Abstract:
A gas-shielded arc welding method includes welding a steel plate having a tensile strength of 780 MPa or more while feeding a consumable electrode via a welding torch and flowing a shielding gas. The consumable electrode includes, in mass %, C: 0 to 0.20%, Si: 0 to 0.50%, Mn: 0 to 0.50%, Cr: 1.00% to 9.00%, S: 0.0020% to 0.0600%, and Ni: 0 to 0.50%. The shielding gas includes, in vol. %, at least one of CO2 and O2: 1% to 15% in total, with the remainder being Ar and unavoidable impurities. Welding is performed under the condition satisfying the relationship of 1≤{−0.05×[CO2+O2]}+[Cr]≤8.3, and [Cr] represents the content of Cr in the consumable electrode, and [CO2+O2] represents a total content of at least one of CO2 and O2 in the shielding gas.
Abstract:
A steel plate frame and a thin plate are made of different materials. A plurality of through holes are formed in a portion of the thin plate to be placed on the steel plate frame. A plurality of projections 6c are formed on a support plate, each of the projections being allowed to be inserted into a corresponding one of the through holes. An adhesive is applied to a portion of the steel plate frame on which the thin plate is placed. The thin plate is placed on the steel plate frame, and the steel plate frame and the thin plate are bonded together by the adhesive. The support plate is placed on the thin plate to insert the projections into the through holes. The projections and the steel plate frame are welded to form a plurality of welded spots.
Abstract:
A method for welding a galvanized steel sheet includes utilizing a pulse welding of repeatedly applying a pulse peak current and a base current, setting a welding speed to 100 cm/min or less, and using a shielding gas in which 1 vol % or more and 10 vol % or less of at least either one of CO2 and O2 is added to Ar. The pulse peak current has a pulse peak time being in a range of 7% or more and less than 50% of one period depending on a sheet thickness of the galvanized steel sheet.
Abstract:
An arc welding apparatus includes a lifting motor. A speed adjustment circuit controls the lifting motor such that the rising speed of the welder decreases if a current of the welding power source is smaller than a set value, or increases if the value of the current is larger than the set value. A voltage adjustment circuit controls the welding power source such that the voltage increases if the number of times that the voltage falls below a determination voltage is larger than a set number of times or if periods for which the voltage remains below the determination voltage are longer than a set time, or decreases if the number of times that the voltage falls below a determination voltage is smaller than a set number of times or if periods for which the voltage remains below the determination voltage is shorter than a set time.
Abstract:
A welding system includes a welding torch that welds a workpiece by using a wire, a suction device that sucks shielding gas, and a sucked shielding gas supply path for allowing the sucked shielding gas to flow, wherein the welding torch includes a contact chip that guides the wire, a shielding gas supply nozzle that supplies the shielding gas to a weld zone, and a suction nozzle that surrounds a periphery of the wire protruding from the contact chip, and is opened toward a tip of the wire to suck the shielding gas.
Abstract:
A solid wire is for gas-shielded arc welding, using a shielding gas, and for galvanized steel sheet welding. The solid wire comprises, to the mass of the whole of the solid wire, predetermined amount of C, Si, Mn, P, S, O, and Cr, with the balance consisting Fe and inevitable impurities. The solid wire satisfies “1.0≦(percentage by mass of Si+that by mass of Mn)/{100(that by mass of S+that by mass of O}≦4.0” and “0.50≦percentage by mass of Mn/that by mass of Si≦2.00”. The shielding gas is an Ar gas comprising 25 to 40% of CO2 gas. It is achieved to improve spatter-decreasing performance and pore-resisting performance (performance of restraining the generation of porosity defects, such as pits and blowholes).
Abstract:
There is provided a flux-cored wire containing flux within a stainless steel or mild steel outer cover for use in stainless steel welding and gas-shielded arc welding using a shielding gas. The flux-cored wire contains, based on the total mass of the flux-cored wire, predetermined amounts of C, Si, Mn, P, S, Cr, Ti, and O. The remainder are Fe and incidental impurities. The shielding gas is pure Ar gas.
Abstract:
In a tandem gas-shielded arc welding method, carbon dioxide is used as a shielding gas for a leading electrode formed by a solid wire, an argon-carbon dioxide gas mixture containing at least 60% by volume of argon gas is used as a shielding gas for a trailing electrode formed by a solid wire or a flux-cored wire, both the leading electrode and the trailing electrode have a reverse polarity, the leading electrode satisfies the relationships “5.00≦(I·V·10−8)/(Wf·πr2)≦10.00” and “(I2·10−3)/V≧4.50”, and the trailing electrode satisfies the relationships “4.00≦(I·V·10−8)/(Wf·πr2)≦7.00” and “(I2 10−3)/V≧8.00”.
Abstract:
The present invention relates to a method for joining a plated steel sheet, in which at least one of a first steel sheet and a second steel sheet is a plated steel sheet, and the first and second steel sheets overlapped with each other are subjected to an arc spot welding. The method includes press-working the first steel sheet into a desired shape and at the same time forming a linear groove on an overlapping surface with the second steel sheet of the first steel sheet, overlapping the first and second steel sheets, and setting a welding torch with the groove as a target position, and performing the arc spot welding so as to overlap the groove when viewed from a direction perpendicular to the overlapping surface.
Abstract:
In this flux-cored wire, the contents of F, Li, acid-soluble Al, Mg, S, CO2, Ba, Ca, Sr, REM, P, C which is not derived from a carbonate, Mn, Ni, and Cu are set to fall within prescribed ranges with respect to the total mass of the wire, and the blending ratio among these components is set to fall within a particular range.