摘要:
A composition suitable for slush molding is disclosed. The composition is mainly comprised of a thermoplastic polyurethane elastomer (A) with a number average molecular weight of 20,000 to 50,000 and a glass transition point of not higher than -35.degree. C., a plasticizer (B), a blocked polyisocyanate (C) and a pigment (D), wherein each of(B), (C) and (D) is respectively contained in a prescribed quantities. The polyurethane-type slush molding composition provides a molded article of low hardness, high elongation at low temperature, and excellent thermal aging resistance and light aging resistance.
摘要:
A composition suitable for slush molding comprising a thermoplastic polyurethane elastomer (A) having a number average molecular weight of 10,000 to 50,000 and a heat softening initiation temperature of 120 to 200° C., a plasticizer (B), a compound (C) containing a radical polymerizable unsaturated group, and optionally an additive. The composition provides a molded article excellent in durability such as thermal/light aging resistance, soft touch at low temperature, and appearance.
摘要:
A composition suitable for slush molding is disclosed. The composition comprises a thermoplastic polyurethane elastomer (A) having a number average molecular weight of 10,000 to 50,000 and mainly comprised of a diol component including an aromatic ring-containing diol and a non-aromatic diisocyanate; a plasticizer (B); and optionally an additive. The composition provides a molded article excellent in durability such as thermal/light aging resistance and chemical resistance, soft touch at low temperature, and appearance.
摘要:
A composition suitable for slush molding is disclosed. The composition comprises a thermoplastic polyurethane elastomer (A) having a number average molecular weight of 10,000 to 50,000, a glass transition point of not higher than −35° C. and a heat softening initiation temperature of 100 to 160° C.; a plasticizer (B); a blocked polyisocyanate (C); a pigment (D); and a blocking inhibitor (E) comprising a resin powder which is not heat-softened even at 160° C. and has an average particle diameter of not more than 10 &mgr;m. The composition has a wide mold temperature range, and provides a molded article excellent in properties at low temperature, anti-fogging, thermal aging resistance and light aging resistance.
摘要:
An instrument panel of a division type, which has distinctly divided portions, reduces restrictions on designing freedom resulting from a break line and a parting line of an air bag door portion and prevents the overall quality of the outward appearance from deteriorating. The instrument panel is of a type that is divided into upper and lower panels, and the lower panel is divided into a passenger-side lower panel and a driver-side lower panel. The parting line of the instrument panel coincides with a cleavage line defined by an upper air bag door portion and a lower air bag door portion. In a lower door insert of the lower air bag door portion, a free end thereof is set wider than a fixed end thereof. The passenger-side lower panel including the lower air bag door portion is entirely covered with a single skin.
摘要:
A method of manufacturing a semiconductor device according to the present invention includes the steps of: (a) introducing hydrogen and oxygen on a SiC substrate; and (b) subjecting the hydrogen and the oxygen to a combustion reaction on the SiC substrate to form a gate oxide film being a silicon oxide film on a surface of the SiC substrate by the combustion reaction.
摘要:
There is provided a liquid discharging head discharging a liquid, including: a channel unit having a liquid channel including a pressure chamber which has an opening at one surface of the channel unit; a piezoelectric element formed of a piezoelectric material; an intermediate member preventing the liquid in the pressure chamber and the piezoelectric element from making contact with each other; a first adhesive layer composed of a first adhesive and adhering the channel unit and the intermediate member, the first adhesive being a thermo-setting adhesive starting to be cured at a first temperature; and a second adhesive layer composed of a second adhesive and adhering the intermediate member and the piezoelectric element, the second adhesive starting to be cured at a second temperature lower than the first temperature.
摘要:
The present invention provides a novel fluorine-containing rubber composite material having both of excellent fuel impermeability and excellent cold resistance, a fuel impermeable sealing material comprising the composite material and a process for preparing the composite material. The fluorine-containing rubber composite material comprises crosslinked particles of fluorine-containing silicone rubber dispersed in a fluorine-containing rubber. It is preferable that the fluorine-containing rubber comprises a vinylidene fluoride/tetrafluoroethylene/perfluoro vinyl ether copolymer, and the composite material has cold resistance of not more than −35° C. and fuel permeability of not more than 500 g·mm/m2·day. The fuel impermeable sealing material comprises the composite material. The process for preparing the composite material comprises a step for co-coagulation of a fluorine-containing rubber emulsion and an emulsion of crosslinked fluorine-containing silicone rubber.
摘要翻译:本发明提供一种具有优异的燃料不渗透性和优异的耐寒性的新型含氟橡胶复合材料,包含该复合材料的燃料不可渗透的密封材料以及该复合材料的制备方法。 含氟橡胶复合材料包含分散在含氟橡胶中的含氟硅橡胶的交联颗粒。 含氟橡胶优选包含偏二氟乙烯/四氟乙烯/全氟乙烯基醚共聚物,复合材料的耐寒性不大于-35℃,燃料渗透率不大于500g·mm / m 2 ·天。 燃料不可渗透的密封材料包括复合材料。 制备复合材料的方法包括使含氟橡胶乳液和交联的含氟硅橡胶的乳液共混的步骤。
摘要:
A planarization apparatus and method that thins and planarizes a substrate by grinding and polishing the rear surface of the substrate with high throughput, and that fabricates a semiconductor substrate with reduced adhered contaminants. A planarization apparatus that houses various mechanism elements in semiconductor substrate loading/unloading stage chamber, a rear-surface polishing stage chamber, and a rear-surface grinding stage chamber. The throughput time of the rear-surface polishing stage that simultaneously polishes two substrates is typically about double the throughput time of the rear-surface grinding stage that grinds one substrate.
摘要:
This invention is to provide a process for producing a glycoprotein comprising a mammalian type sugar chain, characterized in that the process comprises introducing an α-1,2-mannosidase gene into a methylotrophic yeast having a mutation of a sugar chain biosynthesizing enzyme gene, so that the α-1,2-mannosidase gene is expressed under the control of a potent promoter in the yeast; culturing in a medium the methylotrophic yeast cells with a heterologous gene transferred thereinto; and obtaining the glycoprotein comprising a mammalian type sugar chain from the culture. Using the newly created methylotrophic yeast having a sugar chain mutation, a neutral sugar chain identical with a high mannose type sugar chain produced by mammalian cells such as human cells, or a glycoprotein comprising such a neutral sugar chain, can be produced in a large amount at a high purity. By introducing a mammalian type sugar chain biosynthesizing gene into the above-described mutant, a mammalian type sugar chain, such as a hybrid or complex, or a protein comprising a mammalian type sugar chain can be efficiently produced.