Abstract:
An embodiment of the present invention provides a laminated polyester film including: a biaxially oriented polyester film which is produced by stretching an un-stretched polyester film in a first direction and stretching the resultant in a second direction perpendicular to the first direction along a film surface and has a small endothermic peak temperature of 160° C. or higher and 210° C. or lower, which is derived from a heat setting temperature measured by differential scanning calorimetry; and an undercoat layer which is formed by applying an undercoat layer forming composition onto one surface of the polyester film stretched in the first direction before being stretched in the second direction, and stretching the resultant in the second direction, and has a modulus of elasticity of 0.7 GPa or higher, a production method thereof, and a solar cell protective sheet and a solar cell module which include the laminated polyester film.
Abstract:
The invention provides a polyester film including: a polyester substrate; and a layered portion that is disposed on at least one surface of the polyester substrate and has an elastic modulus of from 5 MPa to 800 MPa, a ratio of a peak intensity at 988 cm−1 that is observed by subjecting a surface of the polyester substrate to infrared spectroscopy to a peak intensity at 1410 cm−1 that is observed by subjecting a surface of the polyester substrate to infrared spectroscopy satisfying the following Inequality (I): 0.010≦(peak intensity at 988 cm−1)/(peak intensity at 1410 cm−1)≦0.040 (I).
Abstract:
A liquid crystal display device has a light source unit and a liquid crystal cell sandwiched by two polarizing plates. The light emitted by the light source unit has separated peaks in each of blue, green and red wavelength ranges. The green and red peaks have a full width at half maximum intensity of 20 nm or more. At least one of the polarizing plates has a polarizer and a protective film with a Re of 5,000 nm or more and low moisture permeability. The device exhibits excellent color reproducibility and prevents display nonuniformity under a high temperature and high humidity environment.
Abstract:
A method for producing a polyester film includes: an unstretched film formation step of forming an unstretched polyester film having a thickness of from 2.5 mm to 5.0 mm by melt-extruding a polyester resin using an extruder, and cooling the polyester resin; and a stretching step of stretching the formed unstretched polyester film in at least one direction after heating the formed unstretched polyester film so as to have a mean temperature T1 (° C.), a surface temperature, and a central temperature. The mean temperature T1 (° C.) satisfies a relationship represented by formula (1): Tg−20° C.