摘要:
The invention relates to an at least two-layer polyester film with a total thickness of from 5 to 200 μm which comprises, alongside polyethylene terephthalate, from 2 to 20% by weight—based on the weight of the entire film—of polyethylene naphthalate (PEN), where at least one outer layer comprises less than 0.1% by weight of PEN (based on the weight of this outer layer).
摘要:
The invention relates to a polyester film with a thickness of from about 4 to about 23 μm, which comprises, alongside polyethylene terephthalate as main constituent, from about 2 to about 20% by weight of polyethylene naphthalate (based on the weight of the film), and has fewer than 30 pinholes per 100 m2. The invention further relates to a process for producing these films, and to the use of the films in packaging composites.
摘要:
The invention relates to a white, biaxially-oriented and coextruded polyester film which is matt on at least one side with at least one base layer B, which contains a cycloolefin copolymer (COC) in amounts of 4 to 60 wt. %, based on the weight of the base layer, in addition to polyester starting material. The glass transition temperature Tg of the COC lies in the range from 70 to 270° C. Said film has at least one matt outer layer (A), made from polyester and is particularly suitable for use in fast running machines such as winding, metallising, printing or laminating machines.
摘要:
A process for producing a biaxially oriented polyester film which has a base layer (B) and has a heatsealable outer layer (A) that can be peeled from polyester, where the outer layer (A) includes from 60 to 99% by weight of polyester which is composed of from 12 to 89 mol % of units derived from an aromatic dicarboxylic acid and of from 11 to 88 mol % of units derived from at least one aliphatic dicarboxylic acid, where the total of the molar percentages is 100, encompassing the steps of a) extruding of at least the base layer (B) to give an unoriented film; b) stretching this film in a first direction; c) stretching this film in a second direction perpendicular to the first d) heat-setting the stretched film, and e) producing the outer layer (A) on the base layer (B) by using lamination to apply the outer layer film (A) produced in a separate process, where the lamination step e) takes place prior to step b) or between steps b) and c).
摘要:
Coextruded, biaxially oriented polyester films which have a base layer (B) and have a heatsealable outer layer (A) that can be peeled from APET/CPET and from CPET, where the outer layer (A) includes a) from 80 to 98% by weight of polyester and b) from 2 to 10% by weight of inorganic and/or organic particles with a median diameter d50 of from 3 to 12 μm, and where c) the polyester is composed of from 12 to 89 mol % of units derived from at least one aromatic dicarboxylic acid and of from 11 to 88 mol % of units derived from at least one aliphatic dicarboxylic acid, and d) the ratio calculated from the particle size d50 of the particles and the layer thickness dA of the outer layer (A) is greater than or equal to 1.5, and the shrinkage of the films, at least in one direction, is more than 5%. The films of the invention are especially suitable, owing to their property of self-venting, as a lid film for APET/CPET or CPET trays.
摘要:
Coextruded, biaxially oriented polyester films which have a white base layer (B) and have a heatsealable outer layer (A) that can be peeled from APET/CPET and from CPET, where the outer layer (A) includes a) from 80 to 99% by weight of polyester and b) from 1 to 10% by weight of inorganic and/or organic particles with a median diameter d50 of from 2.5 to 12 μm, and where c) the polyester is composed of from 12 to 89 mol% of units derived from at least one aromatic dicarboxylic acid and of from 11 to 88 mol % of units derived from at least one aliphatic dicarboxylic acid, and d) the ratio calculated from the particle size d50 of the particles and the layer thickness dA of the outer layer (A) is greater than or equal to 1, and the base layer (B) comprises an inorganic white pigment and/or a polymer incompatible with polyester. The films of the invention are suitable as a packaging material for foods and other consumable goods or as a lid film for APET/CPET or CPET trays.
摘要:
This invention relates to a coextruded, transparent, biaxially oriented polyester film comprising a base layer (B) and a heatsealable top layer (A) which is peelable from at least the APET side of an APET/CPET tray, the heatsealable and peelable top layer (A) consisting of a) 50–95% by weight of polyester and b) 5–40% by weight of a polyester-incompatible polymer (=anti-PET polymer) based on the mass of the top layer (A), wherein c) the polyester is composed of 20–95 mol % of units derived from at least one aromatic dicarboxylic acid and 5–80 mol % of units derived from at least one aliphatic dicarboxylic acid, and d) the layer thickness dA is from 1.3 to 3.0 μm. The invention further relates to a process for producing the film and to its use.
摘要翻译:本发明涉及一种共挤出,透明的双轴取向聚酯膜,其包含可从APET / CPET托盘的至少APET侧剥离的基底层(B)和可热封顶层(A),可热封和可剥离顶层 (A)由a)50-95重量%的聚酯和b)基于顶层(A)的质量的5-40重量%的聚酯不相容聚合物(=抗PET聚合物),其中 c)聚酯由20-95mol%的衍生自至少一种芳族二羧酸的单元和5-80mol%衍生自至少一种脂族二羧酸的单元组成,以及d)层厚度d A SUB>为1.3〜3.0μm。 本发明还涉及一种制备该膜及其用途的方法。
摘要:
Three-layer, highly oriented polyester films having an A-B-C layer construction, preferably made of polyethylene terephthalate, which, in addition to a base layer B have a smooth surface layer A which contains no external particles and a rough surface layer C which contains external particles such as antiblocking agents or pigments, preferably SiO2, in defined amounts and particle sizes, and the surface layer A is additionally provided with an acrylate-containing layer D feature in particular good producibility and processibility, high gloss of the film surface A and low opacity. The very smooth surface A or D is suitable in particular for coating with materials, for example SiOx, by means of plasma polymerization of hexamethyldisiloxane by the CVD or PECVD method, which provides the film with a high oxygen barrier and is suitable in particular as packaging for light- and air-sensitive foods or other consumable items.
摘要:
The invention relates to a process for producing a biaxially oriented polyester film which has a base layer (B) and has a heatsealable outer layer (A) that can be peeled from polyester, where the outer layer (A) includes from 60 to 99 % by weight of polyester which is composed of from 12 to 89 mol % of units derived from at least one aromatic dicarboxylic acid and of from 11 to 88 mol % of units derived from at least one aliphatic dicarboxylic acid, where the total of the molar percentages is 100, encompassing the steps of a) coextrusion of at least the base layer (B) and of the outer layer (A) to give an unoriented film, b) simultaneous, biaxial stretching of this unoriented film, and c) heat-setting of the stretched film.
摘要:
Coextruded, biaxially oriented polyester films which have a base layer (B) and have a heatsealable outer layer (A) that can be peeled from APET/CPET and from CPET, where the outer layer (A) includes a) from 60 to 99% by weight of polyester and b) from 1 to 10% by weight of inorganic and/or organic particles with a median diameter d50 of from 2 to 8 μm, and where c) the polyester is composed of from 12 to 89 mol % of units derived from at least one aromatic dicarboxylic acid and of from 11 to 88 mol % of units derived from at least one aliphatic dicarboxylic acid, and the non-sealable surface of the film has been rendered adhesion-promoting. The films of the invention are suitable as a packaging material for foods and other consumable items, and as a lid film for APET/CPET or CPET trays.