摘要:
The present invention provides a rubber composition that improves processability and fuel efficiency without decreasing mechanical strength and abrasion resistance, which are excellent properties of natural rubber, and a pneumatic tire using the rubber composition for a tire tread. Specifically, the present invention provides a rubber composition for a tire tread comprising 5 to 150 parts by weight of silica having nitrogen-adsorbing specific surface area of 100 to 300 m2/g and/or 5 to 150 parts by weight of carbon black having nitrogen-adsorbing specific surface area of at least 70 m2/g and dibutyl phthalate oil absorption of at least 70 ml/100 g, based on 100 parts of a rubber component containing 5 to 100% by weight of a deproteinized natural rubber having a weight average molecular weight of 1,400,000 and nitrogen content of at most 0.1% by weight, and a pneumatic tire comprising the rubber composition for a tire tread.
摘要:
The present invention provides a rubber composition that improves processability and fuel efficiency without decreasing mechanical strength and abrasion resistance, which are excellent properties of natural rubber, and a pneumatic tire using the rubber composition for a tire tread. Specifically, the present invention provides a rubber composition for a tire tread comprising 5 to 150 parts by weight of silica having nitrogen-adsorbing specific surface area of 100 to 300 m2/g and/or 5 to 150 parts by weight of carbon black having nitrogen-adsorbing specific surface area of at least 70 m2/g and dibutyl phthalate oil absorption of at least 70 ml/100 g, based on 100 parts of a rubber component containing 5 to 100% by weight of a deproteinized natural rubber having a weight average molecular weight of 1,400,000 and nitrogen content of at most 0.1% by weight, and a pneumatic tire comprising the rubber composition for a tire tread.
摘要:
The present invention provides a tubeless tire in which air permeability is significantly decreased. Specifically, the present invention relates to a tubeless tire wherein an air chamber is formed between the inner face of a tire body and a rim, by mounting the tire body to the periphery of the rim, and a gas barrier layer, comprising an inorganic layered compound having a particle size of at most 5 μm and an aspect ratio of 50 to 5000 and a resin, is formed on the inner face of the tire body.
摘要:
The present invention provides a tubeless tire in which air permeability is significantly decreased. Specifically, the present invention relates to a tubeless tire wherein an air chamber is formed between the inner face of a tire body and a rim, by mounting the tire body to the periphery of the rim, and a gas barrier layer, comprising an inorganic layered compound having a particle size of at most 5 μm and an aspect ratio of 50 to 5000 and a resin, is formed on the inner face of the tire body.
摘要:
The present invention provides a rubber composition, in which abrasion resistance and gripping performance are improved in a balanced manner and bleeding of the components is inhibited, and a tire using the composition. Specifically, the present invention provides a rubber composition comprising (B) 10 to 200 parts by weight of a low molecular weight aromatic vinyl-conjugated diene copolymer having weight average molecular weight of 1.0×103 to 1.0×105 and aromatic vinyl content of 10 to 75% by weight, wherein the hydrogenation ratio of double bonds in the conjugated diene part is 20 to 60%, based on (A) 100 parts by weight of a rubber component containing at least 60% by weight of a styrene-butadiene copolymer having weight average molecular weight of 5.0×105 to 2.5×106 and styrene content of 20 to 60% by weight, wherein the amount of vinyl bonds in the butadiene part is 20 to 70%; which satisfies the following equation 5% by weight
摘要:
The present invention provides a rubber composition for a tire, in which gripping performance and abrasion resistance are improved in a balanced manner, and a tire using the same. Specifically, the present invention provides a rubber composition for a tire comprising 5 to 200 parts by weight of a low molecular weight aromatic vinyl-conjugated diene copolymer having a specific aromatic vinyl content and weight average molecular weight, based on 100 parts by weight of a rubber component containing aromatic vinyl-conjugated diene copolymer, a rubber composition for a tire comprising 5 to 200 parts by weight of an olefin-conjugated diene-aromatic vinyl copolymer based on 100 parts by weight of a diene rubber component, and a tire using the same.
摘要:
The present invention provides a rubber composition for a tire, in which gripping performance and abrasion resistance are improved in a balanced manner, and a tire using the same. Specifically, the present invention provides a rubber composition for a tire comprising 5 to 200 parts by weight of a low molecular weight aromatic vinyl-conjugated diene copolymer having a specific aromatic vinyl content and weight average molecular weight, based on 100 parts by weight of a rubber component containing aromatic vinyl-conjugated diene copolymer, a rubber composition for a tire comprising 5 to 200 parts by weight of an olefin-conjugated diene-aromatic vinyl copolymer based on 100 parts by weight of a diene rubber component, and a tire using the same.
摘要:
The present invention provides a rubber composition, in which abrasion resistance and gripping performance are improved in a balanced manner and bleeding of the components is inhibited, and a tire using the composition. Specifically, the present invention provides a rubber composition comprising (B) 10 to 200 parts by weight of a low molecular weight aromatic vinyl-conjugated diene copolymer having weight average molecular weight of 1.0×103 to 1.0×105 and aromatic vinyl content of 10 to 75% by weight, wherein the hydrogenation ratio of double bonds in the conjugated diene part is 20 to 60%, based on (A) 100 parts by weight of a rubber component containing at least 60% by weight of a styrene-butadiene copolymer having weight average molecular weight of 5.0×105 to 2.5×106 and styrene content of 20 to 60% by weight, wherein the amount of vinyl bonds in the butadiene part is 20 to 70%; which satisfies the following equation 5% by weight
摘要:
The present invention provides a rubber composition for a tire capable of improving gripping performance of a tire and a tire using the rubber composition. More specifically, the present invention relates to a rubber composition for a tire tread comprising 1 to 150 parts by weight of a piezoelectric material, based on 100 parts by weight of a natural rubber and/or a diene synthetic rubber and a tire using the rubber composition for a tire tread. The average particle size of the piezoelectric material is preferably 0.01 to 50 μm.
摘要:
A rubber waste disposal apparatus processing rubber waste such as an old tire efficiently includes a casing, a rubber waste deformation unit provided in the casing to subject rubber waste to deformation, and an ozone-containing gas supply unit supplying ozone-containing gas into the casing. The rubber waste deformation unit includes a pair of cylindrical rollers having a plurality of protrusions projecting outwards, capable of sandwiching rubber waste at the gap therebetween, and a distance setting unit that can set the distance of the gap between the cylindrical rollers.