Ferrule for optical fiber connector and method for production thereof
    1.
    发明授权
    Ferrule for optical fiber connector and method for production thereof 失效
    光纤连接器用套圈及其制造方法

    公开(公告)号:US6158900A

    公开(公告)日:2000-12-12

    申请号:US993573

    申请日:1997-12-18

    摘要: Disclosed are ferrules for an optical fiber connector provided with an insertion hole for setting an optical fiber in position and methods for the production thereof. The ferrule is formed of an amorphous alloy possessing at least a glass transition region, preferably a glass transition region of not less than 30 K in temperature width. Preferably the ferrule is formed of an amorphous alloy having a composition represented by the following general formula and containing an amorphous phase in a volumetric ratio of at least 50%:X.sub.a M.sub.b Al.sub.cwherein X represents at least one element selected from the group consisting of Zr and Hf, M represents at least one element selected from the group consisting of Mn, Fe, Co, Ni, and Cu, and a, b, and c represent such atomic percentages as respectively satisfy 25.ltoreq.a.ltoreq.85, 5.ltoreq.b.ltoreq.70, and 0

    摘要翻译: 公开了一种用于光纤连接器的套圈,其具有用于将光纤设置在其上的插入孔和用于制造光纤的方法。 套圈由具有至少玻璃化转变区域的非晶合金形成,优选玻璃化转变区域的温度宽度不低于30K。 优选地,套圈由具有由以下通式表示的组成的无定形合金形成,并且含有至少50%的体积比的非晶相:XaMbAlc,其中X表示选自Zr和Hf中的至少一种元素, M表示选自Mn,Fe,Co,Ni和Cu中的至少一种元素,a,b和c分别表示原子百分数,分别满足25≤a≤85,5, = b

    Sleeve for optical connector ferrules and method for production thereof
    2.
    发明授权
    Sleeve for optical connector ferrules and method for production thereof 失效
    用于光学连接器套圈的套筒及其制造方法

    公开(公告)号:US06213649B1

    公开(公告)日:2001-04-10

    申请号:US09075190

    申请日:1998-05-11

    IPC分类号: G02B626

    摘要: Disclosed are a sleeve for abutting, aligning, and retaining opposed optical connector ferrules and methods for the production thereof. The sleeve has a tubular body provided at three points on the inner wall surface thereof with ridges of an arcuate cross section extending from one to the other end of the tubular body in the longitudinal direction thereof and a slit formed therein in the longitudinal direction thereof. The sleeve is formed of an amorphous alloy possessing at least a glass transition region, preferably a glass transition region of not less than 30 K in temperature width. Preferably the sleeve is formed of an amorphous alloy having a composition represented by the following general formula and containing an amorphous phase in a volumetric ratio of at least 50%: XaMbAlc wherein X represents either or both of two elements, Zr and Hf, M represents at least one element selected from the group consisting of Mn, Fe, Co, Ni, and Cu, and a, b, and c represent such atomic percentages as respectively satisfy 25≦a≦85, 5≦b≦70, and 0

    摘要翻译: 公开了用于邻接,对准和保持相对的光学连接器套圈的套筒及其制造方法。 套管具有在其内壁表面上的三个点上设置有沿其纵向方向从管状体的一端延伸到另一端的弓形横截面的脊部和在其纵向方向上形成的狭缝的管状体。 该套筒是由具有至少玻璃化转变区域的非晶合金形成的,优选玻璃化转变区域的温度宽度不低于30K。 优选地,套筒由具有由以下通式表示的组成的非晶态合金形成,并且含有至少50%的体积比的非晶相:其中X表示两种元素中的一种或两种,Zr和Hf,M表示 选自Mn,Fe,Co,Ni和Cu中的至少一种元素,a,b和c表示分别满足25 <= a <=85,5≤b≤70的原子百分比, 0

    Optical connector ferrules and method for production thereof
    3.
    发明授权
    Optical connector ferrules and method for production thereof 失效
    光连接器套圈及其制造方法

    公开(公告)号:US06450696B1

    公开(公告)日:2002-09-17

    申请号:US09515294

    申请日:2000-02-29

    IPC分类号: G02B636

    摘要: Disclosed are a sleeve for abutting, aligning, and retaining opposed optical connector ferrules and methods for the production thereof. The sleeve has a tubular body provided at three points on the inner wall surface thereof with ridges of an arcuate cross section extending from one to the other end of the tubular body in the longitudinal direction thereof and a slit formed therein in the longitudinal direction thereof. The sleeve is formed of an amorphous alloy possessing at least a glass transition region, preferably a glass transition region of not less than 30 K in temperature width. Preferably the sleeve is formed of an amorphous alloy having a composition represented by the following general formula and containing an amorphous phase in a volumetric ratio of at least 50%: XaMbAlc wherein X represents either or both of two elements, Zr and Hf, M represents at least one element selected from the group consisting of Mn, Fe, Co, Ni, and Cu, and a, b, and c represent such atomic percentages as respectively satisfy 25≦a≦85, 5≦b≦70, and 0

