摘要:
An object of the present invention is to provide a pressure sensitive adhesive composition for an optical member, which is excellent in coating property because of low viscosity, can reduce an amount of an organic solvent used, and can form a pressure sensitive adhesive layer excellent in durability and having high surface uniformity. The present invention relates to a pressure sensitive adhesive composition for an optical member, which comprises a (meth)acrylic polymer, a C6 to C9 hydrocarbon-based solvent (A), and a high-boiling highly solubilizing solvent (B) having a boiling point higher than that of the above hydrocarbon-based solvent and having a higher ability to solubilize the (meth)acrylic polymer than that of the above hydrocarbon-based solvent, wherein a content of the hydrocarbon-based solvent (A) is 20 to 60 wt % based on the total amount of the solvents, and a ratio of the content (wt %) of the hydrocarbon-based solvent (A) to the content (wt %) of the high-boiling highly solubilizing solvent (B) (high-boiling highly solubilizing solvent (B)/hydrocarbon-based solvent (A)) is 0.05 to 4.
摘要:
An object of the present invention is to provide a pressure sensitive adhesive composition for an optical member, which is excellent in coating property because of low viscosity, can reduce an amount of an organic solvent used, and can form a pressure sensitive adhesive layer excellent in durability and having high surface uniformity. The present invention relates to a pressure sensitive adhesive composition for an optical member, which comprises a (meth)acrylic polymer, a C6 to C9 hydrocarbon-based solvent (A), and a high-boiling highly solubilizing solvent (B) having a boiling point higher than that of the above hydrocarbon-based solvent and having a higher ability to solubilize the (meth)acrylic polymer than that of the above hydrocarbon-based solvent, wherein a content of the hydrocarbon-based solvent (A) is 20 to 60 wt % based on the total amount of the solvents, and a ratio of the content (wt %) of the hydrocarbon-based solvent (A) to the content (wt %) of the high-boiling highly solubilizing solvent (B) (high-boiling highly solubilizing solvent (B)/hydrocarbon-based solvent (A)) is 0.05 to 4.
摘要:
This invention provides a pressure-sensitive adhesive composition that exhibits excellent pressure-sensitive adhesive properties after crosslinking treatment, does not cause lifting or lifting upon heat treatment or treatment under high-humidity conditions particularly even in the case of a pressure-sensitive adhesive layer having a reduced layer thickness, and has excellent durability. A pressure-sensitive adhesive layer formed using the pressure-sensitive adhesive composition, and a process for producing the same are also provided. Further, an optical member with pressure-sensitive adhesive comprising the pressure-sensitive adhesive layer and an image display using the same are provided. The pressure-sensitive adhesive composition is characterized by comprising 100 parts by weight of an (meth)acrylic polymer and 0.02 to 2 parts by weight of a peroxide, and 0.02 to 2 parts by weight of an isocyanate crosslinking agent, the (meth)acrylic polymer comprising as monomer units 50 to 98% by weight of an (meth)acrylic monomer represented by general formula CH2═C(R1)COOR2, wherein R1 represents hydrogen or a methyl group and R2 represents an alkyl group having 2 to 14 carbon atoms, and 0.1 to 35% by weight of a nitrogen-containing monomer.
摘要:
This invention provides a pressure-sensitive adhesive composition that exhibits excellent pressure-sensitive adhesive properties after crosslinking treatment, does not cause lifting or lifting upon heat treatment or treatment under high-humidity conditions particularly even in the case of a pressure-sensitive adhesive layer having a reduced layer thickness, and has excellent durability. A pressure-sensitive adhesive layer formed using the pressure-sensitive adhesive composition, and a process for producing the same are also provided. Further, an optical member with pressure-sensitive adhesive comprising the pressure-sensitive adhesive layer and an image display using the same are provided. The pressure-sensitive adhesive composition is characterized by comprising 100 parts by weight of an (meth)acrylic polymer and 0.02 to 2 parts by weight of a peroxide, and 0.02 to 2 parts by weight of an isocyanate crosslinking agent, the (meth)acrylic polymer comprising as monomer units 50 to 98% by weight of an (meth)acrylic monomer represented by general formula CH2═C(R1)COOR2, wherein R1 represents hydrogen or a methyl group and R2 represents an alkyl group having 2 to 14 carbon atoms, and 0.1 to 35% by weight of a nitrogen-containing monomer.
摘要:
The present invention provides a pressure sensitive adhesive composition for optical members, which is excellent in durability, re-releasability and stress relaxation, as well as a pressure sensitive adhesive composition for optical members, which hardly increases adhesion after storage for a long time and does not leave a residual adhesive on glass upon disposal or repair. The pressure sensitive adhesive composition for optical members according to the present invention comprises 100 parts by weight of an acrylic polymer (A) having a weight-average molecular weight of 500,000 or more, containing at least 50 wt % alkyl (meth)acrylate having an alkyl group with 5 or more carbon atoms and 0.2 to 2 wt % unsaturated carboxylic acid as the monomer unit, 0.1 to 4 parts by weight of an acrylic polymer (B) having a weight-average molecular weight of 2,000 to 50,000, containing at least 70 wt % alkyl(meth)acrylate and 1 to 7 wt % unsaturated carboxylic acid as the monomer unit and having a higher carboxylic acid equivalent than that of the acrylic polymer (A), 0.01 to 1 part by weight of a silane coupling agent, and a crosslinking agent.
