    摘要: The present invention provides a wholly aromatic liquid-crystalline polyester consisting of the repeating units represented by formulae (I), (II), (III) and (IV): wherein: the molar proportion of the repeating unit represented by formula (I) based on the total repeating units constituting the wholly aromatic liquid-crystalline polyester is 40-80 mol %; the molar ratio of the total amount of the repeating units represented by formulae (II) and (III) to the repeating unit represented by formula (IV) is from 90/100 to 100/90; the molar proportion of the repeating unit represented by formula (II) based on the total amount of the repeating units represented by formulae (II) and (III) is 80-99.9 mol%; and the two “—O—” attached to the benzene ring in formula (III) are positioned meta or para to each other and “Ar” in formula (IV) represents a bivalent aromatic group. The wholly aromatic liquid-crystalline polyester of the present invention exhibits excellent dielectric properties in high frequency regions as well as good mechanical properties such as impact strength.

    摘要翻译: 本发明提供由式(I),(II),(III)和(IV)表示的重复单元组成的全芳族液晶聚酯:其中:由式(I)表示的重复单元的摩尔比例 基于构成全芳香族液晶聚酯的总重复单元为40〜80摩尔%。 由式(II)和(III)表示的重复单元的总量与由式(IV)表示的重复单元的摩尔比为90/100〜100/90; 由式(II)表示的重复单元相对于式(II)和(III)表示的重复单元的总量的摩尔比例为80-99.9摩尔% 并且与式(III)中的苯环相连的两个“-O-”彼此定位为间位或对位,式(IV)中的“Ar”表示二价芳基。 本发明的全芳香族液晶聚酯在高频区域表现出优异的介电性能以及良好的机械性能如冲击强度。

    LIQUID-CRYSTALLINE POLYESTER BLEND
    3.
    发明申请
    LIQUID-CRYSTALLINE POLYESTER BLEND 有权
    液晶聚合物混合物

    公开(公告)号:US20090111926A1

    公开(公告)日:2009-04-30

    申请号:US12260536

    申请日:2008-10-29

    IPC分类号: C08K3/38 C08L71/00 C08K3/40

    摘要: The present invention provides a liquid-crystalline polyester blend, which is obtained by combining a liquid-crystalline polyester (A) and a liquid-crystalline polyester (B) such that the ratio by weight of (A)/(B) is 99/1 to 80/20: liquid-crystalline polyester (A) which consists of aromatic oxycarbonyl repeating units, aromatic dioxy repeating units and aromatic dicarbonyl repeating units, and contains 40-80 mol % of the repeating unit represented by formula (I) based on the total repeating units constituting the liquid-crystalline polyester (A); liquid-crystalline polyester (B) which comprises repeating units represented by formulae (I) and (II), wherein the molar proportion of the total amount of the repeating units represented by formulae (I) and (II) based on the total amount of the repeating units constituting the liquid-crystalline polyester (B) is greater than or equal to 90 mol % and the molar proportion of the repeating units represented by formulae (I) to (II) is from 10/90 to 50/50. The liquid-crystalline polyester blend of the present invention exhibits excellent dielectric properties in high frequency regions as well as good impact strength and molding processability.

    摘要翻译: 本发明提供一种液晶聚酯共混物,其通过将液晶聚酯(A)和液晶聚酯(B)组合使得(A)/(B)的重量比为99 / 1〜80/20:由芳香族氧羰基重复单元,芳香族二氧基重复单元和芳香族二羰基重复单元构成的液晶性聚酯(A),并且含有40〜80摩尔%的式(I)所示的重复单元,基于 构成液晶聚酯(A)的总重复单元; 含有由式(I)和(II)表示的重复单元的液晶聚酯(B),其中由式(I)和(II)表示的重复单元的总量的摩尔比例基于式 构成液晶聚酯(B)的重复单元大于或等于90摩尔%,由式(I)至(II)表示的重复单元的摩尔比为10/90〜50/50。 本发明的液晶聚酯共混物在高频区域表现出优异的介电性能以及良好的冲击强度和成型加工性能。

    Liquid-crystal polyester resin
    5.
    发明申请
    Liquid-crystal polyester resin 审中-公开
    液晶聚酯树脂

    公开(公告)号:US20070010647A1

    公开(公告)日:2007-01-11

    申请号:US10574472

    申请日:2004-09-29

    IPC分类号: C08G63/02

    CPC分类号: C08G63/605

    摘要: The present invention provides a liquid-crystalline polyester resin, essentially consisting of the repeating units represented by formulae [I]-[IV]: wherein p, q, r and s satisfy the following formulae: 0.4≦p/q≦2.0, 2≦r≦15, 2≦s≦15, and p+q+r+s=100, provided that the liquid-crystalline polyester resin has a melting point of 190-250° C. determined by differential scanning calorimetry. The liquid-crystalline polyester resin of the present invention exhibits a good molding processability at low temperatures and excellent mechanical properties.