    摘要翻译: 公开了用于邻接,对准和保持相对的光学连接器套圈的套筒及其制造方法。 套管具有在其内壁表面上的三个点上设置有沿其纵向方向从管状体的一端延伸到另一端的弓形横截面的脊部和在其纵向方向上形成的狭缝的管状体。 该套筒是由具有至少玻璃化转变区域的非晶合金形成的,优选玻璃化转变区域的温度宽度不低于30K。 优选地,套筒由具有由以下通式表示的组成的非晶态合金形成,并且含有至少50%的体积比的非晶相:其中X表示两种元素中的一种或两种,Zr和Hf,M表示 选自Mn,Fe,Co,Ni和Cu中的至少一种元素,a,b和c表示分别满足25 <= a <=85,5≤b≤70的原子百分比, 0

    Highly hard thin film and method for production thereof
    6.
    发明授权
    Highly hard thin film and method for production thereof 失效
    高硬度薄膜及其制造方法

    公开(公告)号:US5648174A

    公开(公告)日:1997-07-15

    申请号:US420606

    申请日:1995-04-12

    摘要: A hard thin film having fine crystalline ceramic particles dispersed in a metallic matrix phase is disclosed. The production of the film is effected by first depositing a substantially amorphous film on a substrate and then heat-treating the deposited film. Deposition of the film on the substrate is carried out by using a source of evaporation having a composition represented by the general formula: Al.sub.a M.sub.b, wherein M stands for at least one element selected from the group consisting of Ti, Ta, V, Cr, Zr, Nb, Mo, Hf, W, Mn, Fe, Co, Ni, and Cu and "a" and "b" respectively stand for atomic % in the ranges of 60.ltoreq.a.ltoreq.98.5 and 1.5.ltoreq.b.ltoreq.40, providing a+b=100. Deposition is effected by a physical vapor deposition process in an atmosphere of an inert gas containing a reaction gas while controlling the feed rate of the reaction gas into a chamber in such a manner that the partial pressure of the react/on gas is kept constant or varied continuously or stepwise. By this method, there can be obtained a hard composite film having fine ceramic particles dispersed in a metallic matrix phase or a dense, hard, and composite film having a composition and structure obliquely varied from a substantially crystalline metallic phase to a crystalline ceramic phase in the direction of thickness of the film.

    摘要翻译: 公开了一种具有分散在金属基体相中的细晶体陶瓷颗粒的硬质薄膜。 通过首先在基板上沉积基本上非晶的膜然后对沉积的膜进行热处理来实现膜的制备。 通过使用具有由通式AlaMb表示的组成的蒸发源进行膜的沉积,其中M表示选自Ti,Ta,V,Cr,Zr中的至少一种元素 ,Nb,Mo,Hf,W,Mn,Fe,Co,Ni和Cu,“a”和“b”分别表示60≤a≤98.5的范围内的原子% b = 40,提供+ b = 100。 通过在包含反应气体的惰性气体的气氛中的物理气相沉积工艺进行沉积,同时将反应气体的进料速率控制在室内,使得反应/导入气体的分压保持恒定,或 连续或逐步变化。 通过该方法,可以获得具有分散在金属基体相中的细微陶瓷颗粒的硬质复合膜或致密的,硬的和复合的膜,其具有从基本上结晶的金属相到结晶陶瓷相倾斜变化的组成和结构 膜的厚度方向。

    High-strength aluminum-based alloy
    7.
    发明授权
    High-strength aluminum-based alloy 失效
    高强度铝基合金

    公开(公告)号:US5607523A

    公开(公告)日:1997-03-04

    申请号:US369818

    申请日:1995-01-09

    IPC分类号: C22C21/00 C22C45/08

    CPC分类号: C22C45/08 C22C21/00

    摘要: A high-strength aluminum-based alloy consisting of a composition represented by the general formula: Al.sub.bal Q.sub.a M.sub.b X.sub.c, wherein Q is at least one element selected from the group consisting of Mn and Cr; M is at least one element selected from the group consisting of Co, Ni, and Cu; X is at least one of rare earth elements including Y, or Misch metal (Mm); and a, b and c are, in atomic percentages, 1.ltoreq.a.ltoreq.7, 0.5.ltoreq.b.ltoreq.5, and 0

    摘要翻译: 一种高强度铝基合金,其由以下通式表示的组成:AlbalQaMbXc,其中Q是选自Mn和Cr中的至少一种元素; M是选自Co,Ni和Cu中的至少一种元素; X是包括Y或稀土金属(Mm)的稀土元素中的至少一种; 和a,b和c以原子百分比为1,其中含有准晶体的铝基合金为1 / 其结构。 准晶体可以是二十面体相(I相),十字相(D相)或类似于其的结晶相,并且该结构可以包括准晶相和由非晶相,铝和 过饱和铝固溶体或其复合(混合相)。 合金结构还可以包含由铝和其它元素形成的金属间化合物和/或由其它元素本身形成的金属间化合物。