摘要:
Provided are a pressure sensitive adhesive composition for optical members and a pressure sensitive adhesive composition for optical members. The pressure sensitive adhesive composition for optical members according to the present invention comprises 100 parts by weight of an acrylic polymer (A) having a weight-average molecular weight of 500,000 or more, containing at least 50 wt % alkyl (meth)acrylate having an alkyl group with 5 or more carbon atoms and 0.2 to 2 wt % unsaturated carboxylic acid as the monomer unit, 0.1 to 4 parts by weight of an acrylic polymer (B) having a weight-average molecular weight of 2,000 to 50,000, containing at least 70 wt % alkyl (meth)acrylate and 1 to 7 wt % unsaturated carboxylic acid as the monomer unit and having a higher carboxylic acid equivalent than that of the acrylic polymer (A), 0.01 to 1 part by weight of a silane coupling agent, and a crosslinking agent.
摘要:
Provided are a pressure sensitive adhesive composition for optical members and a pressure sensitive adhesive composition for optical members. The pressure sensitive adhesive composition for optical members according to the present invention comprises 100 parts by weight of an acrylic polymer (A) having a weight-average molecular weight of 500,000 or more, containing at least 50 wt % alkyl (meth)acrylate having an alkyl group with 5 or more carbon atoms and 0.2 to 2 wt % unsaturated carboxylic acid as the monomer unit, 0.1 to 4 parts by weight of an acrylic polymer (B) having a weight-average molecular weight of 2,000 to 50,000, containing at least 70 wt % alkyl (meth)acrylate and 1 to 7 wt % unsaturated carboxylic acid as the monomer unit and having a higher carboxylic acid equivalent than that of the acrylic polymer (A), 0.01 to 1 part by weight of a silane coupling agent, and a crosslinking agent.
摘要:
The present invention provides a pressure sensitive adhesive composition for optical members, which is excellent in durability, re-releasability and stress relaxation, as well as a pressure sensitive adhesive composition for optical members, which hardly increases adhesion after storage for a long time and does not leave a residual adhesive on glass upon disposal or repair. The pressure sensitive adhesive composition for optical members according to the present invention comprises 100 parts by weight of an acrylic polymer (A) having a weight-average molecular weight of 500,000 or more, containing at least 50 wt % alkyl (meth)acrylate having an alkyl group with 5 or more carbon atoms and 0.2 to 2 wt % unsaturated carboxylic acid as the monomer unit, 0.1 to 4 parts by weight of an acrylic polymer (B) having a weight-average molecular weight of 2,000 to 50,000, containing at least 70 wt % alkyl(meth)acrylate and 1 to 7 wt % unsaturated carboxylic acid as the monomer unit and having a higher carboxylic acid equivalent than that of the acrylic polymer (A), 0.01 to 1 part by weight of a silane coupling agent, and a crosslinking agent.
摘要:
To provide a pressure-sensitive adhesive optical film that can satisfy durability even when a thin pressure-sensitive adhesive layer is formed. A pressure-sensitive adhesive optical film comprising an optical film and a pressure-sensitive adhesive layer on at least one side of the optical film, wherein the pressure-sensitive adhesive layer is formed by a pressure-sensitive adhesive, comprising: a (meth)acrylic polymer having a weight average molecular weight of 1,500,000 to 2,800,000; containing, as a monomer component, 3 to 10% by weight of a heterocyclic ring-containing acrylic monomer; 0.5 to 5% by weight of a carboxyl group-containing monomer; 0.05 to 2% by weight of a hydroxyl group-containing monomer; and 83 to 96.45% by weight of an alkyl(meth)acrylate monomer, and a crosslinking agent.
摘要:
To provide a pressure-sensitive adhesive optical film that can satisfy durability even when a thin pressure-sensitive adhesive layer is formed. A pressure-sensitive adhesive optical film comprising an optical film and a pressure-sensitive adhesive layer on at least one side of the optical film, wherein the pressure-sensitive adhesive layer is formed by a pressure-sensitive adhesive, comprising: a (meth)acrylic polymer having a weight average molecular weight of 1,500,000 to 2,800,000; containing, as a monomer component, 3 to 10% by weight of a heterocyclic ring-containing acrylic monomer; 0.5 to 5% by weight of a carboxyl group-containing monomer; 0.05 to 2% by weight of a hydroxyl group-containing monomer; and 83 to 96.45% by weight of an alkyl(meth)acrylate monomer, and a crosslinking agent.