) or (2), and the content of the resin microparticles is 1% to 15% by mass, R1, R2, and R3 each represent a hydrogen atom or an alkyl group having 1 to 4 carbon atoms; A1 represents —O— or —NR3—; L1 represents an alkylene group having 6 to 22 carbon atoms; M1 and M2 each represent a hydrogen atom, an alkali metal ion, or an ammonium ion; A2 represents a single bond, —COO—, or —CONH—; and L2 represents a divalent linking group having 6 to 23 carbon atoms.
-
公开(公告)号:US09271401B2
公开(公告)日:2016-02-23
申请号:US13792250
申请日:2013-03-11
Applicant: FUJIFILM CORPORATION
Inventor: Toshihiro Kariya , Seishi Kasai , Mitsuyuki Tsurumi
CPC classification number: H05K3/125 , B05D7/14 , C09D11/101 , C09D11/30 , C23C18/1608 , C23C18/206 , C23C18/30 , H05K3/1241 , H05K3/182 , H05K2203/013 , H05K2203/0709
Abstract: The present invention provides a method for manufacturing a metal film material, the method including: applying an ink composition by discharging the ink composition onto a substrate via an inkjet method, the ink composition containing at least one first monomer having at least one group selected from the group consisting of a cyano group, an alkyloxy group, an amino group, a pyridine residue, a pyrrolidone residue, an imidazole residue, an alkylsulfanyl group, or a cyclic ether residue, at least one second monomer that has polyfunctionality, and at least one polymerization initiator, a total monomer content in the ink composition being 85% by mass or greater; forming a cured film by carrying out at least one of light exposure or heating of the ink composition that has been applied; applying a plating catalyst or a precursor thereof to the cured film; and a plating processing step of performing plating with respect to the plating catalyst or precursor thereof that has been applied.
Abstract translation: 本发明提供了一种制造金属膜材料的方法,该方法包括:通过喷墨方法将油墨组合物喷射到基材上来施加油墨组合物,该油墨组合物含有至少一种具有至少一个选自以下的基团的第一单体: 由氰基,烷氧基,氨基,吡啶残基,吡咯烷酮残基,咪唑残基,烷基硫烷基或环醚残基组成的组,至少一种具有多官能度的第二单体,至少 一个聚合引发剂,油墨组合物中的总单体含量为85质量%以上; 通过进行所施加的油墨组合物的曝光或加热中的至少一种来形成固化膜; 将电镀催化剂或其前体施加到固化膜上; 以及对所施加的电镀催化剂或其前体进行电镀的电镀处理工序。
-
公开(公告)号:US20240287341A1
公开(公告)日:2024-08-29
申请号:US18655426
申请日:2024-05-06
Applicant: FUJIFILM Corporation
Inventor: Ayato SATO , Toshihiro Kariya , Tekeshi Miyato
IPC: C09D11/40 , C09D11/322 , C09D11/54
CPC classification number: C09D11/40 , C09D11/322 , C09D11/54
Abstract: Provided are an ink jet ink set for an impermeable base material, comprising: a pretreatment liquid that contains water and a urethane resin having a glass transition temperature of −55° C. to 50° C., and a colored ink that contains water, a pigment other than a white pigment, and a urethane resin, and an application thereof.
-
公开(公告)号:US11299643B2
公开(公告)日:2022-04-12
申请号:US16808372
申请日:2020-03-04
Applicant: FUJIFILM CORPORATION
Inventor: Toshihiro Kariya
IPC: C09D11/107 , B41M5/00 , C09D11/322 , G02B5/20 , B41J11/00 , B41J2/21 , B41J2/01 , C08K3/11
Abstract: An active energy ray curable-type ink jet ink containing: titanium black; and a monomer A which is a non-aromatic heterocyclic compound having an ethylenically unsaturated double bond, a light shielding film, and a method of manufacturing the light shielding film.
-
-
-
-
-
-