    Process for producing amorphous alloy material
    8.
    发明授权
    Process for producing amorphous alloy material 失效
    生产非晶合金材料的方法

    公开(公告)号:US5296059A

    公开(公告)日:1994-03-22

    申请号:US943703

    申请日:1992-09-11

    摘要: A process for producing an amorphous alloy material characterized by imparting ductility to an amorphous alloy having a supercooled liquid region by giving a prescribed amount of strain at a prescribed strain rate to the alloy in the glass transition temperature region of the alloy. The amorphous alloy may be in the form of spherical or irregular-shaped powders or thin ribbons or in the form of primary consolidated shapes thereof or an amorphous alloy casting. The amount of strain and strain rate are preferably 50% or greater and 2.times.10.sup.-2 /sec or higher, respectively, and the worked amorphous alloy material is preferably allowed to cool in a furnace or spontaneously. Suitable examples of the amorphous alloy to be employed include Al-TM-Ln, Mg-TM-Ln, Zr-TM-Al and Hf-TM-Al alloys, wherein TM is a transition metal element and Ln is a rare earth metal element. The thus obtained amorphous alloy is greatly improved in the prevention of embrittlement in hot working peculiar to the alloy.

    摘要翻译: 一种非晶态合金材料的制造方法,其特征在于,在合金的玻璃化转变温度区域中,通过以规定的应变速率向合金赋予规定量的应变率,赋予具有过冷液体区域的非晶质合金的延展性。 非晶合金可以是球形或不规则形状的粉末或薄带的形式,或者是其主要固结形状或非晶态合金铸件的形式。 应变量和应变速率分别优选为50%以上且2×10 -2 /秒以上,加工后的非晶态合金材料优选在炉内自发冷却。 所使用的非晶合金的合适实例包括Al-TM-Ln,Mg-TM-Ln,Zr-TM-Al和Hf-TM-Al合金,其中TM是过渡金属元素,Ln是稀土金属元素 。 由此获得的非晶态合金在防止合金特有的热加工中脆化方面大大提高。

    High-strength aluminum alloy
    9.
    发明授权
    High-strength aluminum alloy 失效
    高强度铝合金

    公开(公告)号:US5458700A

    公开(公告)日:1995-10-17

    申请号:US235129

    申请日:1994-04-28

    IPC分类号: C22C21/00 C22C45/08

    CPC分类号: C22C45/08 C22C21/00

    摘要: A high-strength aluminum alloy consisting of an amorphous phase containing quasicrystals constituted of aluminum as the principal element, a first additive element consisting of at least one rare earth element and a second additive element consisting of at least one element other than aluminum and rare earth elements, and a crystalline phase consisting of the principal element and the first additive element and the second additive element contained in a supersaturated solid solution form, the amorphous phase containing quasicrystals being contained in a volume percentage of 60 to 90%. The contents of the additive elements preferably fall within a hatched range in the figure, still preferably within a range covered with dot-dash lines in the figure.

    摘要翻译: 由含有以铝为主要元素的准晶体的非晶相组成的高强度铝合金,由至少一种稀土元素组成的第一添加元素和由铝和稀土之外的至少一种元素组成的第二添加元素 元素和由主要元素和第一添加元素和第二添加元素组成的结晶相以包含过饱和固溶体形式,含有准晶体的非晶相以体积百分比为60至90%。 添加元素的含量优选落在图中的阴影范围内,更优选在图中用点划线覆盖的范围内。

    Magnetic material
    10.
    发明授权
    Magnetic material 失效
    磁性材料

    公开(公告)号:US5397490A

    公开(公告)日:1995-03-14

    申请号:US96275

    申请日:1993-07-26

    CPC分类号: B82Y25/00 H01F1/147 H01F1/153

    摘要: A magnetic material consisting essentially of A1 and 10 to 50 at. % of at least one capable of alloying with A1 to form quasicrystals (for example, 5 to 25 at. % of at least one member selected between Cu and Pd and 5 to 35 at. % of Mn) and up to 25 at. % of at least one element having a smaller atomic radius than those of the above elements (for example, B). The magnetic material is produced by adding, to a mixture consisting of A1 and at least one element capable of alloying with A1 to form quasicrystals and including at least one transition metal, at least one element having a smaller atomic radius than those of A1 and the above elements to dissolve the element having a smaller atomic radius in a solid solution form in a quasicrystalline phase. The thus obtained magnetic crystal is useful in various applications, such as magnetic recording heads, and a process for producing the same.