摘要:
A flat steel product having a tensile strength of at least 1200 MPa and consists of steel containing (wt %) C: 0.10-0.50%, Si: 0.1-2.5%, Mn: 1.0-3.5%, Al: up to 2.5%, P: up to 0.020%, S: up to 0.003%, N: up to 0.02%, and optionally one or more of the elements “Cr, Mo, V, Ti, Nb, B and Ca” in the quantities: Cr: 0.1-0.5%, Mo: 0.1-0.3%, V: 0.01-0.1%, Ti: 0.001-0.15%, Nb: 0.02-0.05%, wherein Σ(V, Ti, Nb)≦0.2% for the sum of the quantities of V, Ti and Nb, B: 0.0005-0.005%, and Ca: up to 0.01% in addition to Fe and unavoidable impurities. The flat steel product has a microstructure with (in surface percent) less than 5% ferrite, less than 10% bainite, 5-70% untempered martensite, 5-30% residual austenite, and 25-80% tempered martensite, at least 99% of the iron carbide contained in the tempered martensite having a size of less than 500 nm.
摘要:
A flat steel product having a tensile strength of at least 1200 MPa and consists of steel containing (wt %) C: 0.10-0.50%, Si: 0.1-2.5%, Mn: 1.0-3.5%, Al: up to 2.5%, P: up to 0.020%, S: up to 0.003%, N: up to 0.02%, and optionally one or more of the elements “Cr, Mo, V, Ti, Nb, B and Ca” in the quantities: Cr: 0.1-0.5%, Mo: 0.1-0.3%, V: 0.01-0.1%, Ti: 0.001-0.15%, Nb: 0.02-0.05%, wherein Σ(V, Ti, Nb)≦0.2% for the sum of the quantities of V, Ti and Nb, B: 0.0005-0.005%, and Ca: up to 0.01% in addition to Fe and unavoidable impurities. The flat steel product has a microstructure with (in surface percent) less than 5% ferrite, less than 10% bainite, 5-70% untempered martensite, 5-30% residual austenite, and 25-80% tempered martensite, at least 99% of the iron carbide contained in the tempered martensite having a size of less than 500 nm.
摘要:
An apparatus and a method for the treatment of a flat steel product, taking place in throughput. The apparatus includes an indirectly heated annealing furnace chamber, a conveyor device for continuously conveying the flat steel product over a conveyor path leading from an entry to an exit of the annealing furnace chamber, and nozzle arrangements for feeding atmosphere gas, which is reactive in relation to the flat steel product, into the annealing furnace chamber. A controlled treatment of the flat steel product includes a first nozzle arrangement, from which a gas jet induces a first gas flow towards the entry of the annealing furnace chamber and sweeping over the surface of flat steel product to be treated. A second nozzle arrangement includes a gas jet which induces a second gas flow directed towards the exit of the annealing furnace chamber and sweeping over the surface of flat steel product.
摘要:
An apparatus and a method for the treatment of a flat steel product, taking place in throughput. The apparatus includes an indirectly heated annealing furnace chamber, a conveyor device for continuously conveying the flat steel product over a conveyor path leading from an entry to an exit of the annealing furnace chamber, and nozzle arrangements for feeding atmosphere gas, which is reactive in relation to the flat steel product, into the annealing furnace chamber. A controlled treatment of the flat steel product includes a first nozzle arrangement, from which a gas jet induces a first gas flow towards the entry of the annealing furnace chamber and sweeping over the surface of flat steel product to be treated. A second nozzle arrangement includes a gas jet which induces a second gas flow directed towards the exit of the annealing furnace chamber and sweeping over the surface of flat steel product.
摘要:
The invention relates to a coated steel sheet or strip with a ground coating made of steel, onto at least one upper side of which a coating is applied by hot-dip galvanizing, the coating being formed from a melt consisting of 0.05-0.30% by weight Al and 0.2-2.0% by weight Mg, the remainder being zinc and unavoidable impurities, and, with a coating thickness of a maximum of 3.5 μm on each side and a coating weight of a maximum 25 g/m2 on each side, guarantees that the steel sheet, in the salt spray mist test carried out in accordance with DIN 50021-SS, shows the first formation of red rust at the earliest after 250 hours. With such a sheet or strip, a flat steel product is provided which possesses an optimum combination of high corrosion resistance and optimum weldability and which is particularly well-suited for use as a material for motor vehicle chassis construction or for the construction of domestic appliances.
摘要翻译:本发明涉及具有由钢制成的地面涂层的涂覆钢板或带材,其至少一个上侧通过热浸镀锌施加涂层,该涂层由熔体组成,熔体由0.05-0.30% 重量Al和0.2-2.0%重量的Mg,其余为锌和不可避免的杂质,并且每侧涂层厚度最大为3.5μm,涂层重量最大为25g / m 2, / SUP>,确保钢板在按照DIN 50021-SS进行的盐雾试验中,250小时后首次形成红锈。 对于这样的片材或带材,可以提供具有高耐腐蚀性和最佳可焊性的最佳组合的扁钢制品,特别适合用作机动车底盘结构材料或家用电器的构造。
摘要:
A method for hot dip coating a flat stainless steel product with more than 5 wt. % Cr with a protective metallic coating by: heating the flat steel product under an oxygen-free heating atmosphere to 100° C.-600° C. within 1-30 seconds; continuing heating to a holding temperature of 750° C.-950° C., by heating to 550° C.-800° C. under an inert or reducing atmosphere, holding within this temperature window for 1 to 15 seconds under an oxidizing atmosphere, and continuing heating under an inert or reducing atmosphere, until the holding temperature is reached; holding at the holding temperature for 10-120 seconds under a reducing atmosphere; and passing the flat steel product through a nozzle area under an inert or reducing atmosphere at 430°-780° C. and into a molten bath in which the flat steel product is coated with the metallic coating.
摘要:
The invention relates to the field of materials science and to a device for reducing pressure in cavities in media at higher temperatures, such as those devices which can be used for devices for hot-dip coating metal materials in the metal processing industry for example. The aim of the invention is to provide a device by means of which pressure can be reduced in the cavity of the hollow bodies in a reliable and controlled manner and simultaneously the penetration of the media can be delayed or completely prevented at the higher temperatures. This is achieved by a device for reducing pressure in hollow bodies in media at higher temperatures, wherein at least one opening to the cavity of the hollow body is provided in hollow body regions which are not used for the intended application, said opening being closed from the medium surrounding the hollow body by at least one component made of a gas-permeable metal or ceramic material.
摘要:
The invention relates to the field of materials science and to a device for reducing pressure in cavities in media at higher temperatures, such as those devices which can be used for devices for hot-dip coating metal materials in the metal processing industry for example. The aim of the invention is to provide a device by means of which pressure can be reduced in the cavity of the hollow bodies in a reliable and controlled manner and simultaneously the penetration of the media can be delayed or completely prevented at the higher temperatures. This is achieved by a device for reducing pressure in hollow bodies in media at higher temperatures, wherein at least one opening to the cavity of the hollow body is provided in hollow body regions which are not used for the intended application, said opening being closed from the medium surrounding the hollow body by at least one component made of a gas-permeable metal or ceramic material.
摘要:
Optimal wetting and adhesion of the hot-dip coating by way of pre-oxidation in a DFF pre-heating furnace and humidification of the annealing atmosphere in a holding zone is achieved in a hot dip galvanised flat steel product.
摘要:
Optimal wetting and adhesion of the hot-dip coating by way of pre-oxidation in a DFF pre-heating furnace and humidification of the annealing atmosphere in a holding zone is achieved in a hot dip galvanised flat steel product.