    摘要翻译: 本发明提供了一种液晶聚酯树脂,其基本上由式[I] - [IV]表示的重复单元组成:其中p,q,r和s满足下式:0.4 <= p / q <= 2.0 ,如果液晶聚酯树脂的熔点为190-250℃,则通过差示确定,2 <= r <= 15,2 <= s <= 15和p + q + r + s = 扫描量热法。 本发明的液晶聚酯树脂在低温下表现出良好的模塑加工性能和优异的机械性能。

    Liquid-crystalline polyester blend
    6.
    发明授权
    Liquid-crystalline polyester blend 有权
    液晶聚酯共混物

    公开(公告)号:US07842760B2

    公开(公告)日:2010-11-30

    申请号:US12260536

    申请日:2008-10-29

    摘要: The present invention provides a liquid-crystalline polyester blend, which is obtained by combining a liquid-crystalline polyester (A) and a liquid-crystalline polyester (B) such that the ratio by weight of (A)/(B) is 99/1 to 80/20: liquid-crystalline polyester (A) which consists of aromatic oxycarbonyl repeating units, aromatic dioxy repeating units and aromatic dicarbonyl repeating units, and contains 40-80 mol % of the repeating unit represented by formula (I) based on the total repeating units constituting the liquid-crystalline polyester (A); liquid-crystalline polyester (B) which comprises repeating units represented by formulae (I) and (II), wherein the molar proportion of the total amount of the repeating units represented by formulae (I) and (II) based on the total amount of the repeating units constituting the liquid-crystalline polyester (B) is greater than or equal to 90 mol % and the molar proportion of the repeating units represented by formulae (I) to (II) is from 10/90 to 50/50. The liquid-crystalline polyester blend of the present invention exhibits excellent dielectric properties in high frequency regions as well as good impact strength and molding processability.

    摘要翻译: 本发明提供一种液晶聚酯共混物,其通过将液晶聚酯(A)和液晶聚酯(B)组合使得(A)/(B)的重量比为99 / 1〜80/20:由芳香族氧羰基重复单元,芳香族二氧基重复单元和芳香族二羰基重复单元构成的液晶性聚酯(A),并且含有40〜80摩尔%的式(I)所示的重复单元,基于 构成液晶聚酯(A)的总重复单元; 含有由式(I)和(II)表示的重复单元的液晶聚酯(B),其中由式(I)和(II)表示的重复单元的总量的摩尔比例基于式 构成液晶聚酯(B)的重复单元大于或等于90摩尔%,由式(I)至(II)表示的重复单元的摩尔比为10/90〜50/50。 本发明的液晶聚酯共混物在高频区域表现出优异的介电性能以及良好的冲击强度和成型加工性能。

    WHOLLY AROMATIC LIQUID-CRYSTALLINE POLYESTER
    7.
    发明申请
    WHOLLY AROMATIC LIQUID-CRYSTALLINE POLYESTER 有权
    纯粹的芳香液晶聚酯

    公开(公告)号:US20090111964A1

    公开(公告)日:2009-04-30

    申请号:US12260428

    申请日:2008-10-29

    IPC分类号: C08G8/02

    摘要: The present invention provides a wholly aromatic liquid-crystalline polyester consisting of the repeating units represented by formulae (I), (II), (III) and (IV): wherein: the molar proportion of the repeating unit represented by formula (I) based on the total repeating units constituting the wholly aromatic liquid-crystalline polyester is 40-80 mol %; the molar ratio of the total amount of the repeating units represented by formulae (II) and (III) to the repeating unit represented by formula (IV) is from 90/100 to 100/90; the molar proportion of the repeating unit represented by formula (II) based on the total amount of the repeating units represented by formulae (II) and (III) is 80-99.9 mol %; and the two “—O—” attached to the benzene ring in formula (III) are positioned meta or para to each other and “Ar” in formula (IV) represents a bivalent aromatic group. The wholly aromatic liquid-crystalline polyester of the present invention exhibits excellent dielectric properties in high frequency regions as well as good mechanical properties such as impact strength.

    摘要翻译: 本发明提供由式(I),(II),(III)和(IV)表示的重复单元组成的全芳族液晶聚酯:其中:由式(I)表示的重复单元的摩尔比例 基于构成全芳香族液晶聚酯的总重复单元为40〜80摩尔%。 由式(II)和(III)表示的重复单元的总量与由式(IV)表示的重复单元的摩尔比为90/100〜100/90; 由式(II)表示的重复单元相对于式(II)和(III)表示的重复单元的总量的摩尔比例为80-99.9摩尔% 并且与式(III)中的苯环相连的两个“-O-”彼此定位为间位或对位,式(IV)中的“Ar”表示二价芳基。 本发明的全芳香族液晶聚酯在高频区域表现出优异的介电性能以及良好的机械性能如冲击强度。

    Method for producing pellets of liquid-crystalline polymer or pellets of liquid-crystalline polymer composition
    10.
    发明申请
    Method for producing pellets of liquid-crystalline polymer or pellets of liquid-crystalline polymer composition 审中-公开
    制备液晶聚合物或液晶聚合物组合物颗粒的颗粒的方法

    公开(公告)号:US20060284333A1

    公开(公告)日:2006-12-21

    申请号:US11444339

    申请日:2006-06-01

    IPC分类号: B29B9/06

    摘要: The present invention provides a method for producing pellets or pellets of a liquid-crystalline polymer composition with a reduced amount of anionic impurities such as chloride, nitrate and sulfate ions. The present invention provides a method for producing pellets of a liquid-crystalline polymer, which comprises: providing a molten state liquid-crystalline polymer in a polycondensation reaction vessel, pulling out the liquid-crystalline polymer from a valve at the bottom of the reaction vessel through a die to give a strand of the polymer, cooling the strand on a water cooling conveyor positioned below the reaction vessel, and cutting the strand to give the pellets, wherein the cooling water for the strand is pure water whose electrical conductance is not more than 10 μS/cm.