公开(公告)号:US08366980B2
公开(公告)日:2013-02-05
申请号:US12668950
申请日:2008-07-30
摘要: It is intended to provide a method of producing a hollow construct, which may be in various shapes such as a fiber or a film as well as in various sizes and has chemical resistance, made of a fluorinated hydrocarbon polymer, a fluorinated carbon polymer or a polymer carrying a nitrogen-containing group, a silicon-containing group, an oxygen-containing group, a phosphorus-containing group or a sulfur-containing group having been introduced into the above-described polymer; and a hollow construct obtained by this method. The method of producing a hollow construct as described above is characterized by comprising the fluorination step wherein a construct made of a hydrocarbon polymer or a polymer carrying a nitrogen-containing group, a silicon-containing group, an oxygen-containing group, a phosphorus-containing group or a sulfur-containing group having been introduced into the above-described polymer is brought into contact with a treating gas containing fluorine under definite conditions and thus the treating gas is allowed to penetrate from the outer surface of the construct toward the inside thereof to thereby fluorinate the construct excluding the core part, and the removal step wherein the core part having been not fluorinated as described above is removed.
摘要翻译: 本发明提供一种中空构造体的制造方法,该中空构造体可以是各种形状,例如纤维或膜,以及各种尺寸,并且具有耐化学性,由氟化烃聚合物,氟化碳聚合物或 携带含氮基团的聚合物,含有导入到上述聚合物中的含氮基团,含氧基团,含磷基团或含硫基团; 和通过该方法获得的中空构造。 如上所述的制造中空构造体的方法的特征在于包括氟化步骤,其中由烃聚合物或携带含氮基团的聚合物,含硅基团,含氧基团, 导入上述聚合物的含氟基团或含硫基团在一定条件下与含氟处理气体接触,从而允许处理气体从构造体的外表面向其内部渗透 除去核心部分以外的构造物氟化,除去上述未被氟化的芯部的除去工序。
-
公开(公告)号:US20100196645A1
公开(公告)日:2010-08-05
申请号:US12668950
申请日:2008-07-30
摘要: It is intended to provide a method of producing a hollow construct, which may be in various shapes such as a fiber or a film as well as in various sizes and has chemical resistance, made of a fluorinated hydrocarbon polymer, a fluorinated carbon polymer or a polymer carrying a nitrogen-containing group, a silicon-containing group, an oxygen-containing group, a phosphorus-containing group or a sulfur-containing group having been introduced into the above-described polymer; and a hollow construct obtained by this method. The method of producing a hollow construct as described above is characterized by comprising the fluorination step wherein a construct made of a hydrocarbon polymer or a polymer carrying a nitrogen-containing group, a silicon-containing group, an oxygen-containing group, a phosphorus-containing group or a sulfur-containing group having been introduced into the above-described polymer is brought into contact with a treating gas containing fluorine under definite conditions and thus the treating gas is allowed to penetrate from the outer surface of the construct toward the inside thereof to thereby fluorinate the construct excluding the core part, and the removal step wherein the core part having been not fluorinated as described above is removed.
摘要翻译: 本发明提供一种中空构造体的制造方法,该中空构造体可以是各种形状,例如纤维或膜,以及各种尺寸,并且具有耐化学性,由氟化烃聚合物,氟化碳聚合物或 携带含氮基团的聚合物,含有导入到上述聚合物中的含氮基团,含氧基团,含磷基团或含硫基团; 和通过该方法获得的中空构造。 如上所述的制造中空构造体的方法的特征在于包括氟化步骤,其中由烃聚合物或携带含氮基团的聚合物,含硅基团,含氧基团, 导入上述聚合物的含氟基团或含硫基团在一定条件下与含氟处理气体接触,从而允许处理气体从构造体的外表面向其内部渗透 除去核心部分以外的构造物氟化,除去上述未被氟化的芯部的除去工序。
-
公开(公告)号:US20120070669A1
公开(公告)日:2012-03-22
申请号:US13322877
申请日:2010-06-02
CPC分类号: B29C66/026 , B29C65/48 , B29C65/482 , B29C65/4825 , B29C65/4835 , B29C65/484 , B29C66/1122 , B29C66/45 , B29C66/71 , B29C66/72321 , B29C66/72341 , B29C66/73161 , B29K2023/00 , B29K2023/083 , B29K2027/12 , B29K2033/12 , B29K2067/00 , B29K2067/006 , B29K2069/00 , B29K2079/08 , B32B7/10 , B32B27/16 , B32B27/304 , B32B27/306 , B32B27/308 , B32B27/322 , B32B38/0008 , B32B2270/00 , B32B2457/12 , C09J5/02 , C09J2203/322 , C09J2400/226 , C09J2400/228 , C09J2431/006 , H01L31/048 , H01L31/049 , Y02E10/50 , Y10T428/31507 , Y10T428/3154 , Y10T428/31544 , Y10T428/31721 , Y10T428/31786 , Y10T428/31797 , Y10T428/31928 , B29K2027/16 , B29K2067/003 , B29K2027/14
摘要: An object of the invention is to provide a method for producing a laminated film comprising at least two resin films bonded together, which is capable of increasing the adhesiveness of the bonding surface and forming a laminated film with high reliability. The method for producing a laminated film according to the invention comprising at least two resin films laminated together, which comprises: a fluorination treatment step comprising bringing a fluorine and oxygen atoms-containing treatment gas into contact with at least a partial region of the surface of at least one of the two resin films to increase the adhesiveness of the region; and a bonding step comprising bonding the two resin films together using, as a bonding surface, the surface that has been brought into contact with the treatment gas.
