    摘要: In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of surfaces that are curved or inclined with respect to the vertical, having high layer thicknesses which satisfy high requirements on the layer homogeneity, the invention proposes that the slip contain the following components in a dispersion liquid: splintery, amorphous SiO2 granules having a gain size distribution having a D50 value in the range of 3 μm to 30 μm and having a proportion by weight of at least 10% by weight, based on the total solids content; spherical, amorphous SiO2 particles having a particle size distribution having a D50 value in the range of 1 μm to 50 μm and having a proportion by weight of at least 30% by weight, based on the total solids content; SiO2 nano particles having particle sizes of less than 100 nm and having a proportion by weight between 0.2% and 10% by weight, based on the total solids content; and a non-ionic, alkali-free surfactant having a proportion in the range of 0.005 to 0.5%, based on the volume of the dispersion liquid.

    摘要翻译: 在已知的方法中,通过喷涂在SiO 2滑移上将SiO2滑移层施加到碱性石英玻璃体上,将滑移层干燥并烧结以形成含SiO 2的功能层。 为了允许可再生产的功能性石英玻璃层,即使在相对于垂直方向弯曲或倾斜的表面的情况下,具有满足对层均匀性的高要求的高层厚度,本发明提出了滑动 在分散液中含有以下组分:分散体,具有D50值在3μm至30μm范围内并且按重量计至少10重量%的增益尺寸分布的无定形SiO 2颗粒,基于总计 固体含量; 基于总固体含量,具有D50值在1μm至50μm范围内并具有至少30重量%的重量比的粒度分布的球形无定形SiO 2颗粒; 基于总固体含量,粒径小于100nm并且重量比为0.2%至10%的SiO 2纳米颗粒; 和非离子型无碱性表面活性剂,其比例基于分散液体积的0.005〜0.5%。

    Method for producing a coated quartz glass component
    2.
    发明授权
    Method for producing a coated quartz glass component 有权
    涂覆石英玻璃部件的制造方法

    公开(公告)号:US08920878B2

    公开(公告)日:2014-12-30

    申请号:US13501137

    申请日:2010-09-01

    IPC分类号: B05D3/02 C03C17/02

    CPC分类号: C03C17/02 C03C2218/11

    摘要: In a known method, a SiO2 slip layer is applied to a basic quartz glass body by means of spraying on an SiO2 slip, the slip layer is dried and sintered to form an SiO2-containing functional layer. In order to permit the reproducible production of a functional quartz glass layer, even in the case of surfaces that are curved or inclined with respect to the vertical, having high layer thicknesses which satisfy high requirements on the layer homogeneity, the invention proposes that the slip contain the following components in a dispersion liquid: splintery, amorphous SiO2 granules having a gain size distribution having a D50 value in the range of 3 μm to 30 μm and having a proportion by weight of at least 10% by weight, based on the total solids content; spherical, amorphous SiO2 particles having a particle size distribution having a D50 value in the range of 1 μm to 50 μm and having a proportion by weight of at least 30% by weight, based on the total solids content; SiO2 nano particles having particle sizes of less than 100 nm and having a proportion by weight between 0.2% and 10% by weight, based on the total solids content; and a non-ionic, alkali-free surfactant having a proportion in the range of 0.005 to 0.5%, based on the volume of the dispersion liquid.

    摘要翻译: 在已知的方法中,通过喷涂在SiO 2滑移上将SiO2滑移层施加到碱性石英玻璃体上,将滑移层干燥并烧结以形成含SiO 2的功能层。 为了允许可再生产的功能性石英玻璃层,即使在相对于垂直方向弯曲或倾斜的表面的情况下,具有满足对层均匀性的高要求的高层厚度,本发明提出了滑动 在分散液中含有以下组分:分散体,具有D50值在3μm至30μm范围内并且按重量计至少10重量%的增益尺寸分布的无定形SiO 2颗粒,基于总计 固体含量; 基于总固体含量,具有D50值在1μm至50μm范围内并具有至少30重量%的重量比的粒度分布的球形无定形SiO 2颗粒; 基于总固体含量,粒径小于100nm并且重量比为0.2%至10%的SiO 2纳米颗粒; 和非离子型无碱性表面活性剂,其比例基于分散液体积的0.005〜0.5%。

    SOLAR RADIATION RECEIVER HAVING AN ENTRY WINDOW MADE OF QUARTZ GLASS AND METHOD FOR PRODUCING AN ENTRY WINDOW
    9.
    发明申请
    SOLAR RADIATION RECEIVER HAVING AN ENTRY WINDOW MADE OF QUARTZ GLASS AND METHOD FOR PRODUCING AN ENTRY WINDOW 有权
    具有QUARTZ玻璃的入口窗的太阳辐射接收器和用于产生入口窗的方法

    公开(公告)号:US20140360491A1

    公开(公告)日:2014-12-11

    申请号:US14345233

    申请日:2012-09-13

    摘要: Common solar radiation receivers are equipped with a chamber for transmission of an operating gas which is directed along to an absorber for solar radiation for thermal absorption. The absorber has a dome-shaped entry window made of quartz glass, wherein the inner side facing the absorber assumes a nominal interior temperature Ti of at least 950° C. during proper use, preferably at least 1000° C., whereas the outer side facing away from the absorber is exposed to the environment and subject to risk of devitrification. The invention relates to modifying the known solar radiation receiver so that a high absorber temperature can be set and thus a high efficiency of the solar thermal heating is enabled, without increasing the risk of devitrification in the region of the outer side of the entry window.

    摘要翻译: 普通的太阳辐射接收器配备有用于传输工作气体的腔室,该工作气体沿着用于吸收太阳辐射的吸收器而被引导。 吸收器具有由石英玻璃制成的圆顶形入口窗,其中面向吸收器的内侧在适当使用期间呈现至少950℃的标称内部温度Ti,优选地至少为1000℃,而外侧 面向远离吸收器暴露在环境中并且有失透的危险。 本发明涉及修改已知的太阳辐射接收器,从而可以设定高的吸收器温度,从而能够实现太阳能热加热的高效率,而不增加入口窗外侧区域的失透的风险。

    METHOD AND DEVICES FOR PRODUCING OPTICAL GLASS ELEMENTS, PARTICULARLY CONCENTRATOR OPTICS
    10.
    发明申请
    METHOD AND DEVICES FOR PRODUCING OPTICAL GLASS ELEMENTS, PARTICULARLY CONCENTRATOR OPTICS 审中-公开
    用于生产光学玻璃元件的方法和装置,特殊浓度光学元件

    公开(公告)号:US20120094821A1

    公开(公告)日:2012-04-19

    申请号:US13265605

    申请日:2010-04-22

    CPC分类号: C03B23/045 C03B23/055

    摘要: a method and to an apparatus for producing optical glass elements, in particular for producing what is referred to as low-cost optics for focusing light onto small areas, for example, for photovoltaic applications or optical couplers. The method for producing the optical glass elements includes: providing a glass rod having a selected cross-section, heating the glass rod such that it can be deformed in at least some sections, molding at least one optical glass element from the deformable section using a molding tool, separating the optical glass element from the glass rod at the connection, arranging a plurality of separated optical glass elements to form a group, and grinding and/or polishing at least one section of the separating surfaces of the grouped optical glass elements. The invention makes it possible to produce optical glass elements that meet low quality requirements in high quantities and with high output at low cost.