摘要:
According to one aspect of the invention, a method for in situ repair of a turbine part is provided. The method includes the steps of accessing the turbine part while assembled to other turbine components, wherein the turbine part includes a region with a structural flaw near a hole in the turbine part, and wherein the hole is configured to flow a cooling fluid. The method also includes welding the structural flaw without performing a heat treatment of the turbine part, wherein welding the structural flaw includes laser welding that maintains a structure of the region.
摘要:
A method of weld repairing an air-cooled aft frame of a transition piece of a gas turbine engine. The transition piece has an interior surface coated with a ceramic coating. The aft frame has a surface with cooling holes therein and from which cracks have propagated. The method includes removing the transition piece from the engine and, without removing the ceramic coating or the aft frame from the transition piece, weld repairing the cracks by performing a laser beam welding technique that deposits a filler material on the surface but does not close the cooling holes in the surface. The surface of the aft frame can be machined to remove excess filler material prior to re-installing the transition piece in a gas turbine engine.
摘要:
According to one aspect of the invention, a method for in situ repair of a turbine part is provided. The method includes the steps of accessing the turbine part while assembled to other turbine components, wherein the turbine part comprises a region with a structural flaw near a hole in the turbine part, wherein the hole is configured to flow a cooling fluid and welding the structural flaw without performing a heat treatment of the turbine part, wherein welding the structural flaw comprises laser welding that maintains a structure of the region.
摘要:
A process for modifying or repairing a metallic component, such as a combustion cap effusion plate for a gas turbine, is disclosed. The method includes generating a notch or groove in the metallic component and depositing a filler material in the notch or groove. A pulsed laser is applied to the filler material. The pulsed laser has a power, frequency, and pulse width sufficient to apply heat to the metallic component and to the filler material to make at least a portion of the metallic component and the filler material melt in order to weld the filler material to the metallic component and repair or modify the metallic component. Various operating parameters of the pulsed laser can be configured to reduce undesirable heating affects.
摘要:
Disclosed is a projection welding method including providing a first metal substrate, a second metal substrate, and a projection material of separate construction from the first metal substrate and the second metal substrate, disposing the metal projection material between the first metal substrate and the second metal substrate, applying a current and pressure to at least one of the first metal substrate and the second metal substrate, melting the metal projection material via the application of the current and pressure, creating a weld between the first metal substrate and the second metal substrate via the melting, and fixedly associating the first metal substrate and the second metal substrate via the weld.
摘要:
An adaptive control hybrid welding system including hybrid welding apparatus, control system connected to hybrid welding apparatus, and seam tracker connected to control system is provided. Hybrid welding apparatus includes a laser and an electric arc welder. Laser and electric arc welder each have adjustable welding parameters. Control system modifies welding parameters of laser and electric arc welder, and spacing between laser beam and arc of welder. Seam tracker is operable to measure seam property of adjacent workpieces prior to welding. Seam tracker is operable to send signals to control system in response to the measured seam property. Control system modifies welding parameters based on signal from seam tracker and adaptive control hybrid welding apparatus joins adjacent workpieces having variable gap sizes of up to 2.5 mm with full penetration welds. Also provided is a method of controlling the adaptive control hybrid welding system.
摘要:
A process of welding an article and a welded turbine blade are disclosed. The process includes fusion welding over a primary symmetry line determined from a center of gravity on a first side of the article or blade and fusion welding over the primary symmetry line determined from the center of gravity on a second side of the article or blade. The fusion treating includes multiple fusion treatments.
摘要:
A component and a method of processing a component are disclosed. The method includes providing a base metal having a feature, removing the feature to form a processed region, applying a first layer to the processed region, and applying a second layer to the first layer. The base metal, the first layer, and the second layer each have predetermined thermal expansion coefficients, yield strengths, and elongations. The processed component includes the first layer applied to a processed region of the base metal and a second layer applied to the first layer.
摘要:
A method of fabricating a component and a fabricated component are disclosed. The method includes depositing a material to a component and manipulating the material to form a boundary region and a filler region for desired properties. The component includes the boundary region and the filler region, thereby having the desired properties.
摘要:
According to one aspect of the invention, a method for assembling a turbine includes placing a middle layer between a first and second outer member, wherein the middle layer includes a non-continuous layer of material and the first and second outer members each include a member of continuous material and welding a primary joint between the middle layer, first outer member and second outer member, the primary joint extending through the first outer member, the middle layer and at least a portion of the second outer member. The method also includes welding a secondary joint between the middle layer and first outer member, the secondary joint extending through the first outer member and at least a portion of the middle layer.