摘要:
This method for producing anodic porous alumina such that an oxide coating film having a plurality of minute pores is formed at the surface of an aluminum substrate is characterized by containing: a step (a) for immersing the aluminum substrate in an electrolytic liquid resulting from mixing a plurality of acids; a step (b) for imposing a voltage on the aluminum substrate immersed in the electrolytic liquid; a step (c) for holding the aluminum substrate in the state of being immersed in the electrolytic liquid essentially without imposing a voltage on the aluminum substrate; and a step (d) for alternately repeating step (b) and step (c). By means of the present invention, it is possible using a simple device and with few steps to provide a method that easily produces anodic porous alumina such that an oxide coating film having a plurality of minute pores is formed at the surface of an aluminum substrate.
摘要:
The present invention relates to a method of manufacturing a mold having an oxide film with a plurality of pores formed on a surface of an aluminum substrate, the method including (a) a process of applying a voltage to a machined aluminum substrate and anodizing a surface of the aluminum substrate to form an oxide film; and (b) a process of removing at least a part of the oxide film formed in the process (a), wherein a voltage (Va [V]) immediately before the process (a) is terminated and a time (ta [sec]) required to reach the voltage (Va [V]) after starting the application of voltage satisfy the following Equation (i) in the process (a). 0.010
摘要:
A method for manufacturing a mold includes (a) anodizing an aluminum substrate at a voltage of 60 V to 120 V in an electrolytic solution in which two or more species of acid are mixed, and forming an oxide film having a plurality of minute holes on a surface of the aluminum substrate; and (b) removing at least a portion of the oxide film. The electrolytic solution used in (a) satisfies the relation (D1)/2
摘要:
The present invention relates to a method of manufacturing a mold having an oxide film with a plurality of pores formed on a surface of an aluminum substrate, the method including (a) a process of applying a voltage to a machined aluminum substrate and anodizing a surface of the aluminum substrate to form an oxide film; and (b) a process of removing at least a part of the oxide film formed in the process (a), wherein a voltage (Va[V]) immediately before the process (a) is terminated and a time (ta[sec]) required to reach the voltage (Va[V]) after starting the application of voltage satisfy the following Equation (i) in the process (a). 0.010
摘要:
A method for manufacturing a mold includes (a) anodizing an aluminum substrate at a voltage of 60 V to 120 V in an electrolytic solution in which two or more species of acid are mixed, and forming an oxide film having a plurality of minute holes on a surface of the aluminum substrate; and (b) removing at least a portion of the oxide film. The electrolytic solution used in (a) satisfies the relation (D1)/2
摘要:
This dispersion-type acrylic copolymer has a matrix (I) formed of an acrylic copolymer having a glass transition temperature of 50° C. or higher and a polymer unit (II) formed of an acrylic copolymer having a glass transition temperature of less than 50° C., the polymer unit (II) forms localized regions having an average diameter of 5-300 nm in the matrix (I), the matrix (I) and polymer unit (II) contain units of a crosslinking component, and the content of these units of a crosslinking component is more than 2% by mass relative to the total weight of the acrylic copolymer.
摘要:
Described is a method for producing a laminate having a micro concave-convex structural body and a film, wherein the body has, at its surface, a micro concave-convex structure having a period less than a wavelength of visible light, the water contact angle of the surface is 120° or greater, and the film contains a film substrate and a film resin layer to protect the surface. A curable resin composition is disposed as the film resin layer between a side surface of the micro concave-convex structure and the film substrate. The micro concave-convex structural body and the film substrate are bonded via the curable resin composition. The curable resin composition is cured to obtain a cured product thereof. The compressive elastic modulus of the cured product is 30 MPa or greater, and is less than that of a cured product of the material constituting the micro concave-convex structure.
摘要:
The present invention provides an active energy ray-curable resin composition comprising at least a multifunctional monomer having three or more radical polymerizable functional groups in the molecule in which the cured product of the composition exhibits anti-reflective function because of an uneven microstructure formed on the surface of the cured product, and provides a product having the uneven microstructure having high decontaminating properties such as fingerprint removal properties and high scratch resistance.
摘要:
A structural body which comprises a base and a microrelief structure layer having a microrelief structure. The microrelief structure layer is laminated on the base so as to form the surface layer of this structural body, and the microrelief structure layer has at least one physical property selected from the group consisting of (A) and (B) described below. (A) The elastic modulus at 25° C. is 50 MPa or more, and the elastic modulus at 80° C. is 30 MPa or less. (B) The tensile elongation at break at 80° C. is from 20% to 100% (inclusive).
摘要:
The present invention provides an active energy ray-curable resin composition comprising at least a multifunctional monomer having three or more radical polymerizable functional groups in the molecule in which the cured product of the composition exhibits anti-reflective function because of an uneven microstructure formed on the surface of the cured product, and provides a product having the uneven microstructure having high decontaminating properties such as fingerprint removal properties and high scratch resistance.