Abstract:
It is an object of the invention to provide a pressure-sensitive adhesive capable of forming a pressure-sensitive adhesive layer having high resistance to sebum and high resistance to moisture-induced clouding and also having low dielectric constant. The invention relates to a pressure-sensitive adhesive comprising a (meth)acryl-based polymer obtained by polymerization of a monomer component containing 65 to 88 parts by weight of an alkyl (meth)acrylate having an alkyl group of 8 to 22 carbon atoms and 12 to 35 parts by weight of an alkyl (meth)acrylate having a secondary hydroxyl group based on 100 parts by weight of the total amount of the alkyl (meth)acrylate having an alkyl group of 8 to 22 carbon atoms and the alkyl (meth)acrylate having a secondary hydroxyl group.
Abstract:
A pressure-sensitive adhesive composition includes: 100 parts by mass of a polymer (A) having a glass transition temperature lower than 0° C.; 0.05 parts by mass to 3 parts by mass of a (meth)acrylic polymer (B) having a weight average molecular weight (MwB) of 1000≦MwB
Abstract:
A pressure-sensitive adhesive of the invention include a (meth)acryl-based polymer obtained by polymerization of a monomer component including 30 to 99.5% by weight of an alkyl (meth)acrylate having an alkyl group of 10 to 18 carbon atoms at an ester end and 0.5 to 50% by weight of a cyclic nitrogen-containing monomer. The pressure-sensitive adhesive has a satisfactory level of adhesive performance and can form a pressure-sensitive adhesive layer with a lower dielectric constant and reliable moisture resistance.
Abstract:
An acrylic pressure-sensitive adhesive composition contains 100 parts by mass of an acrylic polymer (A), 1 to 70 parts by mass of a (meth)acrylic polymer (B) having a weight average molecular weight (Mw) of 1000≦Mw
Abstract:
The invention relates to a functionalized laminated optical element comprising: —An optical base element; —A functional film structure consisting of a single layer or a multilayer structure; —A layer of a pressure-sensitive adhesive of optical quality, placed between one surface of the optical base element and the functional film structure so as to permanently retain said functional film structure on the surface of the optical base element. Said functionalized laminated optical element maintains its integrity after typical processing of an optical article which includes wheel edging. More particularly the invention relates to the use of a specific adhesive system for improving the wheel edging resistance of functionalized laminated optical element. The functional laminated optical may be an ophthalmic lens.
Abstract:
A pressure-sensitive adhesive sheet has a substrate and a pressure-sensitive adhesive layer laminated on at least one side of the substrate. The pressure-sensitive adhesive layer contains a (meth)acrylic polymer having a weight average molecular weight of 10000 or more but less than 50000. Pressure-sensitive adhesive force, occurring after 30 minutes since the pressure-sensitive adhesive layer was attached to an ABS plate, is 1.0 [N/20 mm] or less, pressure-sensitive adhesive force, occurring after 24 hours since the pressure-sensitive adhesive layer was attached to an ABS plate, is 2.5 [N/20 mm] or less, and pressure-sensitive adhesive force, occurring after 30 minutes at 23° C. since the pressure-sensitive adhesive layer was attached to an ABS plate and then heated at 80° C. for 5 minutes, is 6.5 [N/20 mm] or more.
Abstract:
A pressure-sensitive adhesive composition according to an embodiment includes: 100 parts by mass of a polymer (A) having a glass transition temperature lower than 0° C.; and 0.1 to 20 parts by mass of a polymer (B) that contains, as monomer units, both a monomer having a functional group equivalent (Fge) of 1000 g/mol≦Fge
Abstract:
A pressure-sensitive adhesive composition includes: 100 parts by mass of a polymer (A) (Tg:lower than 0° C.); 0.05 to 3 parts by mass of a (meth)acrylic polymer (B) (MWB:1000≦MWB
Abstract:
An acrylic pressure-sensitive adhesive composition contains: an acrylic polymer (A); and a (meth)acrylic polymer (B) that includes, as a monomer unit, a (meth)acrylic monomer having a tricyclic or higher alicyclic structure and that has a weight average molecular weight of 1000 or more and less than 30000.
Abstract:
Provided is a PSA composition for forming a PSA comprising a (meth)acrylic polymer, comprising, as monomeric components constituting the (meth)acrylic polymer: (A) a C2-18 alkyl (meth)acrylate, (B) an alicyclic monomer, and (C) a monomer having at least either a hydroxyl group or a carboxyl group. The average number of carbons of alkyl group in the (A) is 8 or less. The monomeric components comprise the (C) at 3% by weight or greater while the weights Wb and Wc of the (B) and (C) satisfy a relationship 0.8≦Wb/Wc.