摘要:
The present invention relates to a composition comprising more than 25 weight % (based on the weight of the composition) of one or more ethylene polymers having an Mw of 20,000 g/mole or more and at least 0.1 weight % of a liquid hydrocarbon modifier where the modifier has: 1) a viscosity index of 120 or more, and 2) an kinematic viscosity of 3 to 3000 cSt at 100° C., and 3) a pour point of −10° C. or less, and 4) a flash point of 200° C. or more; and wherein the modifier contains less than 5 weight % of functional groups selected from hydroxide, aryls, substituted aryls, halogens, alkoxys, carboxylates, esters, acrylates, oxygen, nitrogen, and carboxyl, based upon the weight of the modifier.
摘要:
The present invention relates to radiation resistant plasticized polyolefin compositions comprising a polyolefin and a non-functionalized hydrocarbon plasticizer.
摘要:
Polyethylene blend compositions suitable for rotomolding, rotomolded articles, and processes for rotomolding articles are provided. The polyethylene compositions include a first polyethylene having a melt index of 0.4 to 3.0 g/10 min and a density of from 0.910 to 0.930 g/cm3; and a second polyethylene having a melt index of 10 to 30 g/10 min and a density of 0.945 to 0.975 g/cm3. The composition has a density of from 0.930 to 0.955 g/cm3 and a melt index of 1.5 to 12 g/10 min, and the first and second polyethylenes differ in density by from 0.030 to 0.048 g/cm3. These compositions exhibit improved physical properties, such as Environmental Stress Crack Resistance and Izod Impact Strength.
摘要翻译:提供适合于滚塑的聚乙烯共混组合物,滚塑制品和滚塑制品的方法。 聚乙烯组合物包括熔体指数为0.4-3.0g / 10min,密度为0.910-0.930g / cm 3的第一聚乙烯; 和熔体指数为10〜30g / 10min,密度为0.945〜0.975g / cm 3的第二聚乙烯。 该组合物的密度为0.930至0.955g / cm 3,熔体指数为1.5至12g / 10min,第一和第二聚乙烯的密度在0.030至0.048g / cm 3。 这些组合物表现出改善的物理性能,例如环境应力开裂抗力和艾佐德冲击强度。
摘要:
Elastomeric compositions comprising graphite nanoparticles (preferably graphene nanoparticles) and methods for making same. Such compositions are useful for tire innertubes and tire innerliners.
摘要:
Polyethylene blend compositions suitable for rotomolding, rotomolded articles, and processes for rotomolding articles are provided. The polyethylene compositions include a first polyethylene having a melt index of 0.4 to 3.0 g/10 min and a density of from 0.910 to 0.930 g/cm3; and a second polyethylene having a melt index of 10 to 30 g/10 min and a density of 0.945 to 0.975 g/cm3. The composition has a density of from 0.930 to 0.955 g/cm3 and a melt index of 1.5 to 12 g/10 min, and the first and second polyethylenes differ in density by from 0.030 to 0.048 g/cm3. These compositions exhibit improved physical properties, such as Environmental Stress Crack Resistance and Izod Impact Strength. Articles produced from the compositions may also exhibit improved impact resistance properties, enhanced ductile break properties, and improved deflection resistance, which represents a combination of creep and fatigue resistance.
摘要翻译:提供适合于滚塑的聚乙烯共混组合物,滚塑制品和滚塑制品的方法。 聚乙烯组合物包括熔体指数为0.4-3.0g / 10min,密度为0.910-0.930g / cm 3的第一聚乙烯; 和熔体指数为10〜30g / 10min,密度为0.945〜0.975g / cm 3的第二聚乙烯。 该组合物的密度为0.930至0.955g / cm 3,熔体指数为1.5至12g / 10min,第一和第二聚乙烯的密度在0.030至0.048g / cm 3。 这些组合物表现出改善的物理性能,例如环境应力开裂抗力和艾佐德冲击强度。 由组合物制备的制品也可以表现出改进的抗冲击性能,增强的延性断裂性能和改进的抗挠曲性,其代表蠕变和抗疲劳性的组合。
摘要:
The present invention provides a process for producing high elongation elastomers and highly oriented films and fibers from polymers having specific associative groups, such that the end groups on each macromolecule tend to associate with one another after the macromolecules are in a disentangled state, i.e., in the form of a semi-dilute solution. This association is of a force strong enough to prevent the macromolecular chains from slipping past one another and reentangling when the polymer is moderately heated or further concentrated in solution. The association may be manipulated, i.e., is reversible, under a change in parameter such as temperature, pH, polarity of the solvent medium and like parameters. The associated polymer macromolecules can be drawn as a gel from a semi-dilute solution into a highly aligned disentangled polymer to yield shaped articles.
摘要:
Elastomeric compositions comprising graphite nanoparticles (preferably graphene nanoparticles) and methods for making same. Such compositions are useful for tire innertubes and tire innerliners.
摘要:
The present invention relates to a method to produce highly branched polymers with a polyolefin backbone structure of ethylene and precise control of the nature of the branching. In particular, the distribution of branch length and number of branches can be more precisely controlled via the polymerization method of the present invention. The method comprises using anionic chemistry to make unsaturated polydienes with a well-defined, highly-branched structure, and then hydrogenating these polydienes to form highly branched or dendritic saturated hydrocarbon polymers. Highly branched or dendritic polyethylene, ethylene-propylene copolymer and atactic polypropylene are among the saturated hydrocarbon polymers that can be anionically synthesized via the proper selection of diene monomer type, coupling agent, and hydrogenation conditions. The highly branched or dendritic saturated hydrocarbon polymers of the present invention find application in injection molding and extrusion processes as a minor additive for improving processability of linear polyolefins by delaying the onset of melt fracture, and correspondingly increasing melt throughput rates. An additional benefit is that the mechanical properties of the polyolefinic film, sheet, pipe or fiber produced with minor amounts of highly branched or dendritic saturated hydrocarbon polymers of the present disclosure are not negatively impacted.