摘要翻译: 本发明的目的是提供一种层压膜的制造方法,其包括至少两个粘合在一起的树脂膜,其能够提高接合表面的粘合性并且可靠地形成层压膜。 根据本发明的层压膜的制造方法包括至少两层层叠在一起的树脂膜,其包括:氟化处理步骤,包括使含氟和含氧原子的处理气体与至少部分区域的 两种树脂膜中的至少一种,以增加该区域的粘附性; 以及接合步骤,包括使用已经与处理气体接触的表面作为接合表面将两个树脂膜粘合在一起。
-
公开(公告)号:US09352511B2
公开(公告)日:2016-05-31
申请号:US13322877
申请日:2010-06-02
IPC分类号: B32B37/00 , B29C65/00 , B32B38/00 , B32B7/10 , B32B27/16 , B32B27/30 , B32B27/32 , C09J5/02 , H01L31/048 , B29K23/00 , B29K27/12 , B29K33/00 , B29K67/00 , B29K69/00 , B29K79/00 , B29C65/48
CPC分类号: B29C66/026 , B29C65/48 , B29C65/482 , B29C65/4825 , B29C65/4835 , B29C65/484 , B29C66/1122 , B29C66/45 , B29C66/71 , B29C66/72321 , B29C66/72341 , B29C66/73161 , B29K2023/00 , B29K2023/083 , B29K2027/12 , B29K2033/12 , B29K2067/00 , B29K2067/006 , B29K2069/00 , B29K2079/08 , B32B7/10 , B32B27/16 , B32B27/304 , B32B27/306 , B32B27/308 , B32B27/322 , B32B38/0008 , B32B2270/00 , B32B2457/12 , C09J5/02 , C09J2203/322 , C09J2400/226 , C09J2400/228 , C09J2431/006 , H01L31/048 , H01L31/049 , Y02E10/50 , Y10T428/31507 , Y10T428/3154 , Y10T428/31544 , Y10T428/31721 , Y10T428/31786 , Y10T428/31797 , Y10T428/31928 , B29K2027/16 , B29K2067/003 , B29K2027/14
摘要: An object of the invention is to provide a method for producing a laminated film comprising at least two resin films bonded together, which is capable of increasing the adhesiveness of the bonding surface and forming a laminated film with high reliability. The method for producing a laminated film according to the invention comprising at least two resin films laminated together, which comprises: a fluorination treatment step comprising bringing a fluorine and oxygen atoms-containing treatment gas into contact with at least a partial region of the surface of at least one of the two resin films to increase the adhesiveness of the region; and a bonding step comprising bonding the two resin films together using, as a bonding surface, the surface that has been brought into contact with the treatment gas.
摘要翻译: 本发明的目的是提供一种层压膜的制造方法,其包括至少两个粘合在一起的树脂膜,其能够提高接合表面的粘合性并且可靠地形成层压膜。 根据本发明的层压膜的制造方法包括至少两层层叠在一起的树脂膜,其包括:氟化处理步骤,包括使含氟和含氧原子的处理气体与至少部分区域的 两种树脂膜中的至少一种,以增加该区域的粘附性; 以及接合步骤,包括使用已经与处理气体接触的表面作为接合表面将两个树脂膜粘合在一起。
-
公开(公告)号:US11548993B2
公开(公告)日:2023-01-10
申请号:US12992961
申请日:2009-06-18
申请人: Jun Takano , Terunori Yamaguchi
发明人: Jun Takano , Terunori Yamaguchi
IPC分类号: C08J7/12 , H01L31/049 , H01M14/00
摘要: A simple short-time method for modifying a fluorine resin film so that hydrophilicity is not likely to deteriorate over time. The method for modifying a fluorine resin film is characterized in that the surface of the fluorine resin film is provided with hydrophilicity by bringing the fluorine resin film into contact with a process gas, which contains gas containing fluorine atoms and at least one of gas containing oxygen atoms or inert gas.
-
公开(公告)号:US20110086230A1
公开(公告)日:2011-04-14
申请号:US12992961
申请日:2009-06-18
申请人: Jun Takano , Terunori Yamaguchi
发明人: Jun Takano , Terunori Yamaguchi
CPC分类号: C08J7/12 , C08J2327/12 , H01L31/049 , H01M14/005 , Y02E10/50 , Y10T428/3154
摘要: A simple short-time method for modifying a fluorine resin film so that hydrophilicity is not likely to deteriorate over time. The method for modifying a fluorine resin film is characterized in that the surface of the fluorine resin film is provided with hydrophilicity by bringing the fluorine resin film into contact with a process gas, which contains gas containing fluorine atoms and at least one of gas containing oxygen atoms or inert gas.
摘要翻译: 用于改性氟树脂膜的简单的短时间方法,使得亲水性不可能随时间劣化。 氟树脂膜的改性方法的特征在于,通过使氟树脂膜与含有含有氟原子的气体和含氧气体中的至少一种的处理气体接触,使氟树脂膜的表面具有亲水性 原子或惰性气体。
-
-
-
-
-